Optimizing strength-ductility of laser powder bed fusion-fabricated Ti–6Al–4V via twinning and phase transformation dominated interface engineering
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Lutjering · 2007
2. Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
3. The crystallography and deformation modes of hexagonal close-packed metals10.1179/imr.1967.12.1.169 ↗
4. On the mechanistic basis of deformation at the microscale in hexagonal close-packed metals10.1098/rspa.2014.0881 ↗
5. Dynamically reversible shear transformations in a CrMnFeCoNi high-entropy alloy at cryogenic temperature10.1016/j.actamat.2022.117937 ↗
6. Deformation-induced martensitic transformation in a new metastable β titanium alloy10.1016/j.jallcom.2015.07.263 ↗
7. Stress-induced twinning of nanocrystalline hexagonal close-packed titanium in Ti-6Al-4V10.1016/j.matlet.2016.05.098 ↗
8. Enhancing strength and ductility via crystalline-amorphous nanoarchitectures in TiZr-based alloys10.1126/sciadv.abm2884 ↗
9. Cryoforged nanotwinned titanium with ultrahigh strength and ductility10.1126/science.abe7252 ↗
10. Deformation induced face-centered cubic titanium and its twinning behavior in Ti-6Al-4V10.1016/j.scriptamat.2016.03.018 ↗
11. Hierarchical {332}<113> twinning in a metastable β Ti-alloy showing tolerance to strain localization10.1080/21663831.2020.1745920 ↗
12. Complexion-mediated martensitic phase transformation in Titanium
13. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
14. Interface-Mediated twinning-induced plasticity in a fine hexagonal microstructure generated by additive manufacturing10.1002/adma.202105096 ↗
15. A comparison of the tensile, fatigue, and fracture behavior of Ti-6Al-4V and 15-5 PH stainless steel parts made by selective laser melting10.1007/s00170-013-5106-7 ↗
16. Ladani · 2021
17. Strain localization in Ti-6Al-4V Widmanstätten microstructures produced by additive manufacturing10.1016/j.matchar.2016.10.018 ↗
18. Effects of processing parameters on microstructure and mechanical property of selective laser melted Ti-6Al-4V10.1016/j.matdes.2011.09.051 ↗
19. Realizing superior ductility of selective laser melted Ti-6Al-4V through a multi-step heat treatment10.1016/j.msea.2020.140367 ↗
20. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti-6Al-4V10.1016/j.msea.2013.04.099 ↗
21. Anisotropy in the room-temperature deformation of α–β colonies in titanium alloys: role of the α–β interface10.1080/1478643032000158305 ↗
22. Controlling martensitic decomposition during selective laser melting to achieve best ductility in high strength Ti-6Al-4V10.1016/j.msea.2018.12.047 ↗
23. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
24. Coarsening of martensite with multiple generations of twins in laser additively manufactured Ti6Al4V10.1016/j.actamat.2021.116954 ↗
25. Room-temperature ductility of Ti-6Al-4V alloy with α′ martensite microstructure10.1016/j.msea.2010.10.070 ↗
26. Crack propagation and fracture toughness of Ti-6Al-4V alloy produced by selective laser melting
27. Effect of heating treatment on the microstructural evolution and dynamic tensile properties of Ti-6Al-4V alloy produced by selective laser melting10.1016/j.jmapro.2021.12.035 ↗
28. Simulation-informed laser metal powder deposition of Ti-6Al-4V with ultrafine α-β lamellar structures for desired tensile properties
29. Influence of α/β interface phase on the tensile properties of laser cladding deposited Ti-6Al-4V titanium alloy10.1016/j.jmst.2016.09.026 ↗
30. Selective laser melting produced Ti-6Al-4V: post-process BBHeat treatments to achieve superior tensile properties10.3390/ma11010146 ↗
31. Mechanical properties and deformation mechanisms of martensitic Ti-6Al-4V alloy processed by laser powder bed fusion and water quenching10.1016/j.msea.2022.142817 ↗
32. Introducing C phase in additively manufactured Ti-6Al-4V: a new oxygen-stabilized face-centred cubic solid solution with improved mechanical properties10.1016/j.mattod.2022.10.026 ↗
33. Ultrastrong nanotwinned titanium alloys through additive manufacturing10.1038/s41563-022-01359-2 ↗
34. Influence of lowering basal stacking fault energy on twinning behaviours10.1016/j.actamat.2022.118637 ↗
35. Martensitic transformations in Ti-6Al-4V (ELI) alloy manufactured by 3D Printing10.1016/j.matchar.2018.09.042 ↗
36. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
37. Mechanical anisotropy and strain rate dependency behavior of Ti6Al4V produced using E-beam additive fabrication10.1115/1.4027729 ↗
38. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
39. Tailoring hierarchical microstructures to improve the strength and plasticity of a laser powder bed fusion additively manufactured Ti-6Al-4V alloy
40. Shear-induced hexagonal close-packed to face-centered cubic phase transition in pure titanium processed by equal channel angular drawing10.1007/s10853-019-03430-x ↗
41. Rolling-induced face centered cubic titanium in hexagonal close packed titanium at room temperature
42. Stress-induced hexagonal close-packed to face-centered cubic phase transformation in commercial-purity titanium under cryogenic plane-strain compression10.1016/j.scriptamat.2013.05.038 ↗
43. Nishiyama · 2012
44. Generalized stacking fault energies and critical resolved shear stresses of random α-Ti-Al alloys from first-principles calculations10.1016/j.jallcom.2020.156314 ↗
45. Deformation behavior of HCP Ti-Al alloy single crystals10.1007/s11661-002-0153-y ↗
46. Rolling-induced face centered cubic titanium in hexagonal close packed titanium at room temperature
47. Deformation induced FCC lamellae and their interaction in commercial pure Ti10.1016/j.scriptamat.2018.11.037 ↗
48. Impurity and texture driven HCP-to-FCC transformations in Ti-X thin films during in situ TEM annealing and FIB milling10.1016/j.actamat.2019.11.047 ↗
49. Hydride or martensite? Identification of a new phase in cold-rolled hexagonal close-packed Ti10.1016/j.matchar.2020.110294 ↗
50. Ti and its alloys as examples of cryogenic focused ion beam milling of environmentally-sensitive materials10.1038/s41467-019-08752-7 ↗
51. Could face-centered cubic titanium in cold-rolled commercially-pure titanium only be a Ti-hydride?10.1016/j.scriptamat.2019.11.010 ↗