Inheritance of microstructure and mechanical properties in laser powder bed fusion additive manufacturing: A feedstock perspective

D.W. Wang, Y.H. Zhou, X.Y. Yao, Y.P. Dong, S.H. Feng, Z.Y. Liu, H. Wang, M. Yan

Publisher page

Abstract

Abstract Correlation between the feedstock powder and the as-printed products is well expected in laser powder bed fusion (LPBF). However, the inheritance/heredity relationship between the feedstock powder and the products remains broadly overlooked since most atomized powders are printed without any modification. This study addresses the inheritance issue through comparing the hydrogenation/dehydrogenation (HDH) Ti powder with the ball-milled (BM) Ti powder, as well as the respective as-printed samples. Rietveld refinement, focused ion beam, electron backscatter diffraction, and transmission electron microscopy are employed to characterize the microstructure; uniaxial tensile tests and fractographic observation are performed for the mechanical analysis; single-track finite element simulations are conducted to reveal the varied powder-bed properties. A “core-shell” powder structure has been generated through the ball milling modification. Nano-crystallites in the “shell” and stress-induced twins have brought significant grain refinement to the BM powder. A β-to-αm massive transformation has been observed in the samples printed using HDH powder, whereas the microstructure changes to fully-martensitic when using BM powder as the feedstock. Excellent mechanical performance (∼1000 MPa tensile strength with ∼20% ductility) have been achieved through inheriting the fine microstructure and oxygen content from the BM powder, which are induced by the powder modification process. This study has therefore unveiled the comprehensive correlation between the feedstock powder and the as-printed Ti, highlighting a novel methodology for developing additively-manufactured, cost-effective, and high-performance materials through tailoring the feedstock powder.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (80)

Show source-provided references
1. Gibson · 2014
2. Overview on additive manufacturing technologies10.1109/JPROC.2016.2625098 ↗
3. Selective laser melting enabled additive manufacturing of Ti-22Al-25Nb intermetallic: excellent combination of strength and ductility, and unique microstructural features associated10.1016/j.actamat.2019.05.008 ↗
4. Keyhole threshold and morphology in laser melting revealed by ultrahigh-speed x-ray imaging10.1126/science.aav4687 ↗
5. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
6. Low-cost Ti powders for additive manufacturing treated by fluidized bed10.1016/j.powtec.2019.03.042 ↗
7. An overview of powder granulometry on feedstock and part performance in the selective laser melting process
8. Calculation of laser absorption by metal powders in additive manufacturing10.1364/AO.54.002477 ↗
9. A new approach for a flexible powder production for additive manufacturing
10. Effects of powder attributes and laser powder bed fusion (L-PBF) process conditions on the densification and mechanical properties of 17-4 PH stainless steel10.1007/s11837-015-1770-4 ↗
11. Feedstock powder processing research needs for additive manufacturing development10.1016/j.cossms.2018.01.002 ↗
12. A comparative study of Ti-6Al-4V powders for additive manufacturing by gas atomization, plasma rotating electrode process and plasma atomization10.1016/j.powtec.2018.04.013 ↗
13. Densification behavior of gas and water atomized 316L stainless steel powder during selective laser melting10.1016/j.apsusc.2010.02.030 ↗
14. Production of titanium metal powder by the HDH process
15. Ultra-low cost Ti powder for selective laser melting additive manufacturing and superior mechanical properties associated10.29026/oea.2019.180028 ↗
16. Flow behavior of powder particles in layering process of selective laser melting: numerical modeling and experimental verification based on discrete element method10.1016/j.ijmachtools.2017.08.004 ↗
17. High strain-rate superplasticity of AZ91 alloy achieved by rapidly solidified flaky powder metallurgy10.1016/j.matlet.2018.09.090 ↗
18. Design of powder metallurgy titanium alloys and composites10.1016/j.msea.2005.10.057 ↗
19. New microstructure design for commercially pure titanium with outstanding mechanical properties by mechanical milling and hot roll sintering10.2320/matertrans.MB200913 ↗
20. Heredity of aluminum melt by electric pulse modification (II)10.1016/S1006-706X(07)60079-X ↗
21. The heredity of Al-Si-Mg-Mn before and after Remelting10.1007/s11837-997-0010-y ↗
22. Carburiser properties transfer into the structure of melted cast iron10.1016/j.jmatprotec.2013.11.027 ↗
23. 24 - the additive manufacturing (AM) of titanium alloys
24. Titanium in biomedical applications—properties and fabrication: a review10.1166/jbt.2015.1361 ↗
25. Grain morphology evolution behavior of titanium alloy components during laser melting deposition additive manufacturing10.1016/j.jallcom.2015.01.256 ↗
26. Additive manufacturing of pure Ti with superior mechanical performance, Low cost, and biocompatibility for potential replacement of Ti-6Al-4 V10.1016/j.matdes.2020.109142 ↗
27. Cost-affordable Ti-6Al-4V for additive manufacturing: powder modification, compositional modulation and laser in-situ alloying
28. Recent advances in magnetic structure determination by neutron powder diffraction
29. ARPGE: a computer program to automatically reconstruct the parent grains from electron backscatter diffraction data10.1107/S0021889807048777 ↗
30. Prediction of spatiotemporal variations of deposit profiles and inter-track voids during laser directed energy deposition
31. Mechanisms on inter-track void formation and phase transformation during laser Powder Bed Fusion of Ti-6Al-4V
32. Selective laser melting under the reactive atmosphere: a convenient and efficient approach to fabricate ultrahigh strength commercially pure titanium without sacrificing ductility10.1016/j.msea.2019.138078 ↗
33. Characteristics of Ti6Al4V powders recycled from turnings via the HDH technique
34. Powder flowability characterisation methodology for powder-bed-based metal additive manufacturing10.1007/s40964-015-0001-4 ↗
35. The use of bulk density measurements as flowability indicators10.1016/S0032-5910(98)00208-3 ↗
36. Characterization of powder flowability using measurement of angle of repose10.1016/S1672-2515(07)60247-4 ↗
37. XRD line profile analysis of calcite powders produced by high energy milling10.1524/zksu.2008.0019 ↗
38. Line broadening analysis using FullProf*: determination of microstructural properties10.4028/www.scientific.net/MSF.443-444.123 ↗
39. Comparison of residual strains measured by X-ray and neutron diffraction in a titanium (Ti-6Al-4V) matrix composite10.1016/S0921-5093(98)00893-4 ↗
40. Size effects on the tensile properties and deformation mechanism of commercial pure titanium foils10.1016/j.msea.2018.06.009 ↗
41. Deformation behavior of CP-titanium: experiment and crystal plasticity modeling10.1016/j.msea.2018.03.017 ↗
42. A statistical study of the relationship between plastic strain and lattice misorientation on the surface of a deformed Ni-based superalloy10.1016/j.actamat.2020.05.029 ↗
43. Titanium nitride oxidation chemistry - an X-ray photoelectron-spectroscopy study10.1063/1.351465 ↗
44. Fundamental understanding of the dissolution of oxide film on Ti powder and the unique scavenging feature by LaB610.1007/s11661-017-4366-5 ↗
45. Direct observation of pore formation mechanisms during LPBF additive manufacturing process and high energy density laser welding10.1016/j.ijmachtools.2020.103555 ↗
46. In situ radiographic and ex situ tomographic analysis of pore interactions during multilayer builds in laser powder bed fusion
47. A comparative study of water and gas atomized low alloy steel powders for additive manufacturing
48. Failure of metals I: brittle and ductile fracture10.1016/j.actamat.2015.12.034 ↗
49. Comparative study of commercially pure titanium produced by laser engineered net shaping, selective laser melting and casting processes10.1016/j.msea.2017.08.103 ↗
50. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
51. Lütjering · 2007
52. Massive transformations revisited10.1007/s11661-002-0351-7 ↗
53. Microstructural evolution of fusion zone in laser beam welds of pure titanium10.1016/j.matchar.2011.12.010 ↗
54. Massive transformation in Ti–6Al–4V additively manufactured by selective electron beam melting10.1016/j.actamat.2015.11.011 ↗
55. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
56. Taylor factors in materials with many deformation modes10.1016/1359-6462(96)00137-6 ↗
57. In situ monitoring of the deformation mechanisms in titanium with different oxygen contents10.1016/j.msea.2015.03.044 ↗
58. Room-temperature ductility of Ti–6Al–4V alloy with α′ martensite microstructure10.1016/j.msea.2010.10.070 ↗
59. Effects of the prior austenite grain-size on the ductility of fully pearlitic eutectoid steel10.1007/BF02643953 ↗
60. Continuous cooling β-to-α transformation behaviors of extra-pure and commercially pure Ti10.1007/s11661-004-0052-5 ↗
61. In-situ measurement of continuous cooling β → α transformation behavior of CP-Ti10.1007/s11661-002-0206-2 ↗
62. The effect of scan speed and hatch distance on prior-beta grain size in laser powder bed fused Ti-6Al-4V10.1007/s00170-019-03719-w ↗
63. Laser powder-bed fusion additive manufacturing: physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones10.1016/j.actamat.2016.02.014 ↗
64. In-situ characterization of laser-powder interaction and cooling rates through high-speed imaging of powder bed fusion additive manufacturing10.1016/j.matdes.2017.09.044 ↗
65. Selective laser melting of iron powder: observation of melting mechanism and densification behavior via point-track-surface-Part Research
66. Photopyroelectric measurement of thermal conductivity of metallic powders10.1063/1.1832740 ↗
67. Mechanistic models for additive manufacturing of metallic components10.1016/j.pmatsci.2020.100703 ↗
68. Fluid and particle dynamics in laser powder bed fusion10.1016/j.actamat.2017.09.051 ↗
69. Ductility improvement mechanism of Ti–6Al–4V+O sintered10.2320/matertrans.Y-M2019869 ↗
70. Selective laser-melted titanium materials with nitrogen solid solutions for balanced strength and ductility10.1016/j.msea.2020.139641 ↗
71. Mechanical properties of biomedical titanium alloys10.1016/S0921-5093(97)00806-X ↗
72. Additive manufacturing of metallic components - process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
73. Effect of interstitial solutes on the strength and ductility of titanium10.1016/0079-6425(81)90001-3 ↗
74. The rate controlling mechanism during yielding and flow of α-titanium at temperatures below 0.4 TM10.1016/0001-6160(66)90186-6 ↗
75. Grain size and orientation distributions: application to yielding of α-titanium10.1016/j.actamat.2008.12.037 ↗
76. Titanium, metallurgy of the rarer metal, No. 410.1149/1.2430355 ↗
77. Integrated constitutive model for flow behavior of pure titanium considering interstitial solute concentration10.1007/s12540-014-6004-8 ↗
78. Origin of dramatic oxygen solute strengthening effect in titanium10.1126/science.1260485 ↗
79. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium10.1016/j.msea.2013.11.038 ↗
80. Enhanced strength and ductility in a high-entropy alloy via ordered oxygen complexes10.1038/s41586-018-0685-y ↗