Thermal stabilization of additively manufactured superalloys through defect engineering and precipitate interactions
Source abstract
Abstract
Abstract Laser peening (LP) is a mechanical surface modification technique capable of enhancing a treated material's resistance to surface-related failures through the introduction of deep, high-magnitude compressive residual stresses. Conventional LP enables material improvement in systems operating in ambient or low temperature ( 0.5Tm), LP-induced property enhancements and microstructural modifications encounter thermal degradation through dislocation annihilation, stress relaxation, and grain coarsening. Motivated by the need to retain critical material enhancements, a novel, modified LP technique was introduced and employed in this work, coined laser peening plus thermal microstructure engineering (LP + TME). This approach incorporates cyclic LP events with the inclusion of intermittent, 600 °C (0.55Tm) heat treatment steps in order to impart highly thermally stable microstructural modifications in additively manufactured (AM) Inconel 718. Microstructural and mechanical property evolution was evaluated through instrumented indentation and transmission electron microscopy (TEM). Surface-level compressive residual stresses were discovered to increase by as much as 84% from 167.13 MPa to over 300 MPa following LP + TME and a 350-h, 600 °C exposure. Surface and near-surface microhardness of samples subjected to LP + TME was observed to increase by 33% (to 630 HV) compared to untreated, as-built specimens even after exposure to 600 °C. Hardened zones were characterized by the presence of highly dense dislocation networks and precipitated strengthening phases. Both property enhancement and thermal stability were determined to be the result of various mechanisms at work, stemming from the synergistic combination of cyclic strain and thermal input. These include the facilitated nucleation of γ’’ and δ phases which aid in stabilizing LP-induced microstructures and provide material enhancements at high temperatures; precipitate-dislocation interactions including Orowan bypassing, Friedel cutting; and dislocation pinning effects. The results from this work are of significant interest as they are in contrast with what is typically expected at temperatures exceeding 0.5Tm meaning the technique outlined herein could offer a viable solution to overcoming obstacles preventing the widespread use of LP in critical, high temperature applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Treatment and Residual Stress · Additive Manufacturing Materials and Processes · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Improving creep properties of 7075 aluminum alloy by laser shock peening10.1016/j.surfcoat.2018.06.061 ↗
2. Laser and shot peening effects on fatigue crack growth in friction stir welded 7075-T7351 aluminum alloy joints10.1016/j.ijfatigue.2006.05.007 ↗
3. Evolution of a laser shock peened residual stress field locally with foreign object damage and subsequent fatigue crack growth10.1016/j.actamat.2014.09.032 ↗
4. Fatigue crack growth in laser-shock-peened Ti-6Al-4V aerofoil specimens due to foreign object damage10.1016/j.ijfatigue.2013.10.001 ↗
5. Effects of laser peening on stress corrosion cracking (SCC) of ANSI 304 austenitic stainless steel10.1016/j.corsci.2012.03.044 ↗
6. Stress corrosion cracking behavior of peened friction stir welded 2195 aluminum alloy joints10.1007/s11665-008-9303-8 ↗
7. A finite element study of thermal relaxation of residual stress in laser shock peened IN718 superalloy10.1016/j.ijimpeng.2011.02.006 ↗
8. Amrinder Singh Gill · 2012
9. Thermomechanical relaxation of residual stress in shot peened nickel base superalloy10.1179/mst.1994.10.11.947 ↗
10. Schulze · 2005
11. Analysis of shot-peening and residual stress relaxation in the nickel-based superalloy RR100010.1016/j.actamat.2013.01.031 ↗
12. Thermal relaxation of residual stress in laser shock peened Ti-6Al-4V alloy10.1016/j.surfcoat.2012.05.022 ↗
13. Dislocation dynamics IN deformation and recovery10.1139/p67-043 ↗
14. Effect of laser shock peening on wear behaviors of TC11 alloy at elevated temperature10.1016/j.optlastec.2018.07.070 ↗
15. Effect of laser shock peening on elevated temperature residual stress, microstructure and fatigue behavior of ATI 718Plus alloy10.1016/j.ijfatigue.2017.08.006 ↗
16. Effect of temperature on microstructure and residual stresses induced by surface treatments in Inconel 718 SPF10.1016/j.surfcoat.2018.02.094 ↗
17. The strengthening mechanism of a nickel-based alloy after laser shock processing at high temperatures10.1088/1468-6996/14/5/055010 ↗
18. On the influence of mechanical surface treatments-deep rolling and laser shock peening-on the fatigue behavior of Ti-6Al-4V at ambient and elevated temperatures10.1016/S0921-5093(03)00069-8 ↗
19. Effect of laser shock peening on elevated temperature residual stress, microstructure and fatigue behavior of ATI 718Plus alloy10.1016/j.ijfatigue.2017.08.006 ↗
20. Effect of laser shock peening on residual stress, microstructure and fatigue behavior of ATI 718Plus alloy10.1016/j.ijfatigue.2017.04.016 ↗
21. Prevéy · 2000
22. Laser peening: a tool for additive manufacturing post-processing
23. Warm laser shock peening driven nanostructures and their effects on fatigue performance in aluminium alloy 6160
24. Ultrahigh dense and gradient nano-precipitates generated by warm laser shock peening for combination of high strength and ductility10.1016/j.msea.2014.05.003 ↗
25. Effects of warm laser peening at elevated temperature on the low-cycle fatigue behavior of Ti6Al4V alloy10.1016/j.msea.2015.07.017 ↗
26. Fatigue performance improvement in AISI 4140 steel by dynamic strain aging and dynamic precipitation during warm laser shock peening10.1016/j.actamat.2010.10.032 ↗
27. Warm laser shock peening: new developments and process optimization10.1016/j.cirp.2011.03.115 ↗
28. [INVITED] A review: warm laser shock peening and related laser processing technique10.1016/j.optlastec.2015.09.014 ↗
29. Controlled precipitation by thermal engineered laser shock peening and its effect on dislocation pinning: multiscale dislocation dynamics simulation and experiments10.1016/j.actamat.2012.12.016 ↗
30. The mechanisms of thermal engineered laser shock peening for enhanced fatigue performance10.1016/j.actamat.2012.06.024 ↗
31. Ginsztler · 1998
32. The effect of interdendritic δ phase on the mechanical properties of Alloy 718 built up by additive manufacturing10.1016/j.matdes.2016.12.026 ↗
33. Aging effects on the microstructure and creep behavior of Inconel 718 superalloy10.1016/j.msea.2008.04.097 ↗
34. Coherency strengthening in Ni base alloys hardened by DO22 γ′ precipitates10.1007/BF02642938 ↗
35. Effects of annealing on microstructure and mechanical properties of nano-grained Ni-based alloy produced by severe cold rolling10.1016/j.msea.2015.06.043 ↗
36. Imaging and characterization of γ′ and γ″ nanoparticles in Inconel 718 by EDX elemental mapping and FIB-SEM tomography10.1016/j.matchar.2014.12.012 ↗
37. Relationship between the lattice constant of Υ phase and the content of δ phase, γ″ and γ′ phases in Inconel 71810.1016/S1359-6462(97)00064-X ↗
38. Neutron diffraction measurements of residual stress in additively manufactured stainless steel10.1016/j.msea.2016.09.086 ↗
39. Post-processing of the Inconel 718 alloy parts fabricated by selective laser melting: effects of mechanical surface treatments on surface topography, porosity, hardness and residual stress10.1016/j.surfcoat.2019.125136 ↗
40. Comparison of residual stresses in inconel 718 simple parts made by electron beam melting and direct laser metal sintering10.1007/s11661-014-2722-2 ↗
41. Residual stress in TI6AL4V objects produced by direct metal laser sintering
42. Characteristics of surface layers formed on inconel 718 by laser shock peening with and without a protective coating10.1016/j.jmatprotec.2015.06.026 ↗
43. Laser shock processing of aluminium alloys. Application to high cycle fatigue behaviour10.1016/0921-5093(95)10084-9 ↗
44. Effect of temperature on microstructure and residual stresses induced by surface treatments in Inconel 718 SPF10.1016/j.surfcoat.2018.02.094 ↗
45. Delta phase precipitation in inconel 71810.1016/j.matchar.2004.07.004 ↗
46. Effects of cold rolling on the precipitation kinetics and the morphology evolution of intermediate phases in Inconel 718 alloy10.1016/j.jallcom.2015.07.149 ↗
47. On the mechanism of serrated deformation in aged Inconel 71810.1016/S0921-5093(97)00005-1 ↗
48. Activation energy calculations for discontinuos yielding in inconel 718SPF10.1016/S0921-5093(00)01470-2 ↗
49. Effects of cold drawing ratio on δ phase precipitation behaviors of alloy 718 wire10.1007/BF03025928 ↗
50. Effect of serrated grain boundaries on the creep property of Inconel 718 superalloy10.1016/j.msea.2011.10.014 ↗
51. Hot tensile deformation behaviors and fracture characteristics of a typical Ni-based superalloy10.1016/j.matdes.2013.10.071 ↗
52. Characterization of strain-induced precipitation in inconel 718 superalloy10.1007/s11665-016-2154-9 ↗
53. δ Phase precipitation in Inconel 718 and associated mechanical properties10.1016/j.msea.2016.09.114 ↗
54. Effects of initial δ phase on hot tensile deformation behaviors and fracture characteristics of a typical Ni-based superalloy10.1016/j.msea.2014.01.029 ↗
55. Microstructure and phase stability in INCONEL alloy 740 during creep10.1016/j.scriptamat.2004.05.047 ↗
56. Consideration of Orowan strengthening effect in particulate-reinforced metal matrix nanocomposites: a model for predicting their yield strength10.1016/j.scriptamat.2005.12.017 ↗
57. Orowan strengthening and forest hardening superposition examined by dislocation dynamics simulations10.1016/j.actamat.2010.06.028 ↗
58. The Orowan mechanism in anisotropic crystals10.1080/14786437508229295 ↗
59. Precipitation and dispersion hardening
60. The deformation of plastically non-homogeneous materials10.1080/14786437008238426 ↗
61. Friedel · 1964