In-situ characterization of solidification and microstructural evolution during interrupted thermal fatigue in SAC305 and SAC105 solder joints using high energy X-ray diffraction and post-mortem EBSD analysis
Source abstract
Abstract
Abstract Sn based solders used in the electronic packaging industry exhibit unpredictable failures due to their highly anisotropic properties, where thermal stresses, position within a package and microstructure evolution affect the property evolution and hence, lifetime of solder joints. In the present work, non-destructive high energy-X-ray diffraction measurements were performed in-situ on Sn–1Ag-0.5Cu (SAC105) and Sn–3Ag-0.5Cu (SAC305) solder joints in the corner position in chip array ball grid array packages in order to follow the grain evolution in the same joints starting with melting, solidification/cooling rate, and thermal cycling up to 750 cycles. Most of the SAC305 joints had ‘beachball’ (solidification twinned) microstructures, whereas most of the SAC105 joints were single crystals. Following solidification, the initial solder microstructure was affected in some joints by the thermal strain history during cooling, as new orientations emerged during cooling. During the first 100 thermal cycles, a major shift of dominant orientations was observed in all of the samples, and these orientations were stable thereafter, but the relative volume fractions of three twin-related orientations changed with increasing number of thermal cycles. All of the joints were cross-sectioned following the last increment of thermal cycling (750 thermal cycles), indicating that all of the joints had fully cracked. Electron backscatter diffraction mapping is compared to x-ray measurements, indicating that most of the orientations in the x-ray measurements were present in the cross section, but there were also significant differences, consistent with the fact that the 2-D section represents a small fraction of the entire joint. There was no obvious effect on microstructure or fracture associated with the initial cooling rate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. The orientation imaging microscopy of lead-free Sn-Ag solder joints10.1007/s11837-005-0135-9 ↗
2. Modeling thermomechanical fatigue behavior of Sn-Ag solder joints10.1007/s11664-002-0004-z ↗
3. Elastic constants of βTin from 4.2°K to 300°K10.1103/PhysRev.120.1658 ↗
4. Determination of the elastic moduli of tin single crystals, and their variation with temperature10.1088/0508-3443/11/6/308 ↗
5. Reliability of lead-free interconnections under consecutive thermal and mechanical loadings10.1007/BF02692443 ↗
6. The microstructure of Sn in near-eutectic Sn-Ag-Cu alloy solder joints and its role in thermomechanical fatigue10.1557/JMR.2004.0222 ↗
7. Slip, crystal orientation, and damage evolution during thermal cycling in high-strain wafer-level chip-scale packages10.1007/s11664-014-3572-9 ↗
8. Microstructural evolution of SAC305 solder joints in wafer level chip-scale packaging (WLCSP) with continuous and interrupted accelerated thermal cycling10.1007/s11664-016-4343-6 ↗
9. Influence of Sn grain size and orientation on the thermomechanical response and reliability of Pb-free solder joints10.1109/TCAPT.2008.916835 ↗
10. The role of elastic and plastic anisotropy of Sn in recrystallization and damage evolution during thermal cycling in SAC305 solder joints10.1007/s11664-011-1811-x ↗
11. Harnessing heterogeneous nucleation to control tin orientations in electronic interconnections10.1038/s41467-017-01727-6 ↗
12. Grain structure evolution and its impact on the fatigue reliability of lead-free solder joints in BGA packaging assembly
13. Slip, crystal orientation, and damage evolution during thermal cycling in high-strain wafer-level chip-scale packages10.1007/s11664-014-3572-9 ↗
14. Reliability of lead-free solder joints in CSP device under thermal cycling10.1007/s10854-014-1711-y ↗
15. Thermal cycling reliability of Sn-Ag-Cu solder interconnections. Part 1: effects of test parameters10.1007/s11664-013-2551-x ↗
16. Thermal cycling reliability of Sn-Ag-Cu solder interconnections-Part 2: failure mechanisms10.1007/s11664-013-2475-5 ↗
17. Inhomogeneous deformation and microstructure evolution of Sn-Ag-based solder interconnects during thermal cycling and shear testing10.1016/j.microrel.2012.01.009 ↗
18. Incremental recrystallization/grain growth driven by elastic strain energy release in a thermomechanically fatigued lead-free solder joint10.1016/j.actamat.2006.11.023 ↗
19. Recrystallization of Sn grains due to thermal strain in Sn-1.2Ag-0.5Cu-0.05Ni solder10.2320/matertrans.45.1383 ↗
20. Electromigration in submicron interconnect features of integrated circuits10.1016/j.mser.2010.09.001 ↗
21. Electromigration mechanisms in Sn-0.7Cu/Cu couples by four dimensional (4D) X-ray microtomography and electron backscatter diffraction (EBSD)10.1016/j.actamat.2015.08.073 ↗
22. Effect of dwell times on thermomechanical fatigue behavior of Sn-Ag-based solder joints10.1007/s11664-003-0137-8 ↗
23. Residual-mechanical behavior of thermomechanically fatigued Sn-Ag based solder joints10.1007/s11664-002-0188-2 ↗
24. Effect of thermo-mechanically induced microstructural coarsening on the evolution of creep response of SnAg-based microelectronic solders10.1016/j.msea.2005.08.142 ↗
25. Microstructure and damage evolution in Sn-Ag-Cu solder joints
26. Inhomogeneous deformation and microstructure evolution of Sn-Ag-based solder interconnects during thermal cycling and shear testing10.1016/j.microrel.2012.01.009 ↗
27. Thermal cycling reliability of Sn-Ag-Cu solder interconnections. Part 1: effects of test parameters10.1007/s11664-013-2551-x ↗
28. Thermal cycling reliability of Sn-Ag-Cu solder interconnections—Part 2: failure mechanisms10.1007/s11664-013-2475-5 ↗
29. Effect of isothermal aging on the long-term reliability of fine-pitch Sn-Ag-Cu and Sn-Ag solder interconnects with and without board-side Ni surface finish10.1007/s11664-014-3315-y ↗
30. Nanoscale three-dimensional microstructural characterization of an Sn-rich solder alloy using high-resolution transmission X-ray microscopy (TXM)10.1017/S1431927616011429 ↗
31. Synchrotron radiation microtomography for large area 3D imaging of multilevel microelectronic packages10.1007/s11664-014-3375-z ↗
32. In situ synchrotron study of electromigration induced grain rotations in Sn solder joints
33. In situ synchrotron characterization of melting, dissolution, and resolidification in lead-free solders10.1007/s11664-011-1785-8 ↗
34. In situ characterization of twin nucleation in pure Ti using 3D-XRD10.1007/s11661-013-2082-3 ↗
35. Influence of Ni on the refinement and twinning of primary Cu6Sn5 in Sn-0.7Cu-0.05Ni10.1016/j.intermet.2018.08.002 ↗
36. On the 3-D shape of interlaced regions in Sn-3Ag-0.5Cu solder balls
37. Lee · 2015 · vol. XIII · 253
38. Direct observation of gliding and twinning in beta-tin lamellae
39. Cyclic twin nucleation in tin-based solder alloys10.1016/j.actamat.2010.01.030 ↗
40. Recrystallization and precipitate coarsening in Pb-free solder joints during thermomechanical fatigue10.1007/s11664-011-1762-2 ↗
41. Localized recrystallization and cracking behavior of lead-free solder interconnections under thermal cycling, 2009 international conference on electronic packaging technology and high density packaging
42. The microstructure of Sn in near-eutectic Sn-Ag-Cu alloy solder joints and its role in thermomechanical fatigue10.1557/JMR.2004.0222 ↗