Effect of cutting method on hydrogen embrittlement of high-Mn TWIP steel
Source abstract
Abstract
Abstract The objective of this study was to fill a knowledge gap about the effect of cut-edge properties on hydrogen embrittlement (HE) of a cold rolled Fe-20Mn-0.35C-1Al-1.6Cr TWIP (twinning induced plasticity) steel. Slow strain rate tests were performed on hydrogen uncharged and hydrogen pre-charged specimens prepared by four cutting methods: electrical discharge machining, laser cutting, abrasive waterjet cutting, and blanking. It was observed that the laser-cut and hydrogen pre-charged specimens showed the highest total elongation (62%) during tensile test, whereas the blanked and hydrogen pre-charged specimens showed the lowest total elongation (30%). The high HE susceptibility of blanked specimens was explained by the local high dislocation density assisted by the hydrogen-enhanced localized plasticity mechanism. Furthermore, tensile residual stresses generated by blanking facilitated the hydrogen diffusion and the growth of hydrogen-assisted cracks.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. High manganese austenitic twinning induced plasticity steels: a review of the microstructure properties relationships10.1016/j.cossms.2011.04.002 ↗
2. Twinning-induced plasticity (TWIP) steels10.1016/j.actamat.2017.06.046 ↗
3. Revealing the strain-hardening behavior of twinning-induced plasticity steels: theory, simulations, experiments10.1016/j.actamat.2012.09.064 ↗
4. Understanding martensite and twin formation in austenitic steels: a model describing TRIP and TWIP effects10.1016/j.actamat.2017.02.004 ↗
5. Effect of hydrogen content on the embrittlement in a Fe-Mn-C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
6. Hydrogen embrittlement in a Fe-Mn-C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
7. The role of the microstructure on the influence of hydrogen on some advanced high-strength steels10.1016/j.msea.2017.12.079 ↗
8. Delayed static failure of twinning-induced plasticity steels10.1016/j.scriptamat.2012.02.038 ↗
9. Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels10.1016/j.msea.2010.12.085 ↗
10. The mechanism of enhanced resistance to the hydrogen delayed fracture in Al-added Fe–18Mn–0.6C twinning-induced plasticity steels10.1016/j.ijhydene.2012.03.100 ↗
11. Effect of Al addition on low-cycle fatigue properties of hydrogen- charged high-Mn TWIP steels10.1016/j.msea.2016.09.082 ↗
12. Effects of grain size on hydrogen embrittlement in a Fe-22Mn-0.6C TWIP steel10.1016/j.ijhydene.2015.06.112 ↗
13. Effect of grain refinement on hydrogen embrittlement behaviors of high-Mn TWIP steel10.1016/j.msea.2015.11.017 ↗
14. The advantage of grain refinement in the hydrogen embrittlement of Fe–18Mn–0.6C twinning-induced plasticity steel10.1016/j.corsci.2015.01.012 ↗
15. Effect of shear cutting on ductility of a dual phase steel10.1016/j.engfracmech.2008.10.009 ↗
16. The influence of mechanical and CO2 laser cut-edge characteristics on the fatigue life performance of high strength automotive steels10.1016/j.jmatprotec.2010.09.018 ↗
17. Characteristics of abrasive waterjet cut-edges and the affect on formability and fatigue performance of high strength steels10.1016/j.jmapro.2009.12.001 ↗
18. Waterjet — an innovative tool for manufacturing10.1016/j.jmatprotec.2009.05.025 ↗
19. Microstructure analysis of the martensitic stainless steel surface fine-cut by the wire electrode discharge machining ( WEDM)10.1016/j.msea.2003.10.277 ↗
20. Laser and mechanical cutting effects on the cut-edge properties of steel S355N10.1016/j.jcsr.2017.02.012 ↗
21. Degradation of titanium 6Al – 4V fatigue strength due to electrical discharge machining10.1016/j.ijfatigue.2014.02.018 ↗
22. Advanced TEM examinations by an example of microalloyed steels
23. X-ray diffraction study of microstructural changes during fatigue damage initiation in pipe steels: role of the initial dislocation structure10.1016/j.msea.2013.05.042 ↗
24. Grain detection from 2d and 3d EBSD data-Specification of the MTEX algorithm10.1016/j.ultramic.2011.08.002 ↗
25. Role of Cu on hydrogen embrittlement behavior in Fe-Mn-C-Cu TWIP steel10.1016/j.ijhydene.2015.04.022 ↗
26. The effect of Ti precipitates on hydrogen embrittlement of Fe-18Mn-0.6C-2Al-xTi twinning-induced plasticity steel10.1016/j.corsci.2014.08.005 ↗
27. Hydrogen influence on some advanced high-strength steels10.1016/j.corsci.2017.06.012 ↗
28. Formability of TWIP (twinning induced plasticity) automotive sheets10.1016/j.ijplas.2010.03.006 ↗
29. Edge cracking mechanism in two dual-phase advanced high strength steels10.1016/j.msea.2014.06.101 ↗
30. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
31. Spatially and kinetically resolved mapping of hydrogen in a twinning-induced plasticity steel by use of scanning kelvin probe force microscopy10.1149/2.0131512jes ↗
32. Effect of strain rate on hydrogen embrittlement susceptibility of twinning-induced plasticity steel pre-charged with high-pressure hydrogen gas10.1016/j.ijhydene.2016.06.259 ↗
33. Influence of laser peening on the hydrogen embrittlement resistance of 316L stainless steel10.1016/j.surfcoat.2017.08.037 ↗
34. Numerical simulation of the effects of residual stress on the concentration of hydrogen around a crack tip10.1016/j.surfcoat.2011.12.018 ↗
35. High concentration carbon assists plasticity-driven hydrogen embrittlement in a Fe-high Mn steel with a relatively high stacking fault energy10.1016/j.msea.2018.01.087 ↗
36. Hydrogen embrittlement susceptibility of Fe-Mn binary alloys with high Mn content effects of stable and metastable ε martensite, and Mn concentration10.1007/s11661-016-3431-9 ↗
37. Role of martensite in tensile properties and hydrogen degradation of high-Mn steels10.1016/j.msea.2011.11.039 ↗
38. Hydrogen trapping by VC precipitates and structural defects in a high strength Fe-Mn-C steel studied by small-angle neutron scattering10.1016/j.msea.2011.12.080 ↗