Abstract
Wire arc additive manufacturing (WAAM) offers a cost-effective route for producing large, customised Ti-6Al-4V airframe components, yet the influence of heat treatments and process conditions on fatigue life remains unclear. This study examines how fatigue performance is shaped by standard additive manufacturing heat treatments (SR, STA, HIP, annealing) and key process parameters, including nozzle to workpiece distance and shielding atmosphere. STA refined the microstructure and increased strength but produced little improvement in fatigue life, while SR had negligible effects due to already low residual stresses in the as-machined state. In contrast, annealed specimens built with a more optimal nozzle to workpiece distance showed improved fatigue life despite lower yield strength, driven by high relative density (>99.99 percent) and greater ductility. HIP produced full densification and the best fatigue performance. Poor shielding reduced relative density and degraded fatigue resistance, despite strengthening from diffused oxygen. Fractography revealed that fatigue cracks initiated at sharp notches around clustered gas pores, where high stress concentrations accelerated crack coalescence and ligament rupture. Overall, the results demonstrate that clustered porosity, not microstructural refinement or strength alone, governs fatigue life in WAAM Ti-6Al-4V, highlighting the need to control pore nucleation and growth for reliable aerospace use.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (82)
Show source-provided references
1. The Additive Manufacturing (AM) of titanium alloys10.1016/j.mprp.2016.12.062 ↗
2. A review on biomedical titanium alloys: recent progress and prospect10.1002/adem.201801215 ↗
3. Galvanic corrosion protection of Al-alloy in contact with carbon fibre reinforced polymer through plasma electrolytic oxidation treatment10.1038/s41598-022-08727-7 ↗
4. Metal additive manufacturing in aerospace: a review
5. Improving arc stability during wire arc additive manufacturing of thin-walled titanium components10.1016/j.jmapro.2021.03.033 ↗
6. Microstructure of interpass rolled wire + arc additive manufacturing Ti-6Al-4V components10.1007/s11661-015-3172-1 ↗
7. Wire + Arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
8. Wire arc additive manufacturing Ti6Al4V aeronautical parts using plasma arc welding: analysis of heat-treatment processes in different atmospheres10.1016/j.jmrt.2020.11.012 ↗
9. Laser metal deposition of Ti6Al4V—A brief review10.3390/app10030764 ↗
10. Study on arc welding processes for high deposition rate additive manufacturing10.1016/j.procir.2017.12.095 ↗
11. Melt-based additive manufacturing of refractory metals and alloys: experiments and modeling10.1016/j.jmrt.2025.05.207 ↗
12. Influence of deposition strategy on the microstructure and fatigue properties of laser metal deposited Ti-6Al-4V powder on Ti-6Al-4V substrate
13. A review on the fatigue behavior of Ti-6Al-4V fabricated by electron beam melting additive manufacturing10.1016/j.ijfatigue.2018.09.022 ↗
14. Multi-mode fatigue life prediction using machine learning inspired by damage physics10.1016/j.ijmecsci.2025.110723 ↗
15. As-Fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
16. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
17. Influence of position and laser power on thermal history and microstructure of direct laser fabricated Ti–6Al–4V samples10.1179/174328405X21003 ↗
18. Material properties of Ti6Al4V parts produced by laser metal deposition10.1016/j.phpro.2012.10.056 ↗
19. Additive manufacturing and postprocessing of Ti-6Al-4V for superior mechanical properties10.1557/mrs.2016.215 ↗
20. Gushchina · 2022
21. Physics-based modeling of metal additive manufacturing processes: a review10.1007/s00170-024-14156-9 ↗
22. Phase transformations during cooling in α+β titanium alloys
23. Lutjering · 2007
24. Effect of deposition rate on microstructure and mechanical properties of wire arc additive manufacturing of Ti-6Al-4V components10.1007/s11771-021-4683-0 ↗
25. Optimising the mechanical properties of Ti-6Al-4V components produced by wire + arc additive manufacturing with post-process heat treatments10.1016/j.jallcom.2018.04.158 ↗
26. Fatigue of Ti-6Al-4V
27. 2015
28. Effects of solution-aging treatments on microstructure features, mechanical properties and damage behaviors of additive manufactured Ti–6Al–4V alloy10.1016/j.msea.2020.140380 ↗
29. Physicochemical state classification of heat-treated TC4 samples based on laser-induced breakdown spectroscopy (LIBS)
30. Defects in additive manufactured metals and their effect on fatigue performance: a state-of-the-art review10.1016/j.pmatsci.2020.100724 ↗
31. Residual stress effects on fatigue life of welded structures using LEFM10.1016/j.engfailanal.2008.06.017 ↗
32. Effect of residual stresses on fatigue crack growth: a numerical study based on cumulative plastic strain at the crack tip10.3390/ma15062156 ↗
33. Study of residual stress and microstructural evolution in as-deposited and inter-pass rolled wire plus arc additively manufactured inconel 718 alloy after ageing treatment
34. Residual stresses in wire-arc additive manufacturing – hierarchy of influential variables
35. Residual stress of as-deposited and rolled wire+arc additive manufacturing Ti–6Al–4V components10.1080/02670836.2016.1142704 ↗
36. Neutron diffraction measurements of residual stress in additively manufactured stainless steel10.1016/j.msea.2016.09.086 ↗
37. On the simulation scalability of predicting residual stress and distortion in selective laser melting10.1115/1.4038893 ↗
38. Residual stress distribution and its effect on fatigue crack path of laser powder bed fusion Ti6Al4V alloy10.3390/aerospace12020103 ↗
39. Influence of deposition strategies on residual stress in wire + Arc additive manufactured titanium Ti-6Al-4V10.3390/met12020253 ↗
40. Li · 2022
41. A critical review on the effects of process-induced porosity on the mechanical properties of alloys fabricated by laser powder bed fusion10.1007/s10853-022-06990-7 ↗
42. Interrupted fatigue testing with periodic tomography to monitor porosity defects in wire + arc additive manufactured Ti-6Al-4V
43. Criticality of porosity defects on the fatigue performance of wire + arc additive manufactured titanium alloy10.1016/j.ijfatigue.2019.01.017 ↗
44. The influence of porosity on fatigue crack initiation in additively manufactured titanium components10.1038/s41598-017-06504-5 ↗
45. Fatigue-damage initiation at process introduced internal defects in electron-beam-melted Ti-6Al-4V10.3390/met13020350 ↗
46. Influence of powder characteristics on formation of porosity in additive manufacturing of Ti-6Al-4V components10.1007/s11665-017-2796-2 ↗
47. Grain refinement of aluminium welds by Ti, TiB$$_2$$, and TiC filler wire inoculation10.1007/s00170-023-12199-y ↗
48. Anisotropy of fatigue crack growth in wire arc additive manufactured Ti-6Al-4V10.1016/j.msea.2017.10.064 ↗
49. Fatigue assessment of wire and Arc additively manufactured Ti-6Al-4V10.3390/met12050795 ↗
50. Effect of deposition strategies on fatigue crack growth behaviour of wire + arc additive manufactured titanium alloy Ti–6Al–4V10.1016/j.msea.2021.141194 ↗
51. Fatigue crack propagation behaviour in wire+arc additive manufactured Ti‐6Al‐4V: effects of microstructure and residual stress10.1016/j.matdes.2015.10.141 ↗
52. Fatigue of wire+arc additive manufactured Ti-6Al-4V in presence of process-induced porosity defects
53. A comparison between the residual stresses of Ti6Al4V and Ti-6Al-2Sn-4Zr-6Mo processed by laser powder bed fusion10.3390/ma18030689 ↗
54. Fitzpatrick · 2002
55. Determination of strain and stress fields by diffraction methods
56. Crystallographic structure of Ti-6Al-4V, Ti-HP and Ti-CP under high-pressure
57. Investigation of effective coating of the Ti–6Al–4V alloy and 316L stainless steel with graphene or carbon nanotubes with finite element methods10.1016/j.jmrt.2020.11.052 ↗
58. Influence of alloying elements content on high temperature properties of Ti-V-Cr and Ti-Al-V series titanium alloys: a JMatPro program calculation study10.1088/1742-6596/2639/1/012019 ↗
59. Neikter, M., et al. Microstructure Characterisation of Ti-6Al-4V from Different Additive Manufacturing Processes.
60. Residual stress mapping in heat-assisted additive manufacturing of IN 718: an X-Ray diffraction study10.1007/s11665-024-09269-x ↗
61. Influence of residual stresses on the fatigue crack growth from surface anomalies in a nickel-based superalloy10.1016/j.msea.2015.07.077 ↗
62. Recent progress of residual stress measurement methods: a review10.1016/j.cja.2019.10.010 ↗
63. Residual stress analysis in industrial parts: a comprehensive comparison of XRD methods10.1007/s10853-023-09069-z ↗
64. Estimation of residual stress relaxation in low alloy steel with different hardness during fatigue by in situ X-ray measurement10.1016/j.ijfatigue.2023.107989 ↗
65. Role of scanning strategy on residual stress distribution in Ti-6Al-4V alloy prepared by selective laser melting10.1016/j.ijleo.2018.05.128 ↗
66. Residual stress measurement using X-ray diffraction in friction stir-welded dissimilar titanium alloys10.3390/ma17071482 ↗
67. Evaluation of the compressive residual stress relaxation behavior by in situ X-ray stress measurement10.2355/isijinternational.ISIJINT-2021-566 ↗
68. In-situ XRD study on the effects of stress relaxation and phase transformation heat treatments on mechanical and microstructural behaviour of additively manufactured Ti-6Al-4V10.1016/j.msea.2021.141534 ↗
69. Defect structure process maps for laser powder bed fusion additive manufacturing
70. Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting10.1016/j.matdes.2016.05.070 ↗
71. On the mechanism of porosity formation during welding of titanium alloys10.1016/j.actamat.2012.02.035 ↗
72. Vacuum heat treatments of titanium porous structures
73. Visualisation and optimisation of shielding gas coverage during gas metal arc welding10.1016/j.jmatprotec.2017.11.048 ↗
74. The deformation and ageing of mild steel: II characteristics of the lüders deformation10.1088/0370-1301/64/9/302 ↗
75. Lutjering · 2009
76. Modeling the effect of porosity on ductile fracture of powder processed titanium alloy10.1016/S1359-6462(99)00178-5 ↗
77. Effect of porosity distribution on the strength and strain-to-failure of laser-powder bed fusion printed Ti–6Al–4V
78. Stress-based fatigue behavior of Ti–6Al–4V alloy with a discontinuous lamellar microstructure fabricated by thermomechanical powder consolidation10.1016/j.msea.2020.140085 ↗
79. Donachie · 2000
80. Callister · 1997
81. Die Theorie der Elastizität und die Bedürfnisse der Festigkeitslehre
82. Inglis · 1913 · vol. 55 · 219