Gigacycle fatigue of high-strength steel caused by MnS inclusions
Source abstract
Abstract
Abstract Gigacycle fatigue tests were conducted on high-strength steels that contained large amounts of MnS and which had been subjected to different working ratios. Anisotropy was also investigated by fatigue testing in both the longitudinal and transverse directions. The fatigue strengths were positively correlated with higher working ratios, revealing that high working ratios improved fatigue strength. Anisotropy was also observed, indicating that the fatigue strengths in the longitudinal direction were higher than those in the transverse direction. The fracture mode was internal fractures, mostly originating from MnS inclusions. The MnS showed long slender shapes under high working ratios. The inclusion sizes were inversely correlated with working ratios, with small inclusion sizes seen under high working ratios. The inclusion sizes were smaller in the longitudinal direction than in the transverse direction. These results were analyzed by using a prediction derived in the previous study. The results showed the effect of working ratios to be explained by inclusion size. There was little difference between MnS and oxides in that both inclusions revealed almost identical effects when the inclusion sizes were comparable. Anisotropically, some other factor than inclusion size slightly affected the fatigue properties, reducing the fatigue strength in the transverse direction.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels · Fire effects on concrete materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Kanazawa · 1989
2. Murakami · 2002
3. Fatigue tests on rolled alloy steels made in electric and open-hearth furnaces
4. Fatigue strength characteristics of high strength steel10.1299/kikaia.55.45 ↗
5. Stepwise S-N curve and fish-eye failure in gigacycle fatigue10.1046/j.1460-2695.1999.00206.x ↗
6. S-N curve characteristics and subsurface crack initiation behaviour in ultra-long life fatigue of a high carbon-chromium bearing steel10.1046/j.1460-2695.2001.00459.x ↗
7. High-cycle rotating bending fatigue property in very long-life regime of high-strength steels10.1046/j.1460-2695.2002.00575.x ↗
8. Gigacycle fatigue properties of 1800 MPa class spring steels10.1111/j.1460-2695.2004.00737.x ↗
9. Very high cycle fatigue properties of bainitic high carbon-chromium steel under variable amplitude conditions10.1016/j.ijfatigue.2009.02.038 ↗
10. Statistical duplex S-N characteristics of high carbon chromium bearing steel in rotating bending in very high cycle regime10.1016/j.ijfatigue.2009.08.001 ↗
11. Internal friction and fatigue in metals at large strain amplitudes10.1121/1.1908595 ↗
12. ASM Handbook
13. Evaluation of giga-cycle fatigue properties of some maraging steels by intermittent ultrasonic fatigue testing10.1046/j.1460-2695.2002.00561.x ↗
14. Bathias · 2004
15. Recent developments in ultrasonic fatigue10.1111/ffe.12365 ↗
16. WES 1112 · 2017
17. Gigacycle fatigue properties for high-strength low-alloy steel at 100 Hz, 600 Hz, and 20 kHz10.1016/S1359-6462(01)01213-1 ↗
18. 1010-cycle fatigue properties of 1800 MPa-class JIS-SUP7 spring steel10.1046/j.1460-2695.2003.00661.x ↗
19. Gigacycle fatigue properties of hydrogen-charged JIS-SCM440 low-alloy steel under ultrasonic fatigue testing10.1007/s11661-010-0307-2 ↗
20. Gigacycle fatigue properties of Ti-6Al-4V alloy under tensile mean stress10.1016/j.msea.2014.01.019 ↗
21. Specimen size effects on gigacycle fatigue properties of high-strength steel under ultrasonic fatigue testing10.1016/j.scriptamat.2008.01.039 ↗
22. Notable size effects on very high cycle fatigue properties of high-strength steel10.1016/j.msea.2011.03.082 ↗
23. Gigacycle fatigue properties of double-melted SCM440 steel and size effects10.2355/isijinternational.54.1436 ↗
24. Fatigue crack propagation behaviour derived from S-N data in very high cycle regime10.1046/j.1460-2695.2002.00547.x ↗
25. Visualization of internal small fatigue crack growth10.1016/j.matlet.2013.09.015 ↗
26. Small internal fatigue crack growth rate measured by beach marks10.1016/j.msea.2016.09.109 ↗
27. A new model for predicting the gigacycle fatigue strength of high-strength steels10.1016/j.msea.2018.11.109 ↗
28. 1011 gigacycle fatigue properties of high-strength steel10.2355/isijinternational.ISIJINT-2020-212 ↗
29. 1997
30. Inclusion-controlled fatigue properties of 1800 MPa-class spring steels, Metal10.1007/s11661-004-0279-1 ↗
31. The effect of inclusion geometry according to forging ratio and metal flow direction on very high-cycle fatigue properties of steel bars10.1016/j.ijfatigue.2007.10.009 ↗
32. Factors influencing the mechanism of superlong fatigue failure in steels10.1046/j.1460-2695.1999.00187.x ↗
33. Mechanism of fatigue failure in ultralong life regime10.1046/j.1460-2695.2002.00576.x ↗