Study of the relationship among total oxygen, inclusions and fatigue properties of gear steel
Source abstract
Abstract
Abstract In order to control non-metallic inclusions and improve fatigue performance of gear steel, the relationship among total oxygen, inclusion size and fatigue properties of gear steel was investigated. In the work, Mn–Cr system gear steels with different total oxygen contents were selected as the research objects. Inclusions and fatigue properties of gear steels with different total oxygen contents were studied by using traditional metallographic method, extreme value method and fatigue test. The experimental results demonstrates that with the decrease of total oxygen content(i.e., 0.0013%→0.0010%→0.0005%), the number of small-size oxide inclusions in the range of 5–10 μm decreases greatly, whereas the number of large-size oxide inclusions over 10 μm has relatively little change. Meanwhile, it is found that the change of total oxygen content in different ranges has different influences on the size of maximum size oxide inclusion and fatigue properties. Reducing the total oxygen content of gear steel from 0.0013% to 0.0010% decreases the inclusion size of maximum oxide inclusion and improves fatigue resistance of materials, but these benefits do not extend to a total oxygen level of 0.0005%. Accordingly, we can conclude that no evident linear correlation exists between total oxygen content and maximum inclusion size or between the total oxygen content and the fatigue performance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Recent development of bearing steel in Japan[J]10.2355/tetsutohagane1955.74.10_1889 ↗
2. Recent Development of bearing steel in Japan[J]10.2355/isijinternational1966.28.893 ↗
3. Production of high-carbon chromium bearing steel in vertical type continuous caster[J]10.2355/isijinternational1966.26.614 ↗
4. Production and quality of high cleanliness bearing steel[C]
5. Generation mechanisms of non-metallic inclusions in high-cleanliness steel[J]10.2355/tetsutohagane.93.743 ↗
6. Development of secondary refining process and its application to production of clean steel[J]10.2355/tetsutohagane1955.72.9_1309 ↗
7. The measurement of particle size distribution of Al2O3 inclusion in ultra low oxygen steel[J]10.2355/tetsutohagane1955.77.12_2163 ↗
8. Past development and future prospects of secondary refining technology[J]10.2355/tetsutohagane.100.456 ↗
9. Effect of calcium treatment on non-metallic inclusions in ultra-low oxygen steel refined by high basicity high Al2O3 slag[J]10.1016/S1006-706X(11)60083-6 ↗
10. Deoxidation and inclusion control in special steel refining[J]
11. Progress on control of ultra-low-oxygen content and non-metallic inclusions in high quality bearing steel[J]
12. Investigation on technology of non-metallic inclusion control for high grade special steels of important uses
13. Control technology for oxygen content and inclusions of gear steel[J]
14. Study on improving cleanliness of gear steel FAS 3420H steelmaking by 60t EAF-LF-VD-CC flow sheet[J]
15. 2014
16. Production of high carbon chromium bearing steel in BOF-CC process[J]10.2355/tetsutohagane1955.73.3_513 ↗
17. Clean bearing steel, technology for control of nonmetallic inclusions and production of clean steels
18. Investigation on nonmetallic inclusions in ultra-low-oxygen special steels[J]10.1007/s11663-016-0687-9 ↗
19. Inclusion composition control in tyre cord steel by top slag refining[J]10.1179/1743281214Y.0000000182 ↗
20. Inclusion size effect on the fatigue crack propagation mechanism and fracture mechanics of a superalloy[J]10.1007/BF02801169 ↗
21. Influence of non-metallic inclusions on the fatigue properties of heavily cold drawn steel wires[J]10.1016/j.proeng.2010.03.019 ↗
22. Behavior of nonmetallic inclusions in ultra-low oxygen steel 25CrMoVNi for high speed rail axles during RH refining process[
23. Influence of calcium treatment on oxide inclusions in ultra-low oxygen refining process[J]
24. Laboratory study on formation of complex inclusions in ultra-low oxygen steel[J]10.1179/1743281212Y.0000000100 ↗
25. Control of magnesia-alumina spinel inclusions in the ultra-low-oxygen gear steel 28MnCr5[J]
26. Distribution and control of oxide inclusion in tire cord steel bloom[J]
27. A new nonmetallic inclusion rating method by positive use of hydrogen embrittlement phenomenon[J]10.1007/s11661-012-1376-1 ↗
28. Instructions for a new method of inclusion rating and correlations with the fatigue limit[J]10.1520/JTE11840J ↗
29. Statistical analysis of defects for fatigue strength prediction and quality control of materials[J]10.1046/j.1460-2695.1998.00104.x ↗
30. Comparison of extreme value statistics methods for predicting maximum inclusion size in clean steels[J]10.1179/030192399677095 ↗
31. Largest-extreme-value distribution analysis of multiple inclusion types in determining steel cleanliness[J]10.1007/s11663-001-0036-4 ↗
32. Gumbel · 1958
33. Evaluation of inclusions of ultra-low oxygen bearing steel by statistics of extreme values method[J]
34. Inclusion-controlled fatigue properties of 1800 MPa-class spring steels[J]10.1007/s11661-004-0279-1 ↗
35. K. Chan. A fatigue life model for predicting crack nucleation at inclusion in Ni-based superalloys[J]. Metall. Mater. Trans., published online: 17 December 2019.10.1007/s11661-019-05592-4 ↗
36. Gigacycle fatigue properties of high-strength steels according to inclusion and ODA sizes[J]10.1007/s11661-007-9225-3 ↗
37. Control of stringer shaped non-metallic inclusions of CaO-Al2O3 system in API X80 linepipe steel plates[J]10.1016/j.jcsr.2013.01.012 ↗
38. Small defects and inhomgenities in fatigue strength: experiments, models and statistical implications10.1023/A:1009976418553 ↗
39. Murakami · 2002
40. Quantitative evaluation of effects of defects and non-metallic inclusions on fatigue strength of metals[J]10.2355/tetsutohagane1955.75.8_1267 ↗