journal article·2022-10Open access

Occurrence of dynamic strain aging in intercritically annealed low carbon high aluminum medium manganese steels

Shahroz Ahmed, Jani Penttilä, Jari Rämö, Mari Honkanen, Veli-Tapani Kuokkala, Olli Oja, Pasi Peura

Abstract

Medium manganese steel grades heat treated with the quench and partition (Q&P) treatment have shown promising results of strength and formability, but the number of studies on high aluminum medium manganese Q&P steels still remains rather limited. Consequently, this study investigates the mechanical properties, behavior and microstructures of a low carbon-high aluminum medium manganese (3%) steel after intercritical annealing and subsequent Q&P heat treatments with varying heat treatment parameters. Samples that were intercritically annealed above 760 °C showed an ultimate tensile strength (UTS) of around 1500 MPa with uniform elongation values of approximately 10%. On the other hand, the samples annealed at 740 °C showed somewhat lower UTS values (in the range of 1000 … 1200 MPa) but much higher uniform and total elongations, i.e., considerably improved formability. However, the stress-strain curves of the samples annealed at 740 °C showed rather severe serrations that can be connected to the dynamic strain aging (DSA) phenomena, which limits the usability of the steel especially in applications where good surface quality of the deformed (sheet) is required. Therefore, the main focus of this article is on the samples annealed at temperatures close to A1, where DSA serrations tend to appear. The evidence gathered from these investigations leads to the conjecture that the DSA serrations are due to the free carbon and nitrogen originating from the dissolution of M(C,N) and M2(C,N) type carbides, which were formed during the intercritical annealing at temperatures producing less than 50% of the austenite phase. Other reasons for the occurrence of DSA in the current test materials can be the scarcity of martensite and the morphology of the retained austenite.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. The role of transformation-induced plasticity in the development of advanced high strength steels10.1002/adem.201701083 ↗
2. The “quenching and partitioning” process: background and recent progress10.1590/S1516-14392005000400010 ↗
3. Carbon partitioning into austenite after martensite transformation10.1016/S1359-6454(03)00059-4 ↗
4. Speer · 2003 · 505
5. Analysis of microstructure evolution in quenching and partitioning automotive sheet steel10.1007/s11661-011-0869-7 ↗
6. Microstructure development and mechanical properties of quenching and partitioning (Q&P) steel and an incorporation of hot-dipping galvanization during Q&P process10.1016/j.msea.2013.08.021 ↗
7. Austenite stabilization through manganese enrichment10.1016/j.scriptamat.2010.09.040 ↗
8. Quenching and partitioning of CMnSi steels containing elevated manganese levels10.1002/srin.201100318 ↗
9. Comparative study on microstructure and mechanical properties of a C-Mn-Si steel treated by quenching and partitioning (Q&P) processes after a full and intercritical austenitization10.1016/j.msea.2016.12.026 ↗
10. Stability of retained austenite through a combined intercritical annealing and quenching and partitioning (IAQP) treatment10.1007/s40195-015-0217-9 ↗
11. Effect of intercritical annealing on microstructural evolution and properties of quenched & partitioned (Q&P) steels10.1007/s11665-016-1985-8 ↗
12. Quenching and partitioning of multiphase aluminum-added steels10.3390/met9030373 ↗
13. Crystallography and mechanical properties of intercritically annealed quench and partitioned high-aluminum steel10.1016/j.matchar.2018.12.004 ↗
14. Application of quenching and partitioning processing to medium Mn Steel10.1007/s11661-014-2657-7 ↗
15. Microstructure evolution during high-temperature partitioning of a medium-Mn quenching and partitioning steel10.1016/j.mtla.2019.100492 ↗
16. Interaction of carbon partitioning, carbide precipitation and bainite formation during the Q&P process in a low C steel10.1016/j.actamat.2015.11.032 ↗
17. Investigation of Portevin-Le Chatelier band strain and elastic shrinkage in al-based alloys associated with Mg Contents10.1016/j.jmst.2016.05.012 ↗
18. Characterization of localized plastic deformation behaviors associated with dynamic strain aging in pipeline steels using digital image correlation10.1016/j.ijplas.2019.07.010 ↗
19. Gorbatenko · 2017 · 62 · 395
20. Serrated plastic flow10.1007/BF02743993 ↗
21. The Portevin–Le Chatelier effect: a review of experimental findings10.1088/1468-6996/12/6/063001 ↗
22. Explanation of the PLC effect in advanced high-strength medium-Mn steels. A review10.3390/ma12244175 ↗
23. A note on the Portevin-Le Chatelier effect
24. A model for the Portevin-Le Chatelier effect in substitutional alloys10.1016/0001-6160(72)90028-4 ↗
25. Theory of the effect of dynamic strain aging on mechanical properties10.1002/pssa.2210300120 ↗
26. The strain dependence of static and dynamic strain-aging10.1016/0001-6160(82)90211-5 ↗
27. Theory of flow localisation due to dynamic strain ageing10.1016/0001-6160(88)90043-0 ↗
28. Dynamic strain aging of various steels10.1007/BF02647835 ↗
29. Dynamic strain ageing in iron alloys: the shielding effect of carbon10.1016/j.actamat.2016.04.018 ↗
30. Effect of cooling rate after hot rolling and of multistage strain aging on the drawability of low-carbon-steel wire rod10.1007/BF02670614 ↗
31. Dynamic strain aging and the wire drawing of low carbon steel rods10.2355/isijinternational.35.1532 ↗
32. Effects of dynamic strain aging on strain hardening behavior, dislocation substructure, and fracture morphology in a ferritic stainless steel10.1007/s11661-019-05574-6 ↗
33. Dynamic strain aging caused by a new Peierls mechanism at high-temperature in iron10.1016/j.scriptamat.2014.09.019 ↗
34. On the origin of dynamic strain aging in twinning-induced plasticity steels10.1016/j.actamat.2011.07.040 ↗
35. Temperature dependence of the flow stress of Fe-18Mn-0.6C-xAl twinning-induced plasticity steel10.1016/j.actamat.2013.07.042 ↗
36. Correlation between luder strain and retained austenite in TRIP-assisted cold rolled steel sheets10.1016/j.msea.2006.10.046 ↗
37. Study of dynamic strain aging in dual phase steel10.1016/j.msea.2012.02.050 ↗
38. Discontinuous strain-induced martensite transformation related to the Portevin-Le Chatelier effect in a medium manganese steel10.1016/j.scriptamat.2017.01.022 ↗
39. Kinematic and thermal characteristics of Lüders and Portevin-Le Châtelier bands in a medium Mn transformation-induced plasticity steel10.1016/j.actamat.2016.10.069 ↗
40. Interactions of negative strain rate sensitivity, martensite transformation, and dynamic strain aging in 3rd generation advanced high-strength steels10.1016/j.msea.2019.03.042 ↗
41. Coincidence of strain-induced TRIP and propagative PLC bands in Medium Mn steels10.1016/j.msea.2017.08.042 ↗
42. The effects of the initial martensite microstructure on the microstructure and tensile properties of intercritically annealed Fe-9Mn-0.05C steel10.1016/j.actamat.2014.07.005 ↗
43. Microscopic strain partitioning in Lüders band of an ultra fine-grained medium Mn steel10.1016/j.msea.2019.138050 ↗
44. Portevin-Le Chatelier effect in aluminium- magnesium alloys10.2320/matertrans1960.10.429 ↗
45. A new type of stress-strain curve and the Portevin-Le Chatelier effect in Au (14 at.% Cu)10.1016/0001-6160(72)90029-6 ↗
46. Dynamic strain aging phenomena and tensile response of medium-Mn TRIP Steel10.1007/s11661-018-4481-y ↗
47. Influence of temperature and strain rate on the nature of serrations observed in a 15Cr-15Ni-2.2Mo-Ti modified austenitic stainless steel during tensile testing10.2320/matertrans1989.33.1040 ↗
48. A kinetics model for martensite transformation in plain carbon and low-alloyed steels10.1007/s11661-011-0872-z ↗
49. Determination of Ms temperature in steels: a Bayesian neural network model10.2355/isijinternational.42.894 ↗
50. Quenching and partitioning martensite-A novel steel heat treatment
51. Retained austenite and its measurement by X-ray diffraction
52. Effect of alloying additions on the lattice parameter of austenite
53. The effect of morphology on the stability of retained austenite in a quenched and partitioned steel10.1016/j.scriptamat.2012.11.003 ↗
54. On the characteristics of Portevin–Le Chatelier bands in cold-rolled 7Mn steel showing transformation-induced plasticity10.1016/j.ijplas.2018.01.010 ↗
55. Austenite stability effects on tensile behavior of manganese-enriched-austenite transformation-induced plasticity steel10.1007/s11661-011-0687-y ↗
56. Austenite stability and heterogeneous deformation in fine-grained transformation-induced plasticity-assisted steel10.1016/j.scriptamat.2013.02.026 ↗
57. Multistage serrated flow behavior of a medium-manganese high-carbon steel10.1007/s42243-019-00343-6 ↗
58. Serrated yielding in 9Cr-1Mo ferritic steel10.1179/026708399101506580 ↗
59. Plastic instability at elevated temperatures in a TRIP-assisted steel10.1016/j.matdes.2016.01.113 ↗
60. Effect of the intercritical annealing temperature on the mechanical properties of 10 Pct Mn multi-phase steel10.1007/s11661-014-2449-0 ↗
61. Measurement of dynamic strain aging in pearlitic steels by tensile test10.2355/isijinternational.43.428 ↗