journal article·2018-05

Effect of travel speed and sub-β transus post deposition heat treatments on thin Ti-6Al-4V laser wire deposits

N. Chekir, Y. Tian, J.J. Sixsmith, M. Brochu

Publisher page

Abstract

Abstract Annealing or HIP below the β transus temperature was found to coarsen the as-built developed microstructure while preserving the developed macro morphology of Laser Wire Deposition (LWD) buildups. Following these thermal cycles, a general decrease in strength along with an increase in elongation have been observed. However, no trends in the tensile results could be extracted due to the scattering of the results. An additional aging cycle substantially stabilized the developed results. Samples processed at 1.4 mm/s exhibited low strength hardly meeting any of the ASTM and AMS minimum requirements and a strong anisotropy in elongation with lower values when tested along the Z direction. Samples processed at 7.2 mm/s exhibited good strength meeting the minimum wrought requirements as set by AMS4911 while elongation showed an isotropic behavior. Hardness has been found to be mostly independent of the experienced sub-β transus post deposition heat treatment. Moreover, the grain boundary strengthening mechanism with regards to the α platelets thicknesses was found to be travel speed dependent.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Leyens · 2003
2. Cost-affordable titanium: the component fabrication perspective10.1007/s11837-007-0074-8 ↗
3. Gibson · 2010
4. Chua · 2014
5. Lütjering · 2007
6. Deposition of Ti-6Al-4V using laser and wire, Part I: Microstructural properties of single beds10.1016/j.surfcoat.2011.07.095 ↗
7. Morphology, microstructure, and hardness of titanium (Ti-6Al-4V) blocks deposited by wire-feed additive layer manufacturing (ALM)10.1016/j.msea.2011.10.095 ↗
8. Material properties of Ti6Al4V parts produced by laser metal deposition10.1016/j.phpro.2012.10.056 ↗
9. An overview of direct laser deposition for additive manufacturing; Part II: mechanical behavior, process parameter optimization and control10.1016/j.addma.2015.07.002 ↗
10. Effect of deposition parameters on mechanical properties of shaped metal deposition parts10.1177/0954405411403669 ↗
11. Grain morphology evolution behavior of titanium alloy components during laser melting deposition additive manufacturing10.1016/j.jallcom.2015.01.256 ↗
12. Deposition of Ti-6Al-4V using laser and wire, Part II: hardness and dimensions of single beds10.1016/j.surfcoat.2011.07.094 ↗
13. An overview of direct laser deposition for additive manufacturing; Part I: transport phenomena, modeling and diagnostics10.1016/j.addma.2015.07.001 ↗
14. Mechanical properties of additive manufactured titanium (Ti-6Al-4V) blocks deposited by a solid-state laser and wire10.1016/j.matdes.2011.06.062 ↗
15. Fabrication of Ti-6Al-4V scaffolds by direct metal deposition10.1007/s11661-008-9634-y ↗
16. Microstructure of additive layer manufactured Ti–6Al–4V after exceptional post heat treatments10.1016/j.matlet.2012.04.116 ↗
17. Additive Manufactured Ti-6Al-4V using welding wire: comparison of laser and arc beam deposition and evaluation with respect to aerospace material specifications10.1016/j.phpro.2010.08.087 ↗
18. Wire based additive layer manufacturing: comparison of microstructure and mechanical properties of Ti-6Al-4V components fabricated by laser-beam deposition and shaped metal deposition10.1016/j.jmatprotec.2011.01.018 ↗
19. N. Chekir, Y. Tian, R. Gauvin, N. Brodusch, J.J. Sixsmith, M. Brochu, Effect of Travel Speed and Stress Relief on Thin Ti-6Al-4V Laser Wire Deposits.
20. The kinetics of static globularization of Ti-6Al-4V10.1007/s11661-002-0340-x ↗
21. Mechanisms of globularization of Ti-6Al-4V during static heat treatment10.1007/s11661-003-0103-3 ↗
22. Coarsening behavior of an alpha-beta titanium alloy
23. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
24. Anisotropic tensile behavior of Ti-6Al-4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
25. Role of geometry on properties of additively manufactured Ti-6Al-4V structures fabricated using laser based directed energy deposition10.1016/j.matdes.2016.05.045 ↗
26. Influence of microstructure on mechanical properties of laser metal wire-deposited Ti-6Al-4V10.1016/j.msea.2016.07.038 ↗
27. E. Brandl, C. Leyens, C.D. Donne, et al., Deposition of Ti-6Al-4V using Nd:YAG laser & Wire: microstructure and mechanical properties, NATO AVT-163 Specialists Meeting on Additive Technology For Repair of Military Hardware, Bonn, Germany, 2009.
28. P.A. Kobryn, S.L. Semiatin, Mechanical Properties of Laser-Deposited Ti-6Al-4V, AFRL/MLLMP 179-186.
29. Fabrication of large Ti–6Al–4V structures by direct laser deposition10.1016/j.jallcom.2014.12.234 ↗
30. Heat-treated microstructure and mechanical properties of laser solid forming Ti-6Al-4V alloy10.1007/s12598-009-0104-5 ↗
31. Microstructure, static properties, and fatigue crack growth mechanisms in Ti-6Al-4V fabricated by additive manufacturing: LENS and EBM10.1016/j.engfailanal.2016.05.036 ↗
32. Microstructure and mechanical properties of wire and arc additive manufactured Ti-6Al-4V
33. Deposition of Ti-6Al-4V using a high power diode laser and wire, Part II: investigation on the mechanical properties10.1016/j.surfcoat.2008.03.028 ↗
34. Tensile properties and microstructures of laser-formed Ti-6Al-4V10.1007/s11665-010-9670-9 ↗
35. Gage length and sample size effect on measured properties during tensile testing10.1016/j.msea.2009.07.046 ↗
36. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
37. Microstructures and mechanical properties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
38. Study of crack propagation mechanisms during Charpy impact toughness tests on both equiaxed and lamellar microstructures of Ti-6Al-4V titanium alloy10.1016/j.msea.2014.09.048 ↗
39. Gilman · 2009
40. Microstructural evolution and mechanical properties of Ti-6Al-4V wall deposited by pulsed plasma arc additive manufacturing10.1016/j.matdes.2016.04.018 ↗
41. Effects of microstructural factors on Quasi-static and dynamic deformation behaviors of Ti-6Al-4V alloys with Widmanstätten structures10.1007/s11661-003-0013-4 ↗
42. Microstructural effects on the mechanical behavior of B-modified Ti-6Al-4V alloys10.1016/j.actamat.2007.05.009 ↗
43. The effect of alpha platelet thickness on plastic flow during hot working of Ti-6Al-4V with a transformed microstructure10.1016/S1359-6454(01)00236-1 ↗
44. The distribution of dislocations in an elliptical glide zone10.1002/pssb.19630031109 ↗
45. Effect of texture and slip mode on the anisotropy of plastic flow and flow softening during hot working of Ti-6Al-4V10.1007/s11661-001-0155-1 ↗
46. Graded microstructure and mechanical properties of additive manufactured Ti-6Al-4V via electron beam melting10.1016/j.actamat.2015.06.036 ↗
47. Engineering science aspects of the Hall-Petch relation10.1007/s00707-013-1048-2 ↗
48. Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: Part I. Microstructural characterization10.1007/s11661-004-0094-8 ↗
49. Review of effect of oxygen on room temperature ductility of titanium and titanium alloys10.1179/1743290114Y.0000000108 ↗