The effect of microstructure on the plastic strain localization and fatigue crack initiation in cast Mg–8Gd–3Y–0.5Zr alloy
Source abstract
Abstract
Abstract Strain-controlled fatigue tests were performed on a cast Mg–8Gd–3Y–0.5Zr (wt. %, GW83K) alloy to investigate the effect of microstructure on strain localization and fatigue crack initiation. The results show that, in T4 alloys, a large number of basal slips in individual grains and most grains in the bulk material are involved in plastic deformation and fatigue damage because persistent slip bands (PSBs) are dense and uniform. The interaction between dense PSBs and grain boundaries (GBs) occurs continuously along a wide range of GBs, resulting in uniform distribution of residual strains along GBs. The grain-level strain localizations within and among grains are effectively alleviated. In T6 alloys, however, due to the sparse and inhomogeneous PSBs, only a few basal slips in individual grains and only a few grains in the bulk material participate in plastic deformation and fatigue damage. The interaction sites between sparse PSBs and GBs is significantly limited, which leads to highly concentrated deformation at a few specific areas of the GBs. It results in high trans-granular strain localization in long range stretching across both grain interiors and GBs in short cycles. The strain localizations within and among grains are relatively aggravated. Moreover, the saturated strains of the T4 alloys are much larger than those of the T6 alloys. Therefore, under the same loading condition, it takes more cycles for T4 alloys, while fewer cycles for T6 alloys, to reach the saturation strains and initiate micro-cracks. In other words, the crack initiation life of T4 alloys is much longer than that of T6 alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Magnesium alloys development towards the 21(st) century
2. Avedesian · 1999
3. Fatigue of rare-earth containing magnesium alloys: a review10.1111/ffe.12198 ↗
4. Cyclic deformation of ultrafine-grained aluminum10.1016/j.actamat.2006.09.002 ↗
5. The evolution of crack-tip stresses during a fatigue overload event10.1016/j.actamat.2010.03.013 ↗
6. Shu · 2003 · 182
7. Plastic strain localization and fatigue micro-crack formation in Hastelloy X10.1016/j.msea.2012.10.072 ↗
8. A model of extrusions and intrusions in fatigued metals .1. Point-defect production and the growth of extrusions10.1080/01418618108239541 ↗
9. The physics of fatigue crack initiation10.1016/j.ijfatigue.2012.10.009 ↗
10. A physically based fatigue model for prediction of crack initiation from persistent slip bands in polycrystals10.1016/j.actamat.2010.09.036 ↗
11. Mughrabi · 1983 · 5
12. Microstructural mechanisms of cyclic deformation, fatigue crack initiation and early crack growth
13. Microstructural extremes and the transition from fatigue crack initiation to small crack growth in a polycrystalline nickel-base superalloy10.1016/j.actamat.2012.01.049 ↗
14. Localisation of plastic strain at the microstructurlal level in Hastelloy X subjected to monotonic, fatigue, and creep loading: the role of grain boundaries and slip transmission10.1080/09603409.2016.1152421 ↗
15. Suresh · 1998
16. Schijve · 2009
17. Cyclic slip irreversibilities and the evolution of fatigue damage10.1007/s11661-009-9839-8 ↗
18. Cyclic strain localisation, crack nucleation and short crack growth
19. Extrusions and intrusions in fatigued metals. Part 2. AFM and EBSD study of the early growth of extrusions and intrusions in 316L steel fatigued at room temperature10.1080/14786430902917624 ↗
20. Effect of ductile damage evolution in sheet metal forming: experimental and numerical investigations
21. Dependence of intergranular fatigue cracking on the interactions of persistent slip bands with grain boundaries10.1016/S1359-6454(02)00399-3 ↗
22. Microcracks in fatigued FCC polycrystals by interaction between persistent slip bands and grain boundaries10.1002/crat.2170220124 ↗
23. Misorientation measurements near grain boundary cracks after fatigue tests10.1007/BF02206406 ↗
24. The effects of grain size and heat treatment on the deformation heterogeneities and fatigue behaviors of GW83K magnesium alloys10.1016/j.msea.2019.03.063 ↗
25. Basal slip dominant fatigue damage behavior in a cast Mg-8Gd-3Y-Zr alloy10.1016/j.ijfatigue.2018.08.001 ↗
26. An experimental methodology to relate local strain to microstructural texture10.1063/1.3474902 ↗
27. The role of slip transmission on plastic strain accumulation across grain boundaries
28. Strain mapping near a triple junction in strained Ni-based alloy using EBSD and biaxial nanogauges10.1016/j.actamat.2011.01.051 ↗