Influence of precipitation behavior on mechanical properties and hydrogen induced cracking during tempering of hot-rolled API steel for tubing
Source abstract
Abstract
Abstract Precipitation behavior and its effect on hydrogen embrittlement during tempering process of hot-rolled API steel designed with 0.4 wt% Cr and 0.25 wt% Mo were investigated. The base steel was normalized and then tempered at 650 °C for up to 60 min. The precipitation behavior of the examined steel was explored using transmission electron microscopy (TEM) analysis, and it was found that the precipitation sequence during tempering at 650 °C were as follows: MX+M 3 C→MX→MX+M 7 C 3 +M 23 C 6 . The change of particle fraction was measured by electrolytic extraction technique. At the early stage of tempering, the particle fraction greatly decreased due to dissolution of M 3 C particle, and increased after 10 min by the precipitation of M 7 C 3 and M 23 C 6 particles. The particle fraction showed a peak at 30 min tempering and decreased again due to the dissolution of M 7 C 3 particle. Vickers hardness tests of base steel and tempered samples were carried out, and then the hardness was changed by accompanying with the change of particle fraction. The sensitivity of hydrogen embrittlement was evaluated through hydrogen induced cracking (HIC) tests, and the results clearly proved that HIC resistance of tempered samples was better than that of base steel due to the formation of tempered martensite, and then the HIC resistance changed depending on the precipitation behavior during tempering, i.e., the precipitation of coarse M 23 C 6 and M 7 C 3 particles deteriorated the HIC resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Moon · Met. Mater. Int. · 2013 · 19 · 4510.1007/s12540-013-1008-3 ↗
2. Craig · Met. Trans. · 1980 · 11A · 179910.1007/BF02655095 ↗
3. Domizzi · Corros. Sci. · 2001 · 43 · 32510.1016/S0010-938X(00)00084-6 ↗
4. Moon · Met. Mater. Int. · 2012 · 18 · 61310.1007/s12540-012-4007-x ↗
5. Al-Mansour · Mater. Des. · 2009 · 30 · 408810.1016/j.matdes.2009.05.025 ↗
6. Park · Corros. Sci. · 2008 · 50 · 186510.1016/j.corsci.2008.03.007 ↗
7. Carneiro · Mater. Sci. Eng. A · 2003 · 357 · 10410.1016/S0921-5093(03)00217-X ↗
8. Moon · J. Nucl. Mater. · 2014 · 455 · 8110.1016/j.jnucmat.2014.04.048 ↗
9. Janovec · Mater. Sci. Eng. A · 1998 · 249 · 18410.1016/S0921-5093(98)00526-7 ↗
10. Shtansky · Acta Mater. · 2000 · 48 · 96910.1016/S1359-6454(99)00364-X ↗
11. Howell · Met. Trans. · 1979 · 10A · 121310.1007/BF02811976 ↗
12. Herbsleb · Corrosion · 1981 · 37 · 24710.5006/1.3621679 ↗
13. Takeda · Met. Trans. · 1981 · 12A · 125510.1007/BF02642339 ↗
14. Tsay · Corros. Sci. · 1997 · 39 · 116510.1016/S0010-938X(97)00015-2 ↗
15. Sha · Mater. Sci. Eng. A · 2013 · 585 · 21410.1016/j.msea.2013.07.055 ↗