Fatigue crack growth behavior of a nanocrystalline low Young's modulus β-type Ti–Nb alloy
Source abstract
Abstract
Low Young's modulus β-type titanium alloys, such as the Ti–45Nb alloy, with elastic properties close to that of human bone containing non-toxic elements are very desirable for load bearing implants. Their relatively low hardness and strength can be significantly increased by severe plastic deformation (SPD) methods, for example high pressure torsion (HPT). To gain a better understanding of the fatigue characteristics, the fatigue crack growth (FCG) behavior of Ti–45Nb was investigated in various microstructural states (as-received, HPT-deformed, HPT + cold-rolled, HPT + heat-treated). Compact tension (CT) specimens with different crack orientations were tested at different load ratios under tension-tension loading. The microstructure of the HPT and HPT + cold-rolled material shows highly elongated grains parallel to the principal deformation direction with grain sizes in the nanocrystalline regime. Compared to the majority of studies on FCG of SPD-processed materials this titanium alloy exhibits a remarkably weak anisotropy in the FCG-behavior in all material states but especially in the HPT and the cold-rolled state. This is mainly attributed to the transcrystalline fracture mode. The threshold of fatigue crack growth was found to decrease with increasing load ratio. This is related to a lower contribution of plasticity-induced crack closure at higher load ratios.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Microstructure and mechanical properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Ti based biomaterials, the ultimate choice for orthopaedic implants – a review10.1016/j.pmatsci.2008.06.004 ↗
2. Development of low rigidity β -type titanium alloy for biomedical applications10.2320/matertrans.43.2970 ↗
3. Development of new metallic alloys for biomedical applications10.1016/j.actbio.2012.06.037 ↗
4. Metabolism and possible health effects of aluminum
5. Titanium - the material of choice?10.1111/j.1600-0757.1998.tb00119.x ↗
6. Metal-induced developmental toxicity in mammals: a review10.1080/15287399409531868 ↗
7. Ultrasonic wave propagation in human cortical bone - II. Measurements of elastic properties and microhardness10.1016/0021-9290(76)90089-0 ↗
8. A continuous wave techique for the measurement of the elastic properties of cortical bone10.1016/0021-9290(84)90029-0 ↗
9. Stress analysis of the proximo-medial femur total hip replacement10.1016/0141-5425(90)90020-N ↗
10. Role of loads and prosthesis material properties on the mechanics of the proximal femur after total hip arthroplasty10.1002/jor.1100100314 ↗
11. Functional adaptation and ingrowth of bone vary as a function of hip implant stiffness10.1016/S0021-9290(98)00096-7 ↗
12. Titanium-Based biomaterials for preventing stress shielding between implant devices and bone10.1155/2011/836587 ↗
13. Biocompatibility of β-stabilizing elements of titanium alloys10.1016/j.biomaterials.2004.01.021 ↗
14. Titanium alloys in total joint replacement — a materials science perspective10.1016/S0142-9612(97)00146-4 ↗
15. The use of titanium for medical applications in the USA10.1016/0921-5093(96)10243-4 ↗
16. The bone tissue compatibility of a new Ti-Nb-Sn alloy with a low Young's modulus10.1016/j.actbio.2011.02.008 ↗
17. Beta Ti alloys with low young's modulus10.2320/matertrans.45.2776 ↗
18. Elastic constants of single crystalline β-Ti 70 Nb 3010.1016/j.scriptamat.2011.10.039 ↗
19. Mechanical properties, structural and texture evolution of biocompatible Ti-45Nb alloy processed by severe plastic deformation10.1016/j.jmbbm.2016.04.042 ↗
20. Surface treatment, corrosion behavior, and apatite-forming ability of Ti-45Nb implant alloy10.1002/jbm.b.32836 ↗
21. Deformation-induced ω-phase transformation in a β-type titanium alloy during tensile deformation10.1016/j.scriptamat.2016.10.036 ↗
22. ScienceDirect Microstructural evolution of precipitation-hardened b -type titanium alloy through high-pressure torsion10.1016/j.actamat.2014.07.041 ↗
23. Improvement in fatigue strength of biomedical β-type Ti-Nb-Ta-Zr alloy while maintaining low young's modulus through optimizing ω-phase precipitation10.1007/s11661-011-0860-3 ↗
24. Ultrafine grained titanium for biomedical applications : an overview of performance10.1016/j.jmrt.2013.07.003 ↗
25. Influence of testing orientation on mechanical properties of Ti45Nb deformed by high pressure torsion10.1016/j.matdes.2016.10.035 ↗
26. Influence of annealing on microstructure and mechanical properties of ultra fine-grained Ti45Nb10.1016/j.matdes.2019.107864 ↗
27. Materials Characterization Microstructural study of Ti-45Nb alloy before and after HPT processing using experimental and ab initio data mining approach10.1016/j.matchar.2020.110635 ↗
28. Developing biomedical nano-grained β-type titanium alloys using high pressure torsion for improved cell adherence10.1039/C5RA23454A ↗
29. Nanocrystalline β -Ti alloy with high hardness, low Young's modulus and excellent in vitro biocompatibility for biomedical applications10.1016/j.msec.2013.04.044 ↗
30. Grain refinement effect on the Ti-45Nb alloy electrochemical behavior in simulated physiological solution10.1016/j.surfcoat.2021.127609 ↗
31. Improved fatigue properties with maintaining low Young's modulus achieved in biomedical beta-type titanium alloy by oxygen addition10.1016/j.msea.2017.07.078 ↗
32. Improvement in fatigue characteristics of newly developed beta type titanium alloy for biomedical applications by thermo-mechanical treatments10.1016/j.msec.2004.12.007 ↗
33. Fatigue failure of metallic biomaterials
34. Technical parameters affecting grain refinement by high pressure torsion10.3139/146.110224 ↗
35. Use of fatigue specimens precracked in compression for measuring threshold values and crack growth10.1520/JTE12641J ↗
36. Revisiting fatigue crack growth in various grain size regimes of Ni10.1016/j.msea.2015.08.071 ↗
37. A systematic comparison of on-axis and off-axis transmission Kikuchi diffraction10.1016/j.ultramic.2017.12.017 ↗
38. Microstructure and texture evolution during the drawing of tungsten wires10.1016/j.engfracmech.2009.02.012 ↗
39. The effect of heat treatments on pure and potassium doped drawn tungsten wires: Part II – fracture properties10.1016/j.msea.2018.09.029 ↗
40. Fatigue of aluminium-lithium alloys10.1179/imr.1992.37.1.153 ↗
41. On generating fatigue crack growth thresholds10.1016/S0142-1123(02)00066-X ↗
42. The effect of microstructure and environment on fatigue crack closure of 7475 aluminum alloy10.1007/BF02644980 ↗
43. Mechanisms of slow fatigue crack growth in high strength aluminum alloys : role of microstructure and environment10.1007/BF02645122 ↗
44. Abnormal da/dN - ΔK curves: new failure mode with Ti - alloys10.1002/mawe.19970280204 ↗
45. Influence of cold rolling on the fatigue crack growth behavior of tungsten10.1016/j.msea.2021.140791 ↗
46. Suresh · 1998
47. Crack extension by alternating shear10.1016/0013-7944(70)90008-1 ↗
48. Coarse slip model of fatigue10.1016/0001-6160(69)90099-6 ↗
49. Crack propagation in high stress fatigue
50. Rate of growth of fatigue cracks calculated from the theory of infinitesimal dislocations distributed on a plane10.1007/BF00183823 ↗
51. Fatigue crack growth anisotropy in ultra fine-grained iron10.1016/j.actamat.2016.12.059 ↗
52. Threshold and effective threshold of fatigue crack propagation in ARMCO iron I : the influence of grain size and cold working10.1016/0921-5093(91)90671-9 ↗
53. Plastic strain triggers structural instabilities upon cyclic loading in ultrafine-grained nickel10.1016/j.actamat.2020.08.049 ↗
54. Fatigue crack closure: a review of the physical phenomena10.1111/ffe.12578 ↗
55. Simultaneous enhancement of strength and fatigue crack growth behavior of nanocrystalline steels by annealing10.1016/j.scriptamat.2017.05.051 ↗
56. The ductile to brittle transition of ultrafine-grained Armco iron : an experimental study10.1007/s10853-010-4635-9 ↗
57. A simple calculation of da/dN - ΔK in the near-threshold regime and above10.1007/BF00015777 ↗
58. Fatigue crack growth thresholds — the influence of Young ’ s modulus and fracture surface roughness10.1016/S0142-1123(98)00034-6 ↗
59. Dislocation modelling of fatigue cracks: an overview10.2320/matertrans.42.2 ↗
60. Mechanical reasons for plasticity-induced crack closure under plane strain conditions10.1046/j.1460-2695.1998.00131.x ↗
61. Plasticity-induced crack closure under plane-strain conditions in the near-threshold regime10.1080/01418610208240442 ↗
62. Threshold and effective threshold of fatigue crack propagation in ARMCO iron II: the influence of environment10.1016/0921-5093(91)90672-A ↗