Effects of finish rolling temperature on inverse fracture occurring during drop weight tear test of API X80 pipeline steels
Source abstract
Abstract
Abstract In this study, drop-weight tear tests (DWTT) were conducted on API X80 pipeline steels fabricated with different finish rolling temperatures in order to analyze abnormal fracture appearance, i.e ., inverse fracture, occurring in the region impacted by a hammer. Area fractions of fracture modes were measured from fractured DWTT specimens, and the measured data were analyzed in relation to microstructures, DWTT absorbed energy, and strain hardening of the hammer-impacted region. As the finish rolling temperature decreased, the volume fraction of fine-grained acicular ferrite increased, while that of large-grained upper bainite or granular bainite decreased. According to the DWTT results, the absorbed energy tended to increase with increasing volume fraction of acicular ferrite (with decreasing finish rolling temperature). A large area of inverse fracture of cleavage type was found in the hammer-impacted region of the steels fabricated with high finish rolling temperatures, but the area fraction of inverse fracture was reduced in the steels fabricated with low finish rolling temperatures. Since the area fraction of inverse fracture was closely related with strain hardening of the hammer-impacted region, it could be successfully reduced by lowering strain hardening and by promoting the formation of acicular ferrite via low finish rolling temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels · Metal Forming Simulation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Gräf · 2003 · 97
2. Denys · 2000 · 1
3. Pussegoda · 2000 · 239
4. 1996
5. O’Donoghue · Int. J. Pres. Ves. Pip. · 1997 · 70 · 1110.1016/S0308-0161(96)00012-9 ↗
6. Standard ASTM E23-02 · 2002
7. Ma · Met. Mater. Int. · 2010 · 16 · 42710.1007/s12540-010-0613-7 ↗
8. Iwasaki · Mech. Work Steel Process · 1975 · 13 · 294
9. G. Mannucci, D. Harris, Fracture properties of API X100 gas pipeline steels, Final Report, European Commission, Brussels, Belgium, 2002.
10. Hwang · Metall. Mater. Trans. A · 2005 · 36A · 37110.1007/s11661-005-0309-7 ↗
11. Koo · 2003 · 10
12. Kashimura · Met. Prog. · 1976 · 11 · 58
13. Nozaki · Sumitomo Search · 1981 · 26 · 76
14. Seifert · Mater. Test. · 1984 · 26 · 27710.1515/mt-1984-260808 ↗
15. Hwang · Mater. Sci. Eng. · 2004 · A368 · 1810.1016/j.msea.2003.09.075 ↗
16. McClure · J. Eng. Ind. · 1965 · 4 · 26510.1115/1.3670809 ↗
17. Ellwood · 2000
18. Standard ASTM E8m-09 · 2009
19. Bhadeshia · Mater. Sci. Eng. · 2004 · A378 · 3410.1016/j.msea.2003.10.328 ↗
20. Son · Met. Mater. Int. · 2010 · 16 · 35710.1007/s12540-010-0603-9 ↗
21. Krauss · ISIJ Int. · 1995 · 35 · 93710.2355/isijinternational.35.937 ↗
22. Diaz-Fuentes · Metall. Mater. Trans. A · 2003 · 34A · 250510.1007/s11661-003-0010-7 ↗
23. Ohomori · Met. Sci. · 1974 · 8 · 35710.1179/msc.1974.8.1.357 ↗
24. Kim · 2001 · 177
25. Yada · 1986 · 515
26. Matsumura · Trans. Iron Steel Inst. Jpn. · 1987 · 27 · 49210.2355/isijinternational1966.27.492 ↗
27. Yada · 1988 · 200
28. Lee · Metall. Mater. Trans. A · 1995 · 26A · 109310.1007/BF02670605 ↗
29. Wan · Met. Mater. Int. · 2010 · 16 · 86510.1007/s12540-010-1202-5 ↗
30. Kim · Mater. Sci. Eng. · 1990 · A129 · 3510.1016/0921-5093(90)90342-Z ↗
31. Tamura · 1988
32. Araki · 1992
33. Hollomon · Trans. AIME · 1945 · 162 · 268
34. Swift · J. Mech. Phys. Solids · 1952 · 1 · 110.1016/0022-5096(52)90002-1 ↗
35. Jeon · J. Korean Inst. Met. Mater. · 2001 · 39 · 1392
36. Bok · Met. Mater. Int. · 2010 · 16 · 18510.1007/s12540-010-0405-0 ↗