Microstructure and constitutive model for flow behavior of AlSi10Mg by Selective Laser Melting
Source abstract
Abstract
Abstract This work is devoted to investigate the flow behavior and microstructure evolution of AlSi10Mg by additive manufacturing in hot deformation. Tensile test is carried out under different temperatures, i.e. 200 ∘ C, 250 ∘ C, 300 ∘ C, 350 ∘ C and 400 ∘ C, with various strain rates of 0.004/s, 0.002/s and 0.0004/s. Theoretically, the modified Arrhenius-type model of additive manufacturing materials at high temperature is established. Experimentally, scanning electron microscope and optical microscope are used to analyze the mechanism of hot deformation. It is found that at 200 ∘ C both the dendritic eutectic Si and acicular eutectic Si precipitate, forming cellular structure and strengthening phases. And then, the acicular eutectic Si is partially dissolved into Al matrix, but there is no obvious growth of dendritic Si at 300 ∘ C. With the temperature increasing, the cellular structure and melt pool boundary gradually disappear. For 400 ∘ C temperature, like homogenization process, the precipitation of saturated solid solution forms the dispersed phase, and the stress-strain curve shows a weak hardening. Meanwhile, the statistical result shows that that the constitutive model agrees well with the experimental results at high temperature. This study may provide guidance for the improvement of additive manufacturing material properties by post-treatment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. 3D printing of Aluminium alloys: additive Manufacturing of Aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
2. Selective laser melting10.1002/latj.201290018 ↗
3. Effect of selective laser melting process parameters on the quality of Al alloy parts: powder characterization, density, surface roughness, and dimensional accuracy10.3390/ma11122343 ↗
4. Selective laser sintering/melting (SLS/SLM) of pure Al, Al–Mg, and Al–Si powders: effect of processing conditions and powder properties10.1016/j.jmatprotec.2013.03.009 ↗
5. Processing AlSi10Mg by selective laser melting: parameter optimisation and material characterisation
6. On the selective laser melting (SLM) of the AlSi10Mg alloy: process, microstructure, and mechanical properties
7. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSilOMg powder10.1016/j.actamat.2012.11.052 ↗
8. Selective laser melting of AlSi10Mg alloy: process optimisation and mechanical properties development10.1016/j.matdes.2014.09.044 ↗
9. Study on the selective laser melting of AlSi10Mg
10. The microstructure and mechanical properties of selectively laser melted AlSi10Mg: the effect of a conventional T6-like heat treatment10.1016/j.msea.2016.04.092 ↗
11. Comparative study of performance comparison of AlSi10Mg alloy prepared by selective laser melting and casting10.1016/j.jmst.2019.08.049 ↗
12. Crack initiation and early propagation behavior of AlSi10Mg (Cu) cast alloy under thermal fatigue
13. Roughness modeling of AlSi10Mg parts fabricated by selective laser melting10.1016/j.jmatprotec.2016.11.013 ↗
14. High-temperature mechanical properties of AlSi10Mg specimens fabricated by additive manufacturing using selective laser melting technologies (AM-SLM)10.1016/j.addma.2018.09.033 ↗
15. Quality evaluation of A357 cast aluminum alloy specimens subjected to different artificial aging treatment10.1016/j.matdes.2003.11.007 ↗
16. The microstructure and mechanical properties of unidirectionally solidified AlSi alloys10.1007/BF02385422 ↗
17. Alloying AlSi10Mg and Cu powders in laser single scan tracks, melt spinning, and laser powder bed fusion10.1016/j.jallcom.2019.153538 ↗
18. Influence of working environment and built orientation on the tensile properties of selective laser melted AlSi10Mg alloy10.1016/j.msea.2019.01.103 ↗
19. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
20. Microstructure and mechanical properties of Ti-6AL-4V manufactured by SLM10.4028/www.scientific.net/KEM.651-653.677 ↗
21. Effect of build orientation on mechanical properties and microstructure of Ti-6Al-4V manufactured by selective laser melting10.1007/s11661-019-05322-w ↗
22. The AlSi10Mg samples produced by selective laser melting: single track, densification, microstructure and mechanical behavior10.1016/j.apsusc.2017.02.215 ↗
23. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg10.1016/j.jmatprotec.2015.02.013 ↗
24. Mechanical properties of AlSi10Mg produced by selective laser melting10.1016/j.phpro.2012.10.059 ↗
25. Microstructure and mechanical properties of AlSi10Mg parts produced by the laser beam additive manufacturing (AM) technology10.1007/s13632-014-0168-y ↗
26. High temperature dynamic yielding in metastable Ti–6.8Mo–4.5F–1.5Al10.1016/S0921-5093(97)00800-9 ↗
27. Normalised model-based processing diagrams for additive layer manufacture of engineering alloys10.1016/j.actamat.2016.02.025 ↗
28. Flow behavior and processing map for hot deformation of W-1.5ZrO2 alloy10.1016/j.jallcom.2019.06.179 ↗
29. Constitutive modeling of high-temperature flow behavior of Al-0.62Mg-0.73Si aluminum alloy10.1007/s11665-016-1988-5 ↗
30. Aluminum die casting alloys: alloy composition, microstructure, and properties-performance relationships10.1179/imr.1995.40.6.221 ↗
31. A model for relationship between true stress and true strain of stable FCC metals
32. Evaluation of true stress-true strain relationship after local necking by stepwise tensile test10.2355/tetsutohagane1955.91.9_712 ↗
33. TRANSPORT THEORY, Chapter 4: the derivation of continuum description from transport equations
34. On the mechanism of hot deformation10.1016/0001-6160(66)90207-0 ↗
35. Flow behavior and processing map for hot deformation of ATI425 titanium alloy
36. Thermal deformation behavior and processing maps of 7075 aluminum alloy sheet based on isothermal uniaxial tensile tests10.1016/j.jallcom.2018.07.173 ↗
37. A comparative study on Johnson–cook, modified Johnson–cook, modified Zerilli–Armstrong and Arrhenius-type constitutive models to predict hot deformation behavior of TA210.1515/htmp-2019-0026 ↗
38. Constitutive modeling of dynamic flow behavior of Ti-5553 alloy10.1016/j.jallcom.2019.02.101 ↗
39. A comparative study on Johnson Cook, modified Zerilli–Armstrong and Arrhenius-type constitutive models to predict elevated temperature flow behaviour in modified 9Cr–1Mo steel10.1016/j.commatsci.2009.09.025 ↗
40. Role of melt pool boundary condition in determining the mechanical properties of selective laser melting AlSilOMg alloy10.1016/j.msea.2018.10.083 ↗
41. High-temperature tensile deformation behavior of hot rolled CrMnFeCoNi high-entropy alloy10.1016/j.jallcom.2017.09.293 ↗
42. An. , ”Dynamic recrystallization during hot compression in Al-Mg alloy10.1016/0956-716X(92)90050-O ↗
43. Dislocation refinement mechanism of high stacking fault energy 7003 Al alloy during ECAP deformation