Correlation between microstructure evolution and mechanical response in a moderately low stacking-fault-energy austenitic Fe–Mn–Si–Al alloy during low-cycle fatigue deformation
Source abstract
Abstract
Abstract Through in-depth microstructural and mechanical characterization, a mechanism for low-cycle fatigue (LCF) deformation of an Fe-30.7Mn-4.3Si-1.8Al (in wt%) austenitic transformation-induced-plasticity (TRIP) steel at a total strain range of 2% was investigated. The LCF deformation of the steel was performed through two main deformation modes which were planar slip of Shockley partials, and e-martensitic transformation and its reverse transformation. The varying significance of each deformation mode as well as the relevance between the two modes determined the microstructures evolved during fatigue deformation and resulted in a four-stage cyclic hardening behavior. With increasing fatigue cycles, the LCF deformation was dominated sequentially by the multiplication of partial dislocations, development of slip bands, reversible e-martensitic transformation, and formation of more thick and crossed e-martensite along with enhancement of planar dislocation slip, thus generating the characteristic deformation stages of primary cyclic hardening, cyclic softening, cyclic saturation, and secondary cyclic hardening correspondingly. In general, the superior LCF resistance of the steel was attributed to appreciably high plasticity reversibility during the entire fatigue deformation which was caused by reversible planar dislocation slip and e-martensitic transformation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Twinning-induced plasticity (TWIP) steels10.1016/j.actamat.2017.06.046 ↗
2. High strength Fe–Mn–(Al, Si) TRIP/TWIP steels development - properties - application10.1016/S0749-6419(00)00015-2 ↗
3. A remarkable improvement of low-cycle fatigue resistance of high-Mn austenitic TWIP alloys with similar tensile properties: importance of slip mode10.1016/j.actamat.2016.07.034 ↗
4. Microstructure evolution associated with a superior low-cycle fatigue resistance of the Fe-30Mn-4Si-2Al alloy10.1007/s11661-015-3127-6 ↗
5. Effect of alloying composition on low-cycle fatigue properties and microstructure of Fe–30Mn–(6−x)Si–xAl TRIP/TWIP alloys10.1016/j.msea.2013.08.061 ↗
6. Effect of γ to ε martensitic transformation on low-cycle fatigue behaviour and fatigue microstructure of Fe–15Mn–10Cr–8Ni–xSi austenitic alloys10.1016/j.actamat.2015.12.002 ↗
7. Iron-based shape memory alloys for civil engineering structures: an overview10.1016/j.conbuildmat.2014.04.032 ↗
8. Designing Fe–Mn–Si alloys with improved low-cycle fatigue lives10.1016/j.scriptamat.2014.11.024 ↗
9. Development of Fe-based shape memory alloys associated with face-centered cubic-hexagonal close-packed martensitic transformations: Part III. Microstructures10.1007/BF02647328 ↗
10. On secondary variants formed at intersections of ε martensite variants10.1016/0956-7151(92)90187-J ↗
11. Formation of h.c.p. and f.c.c. twins in an Fe-Mn-Cr-Si-Ni alloy10.1016/0956-7151(94)90137-6 ↗
12. Characteristic features of shape memory effect and related transformation behavior in Fe-based alloys10.1016/S0921-5093(99)00290-7 ↗
13. Stacking faults and f.c.c. (γ) → h.c.p. (ε) transformation in 18/8-type stainless steel10.1016/0001-6160(72)90104-6 ↗
14. Observation of dislocations with a Burgers vector containing a ⟨c⟩ component in martensitic hcp ε Fe-17%Mn10.1016/j.scriptamat.2016.10.016 ↗
15. In situ microscopic observations of low-cycle fatigue-crack propagation in high-Mn austenitic alloys with deformation-induced ε-martensitic transformation10.1016/j.actamat.2016.04.042 ↗
16. Total pattern fitting for the combined size–strain–stress–texture determination in thin film diffraction10.1016/j.nimb.2009.09.053 ↗
17. Effect of deformation on damping capacity and microstructure of Fe–22%Mn–8%Co alloy10.2320/matertrans.46.1274 ↗
18. 2013
19. Shape memory effect and related phenomena in a microalloyed Fe-Mn-Si alloy10.1016/1044-5803(94)90091-4 ↗
20. Warren · 1969 · 251
21. Effect of stacking fault probability on γ–ε martensitic transformation and shape memory effect in Fe–Mn–Si based alloys10.1016/S1359-6454(97)00266-8 ↗
22. An X-ray diffraction line profile of cold-worked hexagonal alloys Zn-Ag: η and ε phase10.1007/BF02658675 ↗
23. Application of damping mechanism model and stacking fault probability in Fe–Mn alloy10.1016/j.matchar.2007.05.023 ↗
24. Mechanism of reversible transformation-induced plasticity of Fe–Mn–Si shape memory alloys10.1016/j.scriptamat.2008.06.030 ↗
25. Vibration mitigation by the reversible fcc/hcp martensitic transformation during cyclic tension–compression loading of an Fe–Mn–Si-based shape memory alloy10.1016/j.scriptamat.2006.02.013 ↗
26. A general mechanism of martensitic nucleation: Part I. General concepts and the FCC → HCP transformation
27. Effects of austenite grain size on ε martensitic transformation in Fe-15mass%Mn alloy10.2320/matertrans1989.34.489 ↗
28. Variation of stacking fault energy with austenite grain size and its effect on the MS temperature of γ→ε martensitic transformation in Fe–Mn alloy10.1016/S0921-5093(98)00994-0 ↗
29. Derivation and variation in composition-dependent stacking fault energy maps based on subregular solution model in high-manganese steels10.1007/s11661-009-0050-8 ↗
30. The influence of manganese content on the stacking fault and austenite/ε-martensite interfacial energies in Fe–Mn–(Al–Si) steels investigated by experiment and theory10.1016/j.actamat.2014.01.001 ↗
31. Thermodynamic modeling of the stacking fault energy of austenitic steels10.1016/j.actamat.2010.10.037 ↗
32. On the stress dependence of partial dislocation separation and deformation microstructure in austenitic stainless steels10.1016/S1359-6454(03)00117-4 ↗
33. In situ observations of the formation of martensite in stainless steel10.1016/0001-6160(79)90073-7 ↗
34. Inverse grain size effect on twinning in nanocrystalline TWIP steel10.1016/j.msea.2018.11.085 ↗
35. The influence of grain size on the strain-induced martensite formation in tensile straining of an austenitic 15Cr–9Mn–Ni–Cu stainless steel10.1016/j.msea.2013.04.107 ↗
36. Influence of original austenite grain size on tensile properties of a high-manganese transformation-induced plasticity (TRIP) steel10.1016/j.msea.2017.12.107 ↗
37. Effect of martensitic phase transformation and deformation twinning on mechanical properties of Fe–Mn–Si–AI steels10.1179/mst.1998.14.12.1213 ↗
38. Effect of austenite grain size in Fe-Mn alloys on ε martensitic transformation and their mechanical properties10.2320/jinstmet1952.60.2_141 ↗
39. Effect of Si on the reversibility of stress-induced martensite in Fe–Mn–Si shape memory alloys10.1016/j.actamat.2010.08.041 ↗