Metallurgical analysis of laser powder bed-fused Al–Si–Mg alloys: Main causes of premature failure
Source abstract
Abstract
AlSi7Mg and AlSi10Mg are the most used alloys to manufacture Laser Powder Bed Fusion lightweight components. These products have high specific strengths but a sometimes-limited ductility. Several direct aging and T6 heat treatments were applied to as-built alloys to solve the problem and optimise their tensile properties. Investigations about causes of premature failure in AlSi7Mg and AlSi10Mg tensile samples were performed in the as-built, direct aged (200°C × 4h) and T6 (solution heat treatment at 505°C × 4h followed by aging at 175°C) treated conditions. In as built and direct aged samples, laser scan track boundaries affected the crack propagation and, consequently, the elongation values in each analysed condition. Higher elongation values were obtained when the crack predominantly propagates within the heat affected zones and along the laser scan track boundaries. After T6 treatment, defects and needle-like δ-Al5FeSi intermetallic particles are observed contributing to the crack nucleation of samples. The laser scan track boundaries remain after the solution heat treatment and redirect the crack propagation in T6 Al-alloys. The effects of precipitation hardened α-Al matrix on the fracture mechanisms were also investigated in AlSi7Mg samples.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. 3D metal printing technology: the need to re-invent design practice10.1007/s00146-018-0809-9 ↗
2. A comparison framework to support the selection of the best additive manufacturing process for specific aerospace applications
3. Additive Manufacturing of AlSi10Mg and Ti6Al4V Lightweight alloys via laser powder bed fusion: a review of heat treatments effects10.3390/ma15062047 ↗
4. Influence on microstructure, strength and ductility of build platform temperature during laser powder bed fusion of AlSi10Mg10.1016/j.actamat.2020.10.001 ↗
5. Effect of distance from build platform and the post-heat treatment of AlSi10Mg alloy manufactured by single and multi-laser SLM10.1007/s11665-021-05577-8 ↗
6. Composition-dependent solidifiation cracking of alluminium-silicon alloys during laser powder bed fusion10.1016/j.actamat.2021.116698 ↗
7. A study of the effect of porosity content on the ductility of sintered metals
8. Work hardening of heat-treated AlSi10Mg alloy manufactured by single and double laser selective laser melting: effects of layer thickness and hatch spacing10.3390/ma14174901 ↗
9. Aging profiles of AlSi7Mg0.6 and AlSi10Mg0.3 alloys manufactured via laser-powder bed fusion: direct aging versus T610.3390/ma15176126 ↗
10. Fracture resistance of AlSi10Mg fabricated by laser powder bed fusion10.1016/j.actamat.2021.116869 ↗
11. Damage mechanisms in selective laser melted AlSi10Mg under as built and different post-treatment conditions10.1016/j.msea.2019.138210 ↗
12. Stress partitioning behavior of an AlSi10Mg alloy produced by selective laser melting during tensile deformation using in situ neutron diffraction10.1016/j.jallcom.2016.06.011 ↗
13. Effect of hardening on toughness captured by stress-based damage nucleation in 6061 aluminum alloy10.1016/j.actamat.2019.08.055 ↗
14. The aging characteristic of aluminium alloys electron transmission studied of Al-Mg-Si alloys
15. Morphology and crystallography of β-Mg2Si precipitation in Al-Mg-Si alloys10.2320/matertrans.42.2576 ↗
16. On the occurrence of the metastable phase β’' in an Al-Si-Mg alloy10.1002/pssa.2210240228 ↗
17. Relationship between ductility and the porosity of additively manufactured AlS10Mg10.1016/j.msea.2020.139922 ↗
18. Influence of Si precipitates on fracture mechanisms of AlSi10Mg parts processed by Selective Laser Melting10.1016/j.actamat.2019.06.013 ↗
19. Unravelling the multi-scale structure-property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg10.1038/s41598-021-85047-2 ↗
20. Defect-correlated Vickers microhardness of Al-Si-Mg alloy manufactured by laser powder bed fusion with post-process heat treatments10.1007/s11665-022-06874-6 ↗
21. Influence of microstructural heterogeneity on strain partitioning behavior of metals containing columnar grains10.1016/j.msea.2021.141247 ↗
22. Very-high-cycle fatigue induced growth and amorphization of Si particles in additively manufactured AlSi10Mg alloy: dependence of applied stress ratio10.1016/j.ijfatigue.2022.107167 ↗
23. Simultaneously enhanced strength and ductility of AlSi7Mg alloy fabricated by laser powder bed fusion with on-line static magnetic field, Virtual
24. Influence of microstructure on fracture mechanisms of the heat-treated AlSi10Mg alloy produced by laser-based powder bed fusion10.3390/ma16052006 ↗
25. Thermal post-processing of AlSi10Mg parts produced by Selective Laser Melting using recycled powder
26. The role of defects on tensile deformation and fracture mechanisms of AM AlSi10Mg alloy at room temperature and 250 °C10.1016/j.engfracmech.2021.108215 ↗
27. Factors that affect the properties of additively-manufactured AlSi10Mg: porosity versus microstructure
28. Investigation of porosity, microstructure and mechanical properties of additively manufactured graphene reinforced AlSi10Mg composite
29. Characterization of the effects of internal pores on tensile properties of additively manufactured austenitic stainless steel 316L10.1007/s11340-018-00465-0 ↗
30. The effect of porosity defects on the mid-cycle fatigue behavior of directed energy deposited Ti-6Al-4V10.1016/j.tafmec.2022.103322 ↗
31. Selective laser melting of AlSi10Mg alloy: process optimization and mechanical properties development10.1016/j.matdes.2014.09.044 ↗
32. The influence of the characteristic microstructure of additively manufactured AlSi10Mg on the plastic behaviour at various strain rates10.1016/j.matdes.2022.111112 ↗
33. Numerical and experimental investigations of built orientation dependent Johnson–Cook model for selective laser melting manufactured AlSi10Mg10.1016/j.jmrt.2021.11.062 ↗
34. Heat treatment effect on the mechanical properties and fracture mechanism in AlSi10Mg fabricated by additive manufacturing selective laser melting process10.1016/j.msea.2018.05.074 ↗
35. Effect of soft and hard inclusions in tensile deformation and damage mechanism of Aluminum: a molecular dynamics study10.1016/j.jallcom.2021.159213 ↗
36. Effects of inclusions, grain boundaries and grain orientations on the fatigue crack initiation and propagation behavior of 2524-T3 Al alloy10.1016/j.msea.2013.05.053 ↗
37. The role of inclusions in ductile fracture and fracture toughness10.1016/0013-7944(73)90007-6 ↗
38. High temperature oxidation of Al4C310.1016/j.corsci.2020.108793 ↗
39. Synthesis and some properties of Al4SiC4-Al4O4C composites10.1016/j.ceramint.2018.06.169 ↗
40. Review on the correlation between microstructure and mechanical performance for laser powder bed fusion AlSi10Mg
41. On the competition between particle fracture and particle decohesion in metal matrix composites10.1016/j.actamat.2004.06.009 ↗
42. Influence of aging heat-treatment on damage mechanisms of particulate reinforced aluminium matrix composites10.1515/SECM.2000.9.1.25 ↗
43. Effect of heat treatment on ductility and precipitation size of additively manufactured AlSi10Mg10.3390/met12081311 ↗
44. Experimental and modelling assessment of ductility in a precipitation hardening AlMgScZr alloy10.1016/j.ijplas.2021.102971 ↗