Mechanical response of titanium tri-aluminide intermetallic alloy
Source abstract
Abstract
Abstract The bulk titanium tri-aluminide intermetallic alloy was fabricated via foil reactive sintering using Ti and Al foils in the vacuum. Scanning electron microscopy (SEM) results demonstrated that the original Ti and Al foils were fully reacted and the only synthesized product is monolithic intermetallic Al3Ti. The basic physical properties of the fabricated intermetallic, such as Young's modulus and Poisson ratio, were determined using an ultrasonic wave measurement technique, and the compressive mechanical responses under both quasi-static and high strain rates were studied using universal load frame and modified split Hopkinson pressure bar system, respectively. The experimental results indicated that intermetallic Al3Ti exhibits brittle features, and its compressive strength was sensitive to strain rate. Moreover, the strain rate hardening behavior under high rate range is stronger than that under quasi-static deformation conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Energetic Materials and Combustion · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Intermetallic-matrix composites—a review10.1016/0966-9795(95)00037-2 ↗
2. Progress in the understanding of gamma titanium aluminides10.1007/BF03221103 ↗
3. Alloy modification of [gamma]TiAl for improved mechanical properties10.1016/0956-716X(94)90487-1 ↗
4. A Fundamental Study on Preparation of Al3Ti Powders by Calciothermic Reduction of Oxides10.2320/matertrans1989.32.272 ↗
5. Fabrication of thick intermetallic compound Al3Ti layer on metal substrate by combustion synthesis of ball-milled powder10.2320/matertrans1989.41.631 ↗
6. Synthetic multifunctional metallic-intermetallic laminate composites10.1007/s11837-005-0229-4 ↗
7. Dwivedi · 2010
8. Plastic deformation of the intermetallic compound Al3Ti10.1080/01418618708209869 ↗
9. Deformation and improvement of ductility of the intermetallic compounds AlV and Al(V, Ti)10.1080/01418618808209943 ↗
10. Microstructure, deformation and fracture characteristics of an Al67Ni8Ti25 intermetallic alloy10.1016/0001-6160(89)90296-4 ↗
11. Compression behavior of the forged L12 compounds Al67Ti25Cr8 and Al66Ti25Mn910.1016/0956-716X(90)90066-P ↗
12. DO22 to L12 transition in intermetallic systems10.1007/BF01117910 ↗
13. Ordering, ternary atom location and ageing in Ll2 trialuminide alloys10.1016/0956-7151(92)90469-U ↗
14. Response to three-point bending of the forged L12 compound Al66Ti25Cr910.1016/0966-9795(95)00042-9 ↗
15. Deformation mechanisms and ductility of mechanically alloyed NiAl10.1016/0921-5093(92)90062-6 ↗
16. Temperature dependence of the compressive strength of cubic phases formed by alloying Al3Ti with Mn And Cr10.1016/0956-716X(90)90411-9 ↗
17. Tensile deformation of the forged l12 compound al66ti25mn910.1080/01418619208201482 ↗
18. Tensile behavior of the Ll2 compound Al67Ti25Cr810.1016/0956-7151(92)90178-H ↗
19. Microstructure evolution in metal-intermetallic laminate (MIL) composites synthesized by reactive foil sintering in air10.1007/s11661-001-0237-0 ↗
20. Fracture of Ti-Al3Ti metal-intermetallic laminate composites: effects of lamination on resistance-curve behavior10.1007/s11661-005-0092-5 ↗
21. Resistance-curve and fracture behavior of Ti–Al3Ti metallic–intermetallic laminate (MIL) composites10.1016/S1359-6454(03)00108-3 ↗
22. Vecchio · 2005
23. Combustion synthesis of cubic Al3Ti alloys10.1557/JMR.1992.2733 ↗
24. Standard Practice for Measuring Ultrasonic Velocity in Materials, ASTM, 2010.
25. Fracture behavior of Ti/Al3Ti metal-intermetallic laminate (MIL) composite under dynamic loading10.1016/j.msea.2015.04.025 ↗
26. Materials testing at high constant strain rates10.1088/0022-3735/15/3/009 ↗
27. Split Hopkinson bar techniques for Characterizing soft materials
28. Dynamic compression testing of soft materials10.1115/1.1464871 ↗
29. Improved pulse shaping to achieve constant strain rate and stress equilibrium in split-Hopkinson pressure bar testing10.1007/s11661-007-9204-8 ↗
30. Characterization and properties of intermetallic Al3Ti alloy synthesized by reactive foil sintering in vacuum10.1557/jmr.2016.298 ↗
31. Harach · 2000
32. Effect of strain rate on compressive mechanical properties of extruded Mg–8Li–1Al–1Ce alloy10.1016/j.matdes.2013.01.049 ↗