The relationship between fracture mechanism and substructures of primary M7C3 under the hot compression process of self-healing hypereutectic high chromium cast iron
Source abstract
Abstract
Abstract Hypereutectic high chromium cast iron (HHCCI) possesses excellent thermal deformation potential, although it is difficult to deform at room temperature. It can release stress through the fracture of primary M7C3 (P-M), and the softened eutectic structure has a self-healing effect on the cracks to ensure the continuity of material. The morphology of the P-M is very irregular, with the distinct relative dimensions between P-MH ((001) plane//compression plane) and P-ML ((100) or (110) plane//compression plane). From TEM and SEM characterizations, the crack propagation site of P-ML is consistent with the interface of internal multidirectional stacking faults. The fractures of P-ML extend along the (100) (or (110)) and (001) planes during room-temperature and hot compression, respectively. This difference is contributed to the change of the stress state of P-ML by softened austenite and the improvement of the deformation ability of P-M itself. In addition, the anisotropic hardness and strain hardening behavior of P-ML and P-MH were also contributed to the anisotropy of internal stacking faults.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Variations in microstructure of high chromium cast irons and resultant changes in resistance to wear, corrosion and corrosive wear10.1016/j.wear.2008.11.025 ↗
2. Abrasion resistance of high Cr cast irons at an elevated temperature10.1016/S0043-1648(01)00665-2 ↗
3. Advanced chromium carbide-based hardfacings10.1016/j.surfcoat.2012.04.039 ↗
4. Comparative behaviour of cobalt and iron base hardfacing alloys10.1179/1743294411Y.0000000090 ↗
5. Effects of vanadium additive on structure property and tribological performance of high chromium cast iron hardfacing metal10.1016/j.surfcoat.2011.06.027 ↗
6. Effect of heat treatment on microstructure and mechanical properties of a Ti-bearing hypereutectic high chromium white cast iron10.1016/j.msea.2007.10.009 ↗
7. Wear behavior-hardness-microstructure relation of Fe-Cr-C and Fe-Cr-C-B based hardfacing alloys10.1016/j.matdes.2014.02.032 ↗
8. Effect of titanium on the morphology of primary M7C3 carbides in hypereutectic high chromium white iron10.1016/j.msea.2006.12.006 ↗
9. Correlation of microstructure with the wear resistance and fracture toughness of hardfacing alloys reinforced with complex carbides10.1007/s11661-000-0083-5 ↗
10. Effect of cerium modification on microstructure and properties of hypereutectic high chromium cast iron10.1016/j.msea.2014.02.080 ↗
11. Refinement and homogenization of M7C3 carbide in hypereutectic Fe-Cr-C coating by Y2O3 and TiC10.1016/j.matchar.2017.08.004 ↗
12. Refining effect of TiC on primary M7C3 in hypereutectic Fe-Cr-C harden-surface welding coating: experimental research and first principles calculation10.1016/j.jallcom.2016.08.133 ↗
13. Refinement mechanism of NbC by CeO2 in hypereutectic Fe-Cr-C hardfacing coating10.1016/j.jallcom.2018.08.162 ↗
14. The effect of nano-additives containing rare earth oxides on sliding wear behavior of high chromium cast iron hardfacing alloys10.1016/j.triboint.2016.06.041 ↗
15. Microstructure and crystallography of M7C3 carbide in chromium cast iron10.1016/j.matchemphys.2015.05.008 ↗
16. Fe-Cr-C hardfacing alloys for high-temperature applications10.1007/BF01117388 ↗
17. Texture, microstructure and microhardness evolution of a hot-rolled high chromium cast iron10.1016/j.msea.2010.06.036 ↗
18. The rolling/sliding wear response of conventionally processed and spray formed high chromium content cast iron at ambient and elevated temperature10.1016/S0043-1648(99)00053-8 ↗
19. Effects of temperature and strain rate on microstructure and mechanical properties of high chromium cast iron/low carbon steel bimetal prepared by hot diffusion-compression bonding10.1016/j.matdes.2014.06.067 ↗
20. Plastic deformation behaviors and hardening mechanism of M7C3 carbide10.1016/j.msea.2016.03.062 ↗
21. Optimization on mechanical properties of Fe7-xCrxC3 carbides by first-principles investigation10.1016/j.jallcom.2013.01.103 ↗
22. Thermodynamic investigations of Cr3C2 and reassessment of the Cr-C system10.1007/s11661-004-0273-7 ↗
23. Theoretical study on the stability and mechanical property of Cr7C310.1016/j.physb.2007.12.012 ↗
24. The electronic, mechanical properties and theoretical hardness of chromium carbides by first-principles calculations10.1016/j.jallcom.2011.02.009 ↗
25. Stacking faults in chromium, iron and vanadium mixed carbides of the type M7C310.1007/BF00752118 ↗
26. A re-examination of Westbrook's X-ray diffraction pattern for Cr7C310.1016/0025-5408(96)00045-1 ↗
27. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe-Mn-C alloys10.1016/j.msea.2004.01.059 ↗
28. Mechanism of twinning-induced grain boundary engineering in low stacking-fault energy materials10.1016/S1359-6454(99)00277-3 ↗
29. The conflicts between strength and toughness10.1038/nmat3115 ↗
30. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
31. Temperature dependence of stacking fault energy in close-packed metals and alloys10.1016/0025-5416(78)90194-5 ↗
32. Effect of (Fe,Cr)7C3 carbide orientation on abrasion wear resistance and fracture toughness10.1016/j.wear.2010.10.070 ↗
33. Effect of carbide orientation on abrasion of high Cr white cast iron10.1016/0043-1648(95)06682-9 ↗
34. 3D microstructure reconstruction of chrome carbide weld overlays10.1179/1362171814Y.0000000244 ↗
35. Mechanical properties and chemical bonding characteristics of Cr7C3 type multicomponent carbides10.1063/1.3532038 ↗
36. Tailoring the anisotropic mechanical properties of hexagonal M7X3 (M= Fe, Cr, W, Mo; X= C, B) by multialloying10.1016/j.actamat.2019.03.015 ↗
37. A crystallographic mechanism for fatigue crack propagation through grain boundaries10.1016/S1359-6454(00)00214-7 ↗
38. Comparison of fatigue cracking possibility along large-and low-angle grain boundaries10.1016/S0921-5093(00)00796-6 ↗
39. The composition dependence of stacking fault energy in austenitic stainless steels10.1007/BF02646563 ↗
40. Deformation-mechanism map for nanocrystalline metals by molecular-dynamics simulation10.1038/nmat1035 ↗
41. Effect of stacking fault energy on mechanism of plastic deformation in nanotwinned FCC metals
42. Fracture toughness of carbides in tool steels evaluated by nanoindentation10.1016/j.actamat.2007.03.028 ↗