Effect of extrusion speed on mixed grain microstructure and tensile properties of a Mg-2.9Zn-1.1Ca-0.5Mn nanocomposite reinforced by a low mass fraction of TiCp

Kaibo Nie, Zhihao Zhu, Paul Munroe, Kunkun Deng, Jungang Han

Abstract

Abstract In this work, a novel TiC nanoparticle (0.5 wt %) reinforced Mg-2.9Zn-1.1Ca-0.5Mn nanocomposite, with a mixed grain microstructure exhibiting high strength and targeted for biocompatible/structural applications was successfully prepared by ultrasonic assisted semi-solid stirring and extrusion at ultra-slow speeds of 1, 0.1 and 0.01 mm/s. The experimental results revealed that the morphology of the eutectic Ca2Mg6Zn3 phase in the as-cast nanocomposite changed from plate-like to lamellar as a low mass fraction of TiCp was added. Both dynamically recrystallized grains and precipitates were gradually refined with decreasing extrusion speed. The finest recrystallized grains (∼0.46 μm), with a high volume fraction (∼4.3%) of fine precipitates, appeared after extrusion at 0.01 mm/s. The refined grain structure was not only due to dynamic recrystallization, but also the synergistic pinning effects from nano-TiCp as well as precipitated MgZn2 and α-Mn particles. The superior ultimate tensile strength (∼410.3 MPa), yield strength (∼384.5 MPa) and elongation to failure (∼4%) were obtained in the nanocomposite extruded at the slowest speed (0.01 mm/s) and had the potential to serve as a candidate material in orthopaedic applications. The improved strength was mainly related to grain refinement, thermal expansion effects and Orowan strengthening. Grain refinement, in particular, contributed to the largest strengthening increment. High tensile toughness of ∼66.6 KJ mm−3 was achieved for the nanocomposite extruded at a speed of 1 mm/s. Further, it exhibited a high strain hardening rate, θ, at stage IV. The fracture surface exhibited abundant dimples and consistent with high ductility. Remnant coarse Ca2Mg6Zn3 particles acted as crack initiators under high applied stress in tension, leading to structural failure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
2. Strengthening of Mg based alloy through grain refinement for orthopaedic application
3. New Mg-Ca-Zn amorphous alloys: biocompatibility, wettability and mechanical properties10.1016/j.mtla.2020.100799 ↗
4. Microstructure and properties of biodegradable β-TCP reinforced Mg-Zn-Zr composites10.1016/S1003-6326(11)60786-3 ↗
5. Improving the mechanical properties and biocorrosion resistance of extruded Mg-Zn-Ca-Mn alloy through hot deformation10.1016/j.matchemphys.2019.06.010 ↗
6. Preparation and characterization of biodegradable Mg-Zn-Ca/MgO nanocomposites for biomedical applications10.1016/j.matchar.2018.06.028 ↗
7. Magnesium matrix nanocomposites for orthopedic applications: a review from mechanical, corrosion, and biological perspectives10.1016/j.actbio.2019.06.007 ↗
8. Microstructure, mechanical properties, in vitro degradation behavior and hemocompatibility of novel Zn-Mg-Sr alloys as biodegradable metals10.1016/j.matlet.2015.07.151 ↗
9. In vitro and in vivo biocompatibility of Mg-Zn-Ca alloy operative clip
10. Degradation of biodegradable implants: the influence of microstructure and composition of Mg-Zn-Ca alloys10.1016/j.jallcom.2018.09.346 ↗
11. Corrosion studies and microstructure of Mg-Zn-Ca alloys for biomedical applications10.1016/j.surfin.2018.11.011 ↗
12. Influence of Ca and Zn on the microstructure and corrosion of biodegradable Mg–Ca–Zn alloys10.1016/j.corsci.2015.01.027 ↗
13. The microstructure, texture and mechanical properties of extruded Mg-5.3Zn-0.2Ca-0.5Ce (wt%) alloy10.1016/j.msea.2014.10.028 ↗
14. Effects of gas produced by degradation of Mg–Zn–Zr Alloy on cancellous bone tissue10.1016/j.msec.2015.05.082 ↗
15. Homogenization-induced age-hardening behavior and room temperature mechanical properties of Mg-4Zn-0.5Ca-0.16Mn (wt%) alloy10.1016/j.matdes.2018.107554 ↗
16. Development of dilute Mg-Zn-Ca-Mn alloy with high performance via extrusion10.1016/j.jallcom.2016.01.195 ↗
17. Effect of microalloying with Ca on the microstructure and mechanical properties of Mg-6 mass%Zn alloys10.1016/j.matdes.2016.03.025 ↗
18. Effect of extrusion ratio on microstructure, texture and mechanical properties of indirectly extruded Mg-Zn-Ca alloy10.1016/j.msea.2013.01.052 ↗
19. Fabrication of biodegradable materials with high strength by grain refinement of Mg-0.3 at.% Ca alloys10.1016/j.matlet.2018.03.188 ↗
20. Microstructure, tensile properties and work hardening behavior of an extruded Mg-Zn-Ca-Mn magnesium alloy10.1007/s40195-020-01061-9 ↗
21. Effect of ultra-slow extrusion speed on the microstructure and mechanical properties of Mg-4Zn-0.5Ca alloy10.1016/j.msea.2016.09.059 ↗
22. Achieving high-strength magnesium matrix nanocomposite through synergistical effect of external hybrid (SiC+TiC) nanoparticles and dynamic precipitated phase10.1016/j.jallcom.2018.09.030 ↗
23. A new semi-solid casting technique for fabricating SiC-reinforced Mg alloys matrix composites10.1016/j.compositesb.2016.02.019 ↗
24. Hierarchical magnesium nano-composites for enhanced mechanical response10.1016/j.actamat.2010.07.028 ↗
25. Magnesium matrix nanocomposites for orthopedic applications: a review from mechanical, corrosion, and biological perspectives10.1016/j.actbio.2019.06.007 ↗
26. Mechanical behavior of bioactive TiC nanocomposite thin films10.4028/www.scientific.net/MSF.729.296 ↗
27. Microstructure and tensile properties of SiC nanoparticles reinforced magnesium matrix composite prepared by multidirectional forging under decreasing temperature conditions10.1016/j.msea.2015.05.030 ↗
28. Microstructure and mechanical properties of SiCp/Mg-Al-Zn composites containing Mg17Al12 phases processed by low-speed extrusion10.1016/j.msea.2014.05.062 ↗
29. Fabrication of nano-SiC particulate reinforced Mg-8Al-1Sn composites by powder metallurgy combined with hot extrusion10.1007/s11665-016-2326-7 ↗
30. Hot deformation behavior of in-situ nanosized TiB2 particulate reinforced AZ91 Mg matrix composite10.1016/j.jallcom.2019.05.244 ↗
31. Fabrication of biodegradable magnesium matrix composite with ultrafine grains and high strength by adding TiC nanoparticles to Mg-1.12Ca-0.84Zn-0.23Mn (at.%) alloy10.1016/j.msec.2019.110360 ↗
32. Effects of Ca/Al ratio and extrusion process on Mg-Al-Ca alloys to produce a high toughness in-situ composite10.1080/14786435.2018.1508898 ↗
33. Hot deformation behavior and processing maps of SiC nanoparticles and second phase synergistically reinforced magnesium matrix composites10.3390/nano9010057 ↗
34. Microstructures and mechanical properties of SiCp/Mg-xAl-2Ca composites collectively influenced by SiCp and Al content10.1016/j.msea.2018.04.034 ↗
35. Adding TiC nanoparticles to magnesium alloy ZK60A for strength/ductility enhancement10.1155/2011/642980 ↗
36. Development of high performance magnesium matrix nanocomposites using nano-SiC particulates as reinforcement10.1007/s11665-015-1707-7 ↗
37. Work hardening behavior of Mg-based nano-composites strengthened by Al2O3 nano-particles10.1016/j.msea.2012.12.083 ↗
38. Microstructure, texture and mechanical properties of Mg-3.0Zn-0.2Ca alloys fabricated by extrusion at various temperatures10.1016/j.jallcom.2015.08.215 ↗
39. Processing, microstructure and mechanical properties of magnesium matrix nanocomposites fabricated by semisolid stirring assisted ultrasonic vibration10.1016/j.jallcom.2011.06.091 ↗
40. Microstructure stability of as-extruded bimodal size SiCp/AZ91 composite10.1016/j.msea.2014.07.105 ↗
41. High strength Mg-9Al serial alloy processed by slow extrusion10.1016/j.msea.2017.05.017 ↗
42. Friedrich · 2006
43. Christian · 2005
44. Effect of extrusion parameters on microstructure, texture and mechanical properties of Mg-1.38Zn-0.17Y-0.12Ca (at. %) alloy10.1016/j.matchar.2019.03.004 ↗
45. The synergy effect of fine and coarse grains on enhanced ductility of bimodal-structured Mg alloys10.1016/j.jallcom.2018.11.229 ↗
46. Dynamic precipitation, microstructure and mechanical properties of Mg-5Zn-1Mn alloy sheets prepared by high strain-rate rolling10.1016/j.matdes.2016.03.129 ↗
47. Enhanced properties of Mg-based nano-composites reinforced with Al2O3 nano-particles10.1016/j.msea.2009.05.001 ↗
48. Callister · 2008
49. Microstructure and strengthening mechanism of bimodal size particle reinforced magnesium matrix composite10.1016/j.compositesa.2012.03.007 ↗
50. Comparison between current models for the strength of particulate-reinforced metal matrix nanocomposites with emphasis on consideration of Hall-Petch effect10.1016/j.msea.2011.10.043 ↗
51. Microstructures and mechanical properties of Mg-Al-Ca alloys affected by Ca/Al ratio10.1016/j.msea.2015.03.100 ↗
52. Influence of the Al2Ca phase on microstructure and mechanical properties of Mg-Al-Ca alloys10.1016/j.jallcom.2015.06.060 ↗