Microstructural evolution and martensitic transformation in FeCrV alloy fabricated via additive manufacturing
Source abstract
Abstract
Abstract FeCrV alloy (high-wear-resistance steel or HWS) has been extensively used in additive manufacturing for hardfacing and repairing owing to its excellent hardness, superior weldability, and wear resistance. This alloy must possess superior mechanical property under harsh environments, such as friction and wear, to facilitate its application in repairing gears and strengthening the surface of a die locally. HWS deposited by directed energy deposition was subjected to heat treatment by quenching and tempering (QT) to improve the mechanical property and investigate the influence of martensitic transformation. During the solidification of the molten pool, the as-deposited HWS exhibited compressive residual stress (−102 (±72) MPa) on the surface, resulting from martensitic transformation. In contrast, the surface of the heat-treated HWS (HT-HWS) had tensile residual stress (150 (±34) MPa), which was induced by released carbon from the matrix and decarburization at the surface. QT heat treatment precipitated spherical chromium carbide (W0·07Mo0·07Cr1·31V0·31Fe1·38C) and rod-like vanadium carbide (W0·07Mo0·08Cr0·48V0·56Fe1·08C) on the grain boundaries and nanosized-vanadium carbide on the martensite lath boundaries. During heat treatment, the austenite of the as-deposited HWS transformed into martensite, and only 4.80% of the austenite remained. Despite heat treatment, the dislocation density did not decrease because the martensitic transformation caused plastic deformation of the adjacent grains. In addition, the precipitation of fine carbide inhibited grain growth during the heat treatment. For these reasons, the hardness of the as-deposited HWS increased by 17% (i.e., from 659 (±18.7) HV to 773 (±3.33) HV), corresponding to the hardness of carburized SCM420 (774 (±4.31) HV). The tensile strength of the as-deposited HWS increased from 570.6 (±21.5) MPa to 848.1 (±47.7) MPa by removing the melt pool boundary and needle-shaped austenite which are the crack propagation paths of the QT-heat-treated alloy. The carbide that precipitated during heat treatment changed the fracture mechanism from intergranular with dimples to cleavage.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Evaluation of bending strength of carburized gears
2. Effects of slip ratio on damage and microcracks in carburized SCM420 steel under rolling contact fatigue10.4028/www.scientific.net/KEM.741.94 ↗
3. Crack repair welding by CMT brazing using low melting point filler wire for long-term used steam turbine cases of Cr-Mo-V cast steels10.1016/j.msea.2016.04.035 ↗
4. Solid-state additive manufacturing and repairing by cold spraying: a review10.1016/j.jmst.2017.09.015 ↗
5. Application of directed energy deposition-based additive manufacturing in repair10.3390/app9163316 ↗
6. Mechanical characteristics of a tool steel layer deposited by using direct energy deposition10.1007/s12540-017-6442-1 ↗
7. Effect of layer thickness setting on deposition characteristics in direct energy deposition (DED) process10.1016/j.optlastec.2016.07.001 ↗
8. Thermal and stress modeling of multi-material laser processing10.1016/S1359-6454(01)00312-3 ↗
9. A study on the mechanical properties of HWS (high wear resistance steel) powder material deposited by directed energy deposition process
10. The design of a semi-additive manufacturing shape using metal 3D printing for a partially strengthened mold based on a high-alloy tool steel powder10.1007/s12206-020-0907-8 ↗
11. Improvement of laser deposited high alloyed powder metallurgical tool steel by a post-tempering treatment10.1016/j.phpro.2012.10.053 ↗
12. Effects of heat treatment condition and counter materials on the wear behavior of laser direct energy deposited Fe-8Cr-3V-2Mo-2W alloy10.3365/KJMM.2020.58.10.680 ↗
13. A study on strengthening mechanical properties of a punch mold for cutting by using an HWS powder material and a DED semi-AM method of metal 3D printing10.3390/jmmp4040098 ↗
14. Mechanical properties of tool steels with high wear resistance via directed energy deposition10.3390/met9030282 ↗
15. Residual stress in metal additive manufacturing10.1016/j.procir.2018.05.039 ↗
16. Effects of cooling rate on precipitate evolution and residual stresses in Al-Si-Mn-Mg casting alloy10.1007/s12540-018-0094-7 ↗
17. ORSA Endüstriyel Malzemeler
18. Beausir · 2017
19. New generation X-Ray stress measurement using Debye ring image data by two-dimensional detection
20. Comparison of X-ray residual stress measurement values by cos α method and sin2 ψ method
21. Measurement of residual stress in arc welded lap joints by cosα X-ray diffraction method10.1016/j.jmatprotec.2016.12.021 ↗
22. On residual stress development, prevention, and compensation in metal additive manufacturing10.3390/ma13020255 ↗
23. Bending strength of tool steel preheated to various temperatures and layered by direct energy deposition10.1016/j.msea.2018.12.009 ↗
24. Microstructure evolution and mechanical stability of retained austenite in medium-Mn steel deformed at different temperatures10.3390/ma12183042 ↗
25. Effect of real-time cooling rate on microstructure in laser additive manufacturing10.1016/j.jmatprotec.2016.01.017 ↗
26. Numerical study of the effect of progressive solidification on residual stress in single-bead-on-plate additive manufacturing10.1016/j.addma.2020.101245 ↗
27. Rapid tooling by laser powder deposition: process simulation using finite element analysis10.1016/j.actamat.2005.05.003 ↗
28. In-situ observations of lattice parameter fluctuations in austenite and transformation to bainite10.1007/s11661-005-0002-x ↗
29. Bhadeshia · 2017
30. Effect of low transformation temperature weld filler metal on welding residual stress10.1179/136217110X12714217309614 ↗
31. Prediction of martensite start temperature in alloy steels with different grain sizes10.1007/s11661-013-1798-4 ↗
32. Modeling and Experimental verification of transient/residual stresses and microstructure formation of multi-layer laser aided DMD process10.1115/1.2194037 ↗
33. Residual stresses and dimensional changes related to the lattice parameter changes of heat-treated JIS SKD 11 tool steels10.2320/matertrans.M2014031 ↗
34. Mechanism for formation of the residual stresses from quenching10.1088/0965-0393/6/3/006 ↗
35. Characterization of microstructure and residual stress in a 3D H13 tool steel component produced by additive manufacturing10.1557/jmr.2014.190 ↗
36. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
37. Microstructure and properties of an as-deposited and heat treated martensitic stainless steel fabricated by direct laser deposition10.1016/j.jmapro.2016.12.014 ↗
38. Modeling the effect of solute drag on recovery and recrystallization during hot deformation of Nb microalloyed steels10.2355/isijinternational.50.239 ↗
39. Additive manufacturing of ultrafine-grained austenitic stainless steel matrix composite via vanadium carbide reinforcement addition and selective laser melting: formation mechanism and strengthening effect10.1016/j.msea.2019.01.008 ↗
40. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
41. Microstructure and mechanical characteristics of multi-layered materials composed of 316L stainless steel and ferritic steel produced by direct energy deposition10.1016/j.jallcom.2018.09.390 ↗
42. Evaluation of the microstructural changes in Cr-V ledeburitic tool steels depending on the Austenitization temperature
43. Comparison of maraging steel micro- and nanostructure produced conventionally and by laser additive manufacturing10.3390/ma10010008 ↗
44. Maalekian · 2007
45. The hardness of additively manufactured alloys10.3390/ma11112070 ↗
46. Deformation mechanisms and defect tolerance in the microstructure of 3D-printed alloys10.1557/jmr.2020.60 ↗