Effect of powder layer thickness and scan orientation on the deformation and failure of selectively laser melted Ti-6Al-4V alloy over six decades of strain rates
Source abstract
Abstract
Abstract The plastic deformation and failure behavior of additively manufactured Ti-6Al-4V coupons via selective laser melting (SLM) are investigated over 6 decades of strain rates i.e., 10−3, 10, 2000, and 7000 s−1. Four different types of mesostructures are generated by varying the powder layer thickness and scan rotation in the SLM process. A scan rotation, ψ, 90° produces mesostructures having cuboidal grains along the build direction and columnar prior β grains on the scanned direction, while ψ of 67° produces nearly equiaxed grains along the build and scanned directions. All the mesostructures, independent of ψ, consists of fine acicular martensitic α ′ laths. Experimental results show that the flow stress increases with strain rate suggesting that all the samples exhibit positive strain rate sensitivity. Post deformation macroscopic images of the failed samples show that plastic strain localization increased with strain rate. At high strain rates, the deformation is dominated by adiabatic shear bands (ASBs) and significant macro-cracks are observed along with the shear bands particularly at high strain rates. The ASBs are more tortuous in the samples fabricated using scan rotation of 67° as compared to 90° suggesting that the nature of mesostructure has a pronounced effect on the deformation characteristics. Further, the fractographs analyzed using a scanning electron microscope clearly show both ductile and brittle features.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Lütjering · 2007
2. Microstructure engineering of titanium alloys via small boron additions10.1007/s12572-011-0033-z ↗
3. Dutta · 2016
4. Ladani · 2020
5. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
6. Mechanical anisotropy and strain rate dependency behavior of Ti6Al4V produced using E-beam additive fabrication10.1115/1.4027729 ↗
7. Microstructural characteristic and mechanical property of Ti6Al4V alloy fabricated by selective laser melting10.1016/j.vacuum.2018.01.026 ↗
8. Sliding wear of selective laser melting processed Ti6Al4V under boundary lubrication conditions10.1016/j.wear.2016.09.020 ↗
9. “Elastic properties of the α’ martensitic phase in the Ti-6Al-4V alloy obtained by additive manufacturing10.1016/j.scriptamat.2019.03.042 ↗
10. “Influence of heat-treatment on the dynamic behavior of 3D laser-deposited Ti–6Al–4V alloy10.1016/j.msea.2016.09.036 ↗
11. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
12. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti6Al4V alloy10.1016/j.actamat.2019.03.003 ↗
13. “Thermomechanical response of 3D laser-deposited Ti–6Al–4V alloy over a wide range of strain rates and temperatures10.1016/j.msea.2015.08.043 ↗
14. Microstructure, static properties, and fatigue crack growth mechanisms in Ti-6Al-4V fabricated by additive manufacturing: LENS and EBM10.1016/j.engfailanal.2016.05.036 ↗
15. Strain rate effect on the tension and compression stress-state asymmetry for electron beam additive manufactured Ti6Al4V10.1016/j.msea.2017.12.062 ↗
16. Local and global mechanical behavior and microstructure of Ti6Al4V parts built using electron beam melting technology10.1007/s11661-016-3402-1 ↗
17. “Compressive properties and micro-structural characteristics of Ti–6Al–4V fabricated by electron beam melting and selective laser melting10.1016/j.msea.2019.138204 ↗
18. Influence of process parameter and strain rate on the dynamic compressive properties of selective laser-melted Ti-6Al-4V alloy10.1007/s00339-018-2359-x ↗
19. Deformation and fracture behavior of laser processed dense and porous Ti6Al4V alloy under static and dynamic loading10.1016/j.msea.2012.04.036 ↗
20. Dynamic mechanical behavior of additively manufactured Ti6Al4V with controlled voids10.1115/1.4029745 ↗
21. Defect formation mechanisms in selective laser melting: a review10.1007/s10033-017-0121-5 ↗
22. Meyers · 1994
23. Chen · 2011
24. The rate-dependent deformation and localization of fully dense and porous Ti-6Al-4V10.1016/S0921-5093(97)00076-2 ↗
25. Room and high temperature dry sliding wear behavior of Boron modified as-cast Ti-6Al-4V alloys against hardened steel10.1016/j.wear.2018.10.021 ↗
26. Grain morphology evolution behavior of titanium alloy components during laser melting deposition additive manufacturing10.1016/j.jallcom.2015.01.256 ↗
27. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium10.1016/S0031-8914(34)80244-3 ↗
28. “Correlation of microstructural, textural characteristics and hardness of Ti–6Al–4V sheet β-cooled at different rates10.1007/s10853-020-04603-9 ↗
29. The effect of microstructure on the mechanical properties of two-phase titanium alloys10.1016/S0924-0136(02)00248-0 ↗
30. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
31. “Graded microstructure and mechanical properties of additive manufactured Ti–6Al–4V via electron beam melting10.1016/j.actamat.2015.06.036 ↗
32. “Capturing of the propagating processes of adiabatic shear band in Ti–6Al–4V alloys under dynamic compression10.1016/j.msea.2016.01.062 ↗
33. A microstructure sensitive model for deformation of Ti-6Al-4V describing Cast-and-Wrought and Additive Manufacturing morphologies10.1016/j.matdes.2018.09.028 ↗
34. “Constitutive analysis of compressive deformation behavior of ELI-grade Ti–6Al–4V with different microstructures10.1007/s10853-011-6145-9 ↗
35. The structure of adiabatic shear bands in a titanium alloy10.1016/0001-6160(85)90030-6 ↗
36. The structure of adiabatic shear bands in metals: a critical review10.1016/0001-6160(87)90238-0 ↗
37. “Dynamic behavior of HIPed Ti–6Al–4V10.1016/j.ijimpeng.2006.01.006 ↗
38. “Dynamic mechanical properties and adiabatic shearing behavior of the shock prestrained Ti–6Al–4V alloy having bimodal microstructure10.1016/j.jallcom.2018.09.207 ↗
39. Adiabatic shear fracture in Ti-6Al-4V alloy10.1016/S1003-6326(11)61026-1 ↗
40. The dynamic flow and failure behavior of magnesium and magnesium alloys10.1007/s11837-013-0850-6 ↗
41. Microstructural characterization and evolution mechanism of adiabatic shear band in a near beta-Ti alloy10.1016/j.msea.2010.12.053 ↗
42. The latent energy remaining in a metal after cold working
43. Understanding the effect of laser scan strategy on residual stress in selective laser melting through thermo-mechanical simulation
44. “The dependence of the Taylor–Quinney coefficient on the dynamic loading mode10.1016/j.jmps.2017.06.016 ↗
45. Adiabatic shear failure and dynamic stored energy of cold work10.1103/PhysRevLett.96.075502 ↗
46. Shear localization in dynamic deformation of materials: microstructural evolution and self-organization10.1016/S0921-5093(01)01160-1 ↗
47. Shear localization and recrystallization in high-strain, high-strain-rate deformation of tantalum10.1016/S0921-5093(96)10847-9 ↗
48. Microstructure of adiabatic shear bands in Ti6Al4V10.1016/j.matchar.2012.10.009 ↗
49. Dynamic recrystallization as a potential cause for adiabatic shear failure10.1103/PhysRevLett.101.165501 ↗
50. Adiabatic shear localization in titanium and Ti-6 pct Al-4 pct V alloy10.1007/BF02814827 ↗
51. Correlation of adiabatic shearing behavior with fracture in Ti-6Al-4V alloys with different microstructures10.1016/j.ijimpeng.2008.12.007 ↗