Abstract Cost reducing has always been a very important future development for Ti alloys. A new series of low cost TiZrAlFe alloys with ultra-high strength and favorable ductility are developed in this work. The microstructure and mechanical properties of the new series of low cost TiZr based alloys with Fe content from 0.5 to 2.0 wt% are investigated. As Fe content increases from 0.5 to 2.0 wt%, the β to α phase transition temperature decreases from 836 to 768 °C, and the phase constitution of the examined alloys changes from α′+β to αʺ+β and finally whole β phase. That acicular α′ martensite precipitating out of β matrix is the microstructural feature of the developed low cost alloy with Fe content of 0.5 wt%. As the Fe content increases to 1.0 wt%, the microstructural characteristic is some ultra-fine lenticular αʺ martensites with tens nanometers thickness enchased in β matrix. As the Fe content further increases to 1.5 wt%, the β grains generate recrystallization. Microstructural features of β grains further recrystallization and growth exhibit in the examined alloy with Fe content of 2.0 wt%. Tensile results show that the new series of low cost alloys have ultra-high strength and favorable ductility. The strength of the examined alloys changes from 1495 to 1212 MPa as the increasing of Fe content from 0.5 to 2.0 wt%. Meanwhile the total elongation ranges from 8.3% to 12.4%. The strengthening mechanism of the developed low cost TiZr based alloys is also discussed. The current finding not only presents an excellent alloy with superior combination of strength and ductility but promotes the development and application of low cost Ti alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Microstructure and Mechanical Properties of Steels · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Failure analysis and optimization of thermo-mechanical process parameters of titanium alloy (Ti–6Al–4V) fasteners for aerospace applications10.1016/j.csefa.2013.04.003 ↗
2. Microstructure and mechanical properties of new high strength beta-titanium alloy Ti-130010.1016/j.msea.2014.10.072 ↗
3. Effect of solution treatment and aging on microstructure and tensile properties of high strength β Titanium alloy, Ti–5Al–5V–5Mo–3Cr10.1016/j.matdes.2014.04.015 ↗
4. Effect of heat treatments on microstructure and property of a high strength/toughness Ti–8V–1.5Mo–2Fe–3Al alloy10.1016/j.msea.2014.08.025 ↗
5. Enhanced yielding strength of near-α Ti–Al–Zr–Sn high temperature alloys10.1016/j.msea.2014.11.099 ↗
6. Influence of thermal exposure on the tensile properties and microstructures of Ti60 Titanium alloy10.1016/j.msea.2011.10.011 ↗
7. Microstructure and properties of a laser fabricated burn-resistant Ti alloy10.1016/j.matdes.2003.10.004 ↗
8. Oxidation behavior of a burn resistant highly stabilized β Titanium alloy10.1016/S0921-5093(01)01238-2 ↗
9. Titanium alloys: current status of application and low cost manufacturing technologies
10. High strength and ductile binary Ti–Fe composite alloy10.1016/j.jallcom.2004.03.114 ↗
11. Design of low-cost titanium aluminide intermetallics10.1016/j.jallcom.2015.03.239 ↗
12. Mechanical properties and microstructures of low cost β Titanium alloys for healthcare applications10.1016/j.msec.2004.12.015 ↗
13. Blended elemental P/M synthesis of Ti–6Al–1.7Fe–0.1Si alloy with improved high cycle fatigue strength10.1016/S1359-6462(98)00310-8 ↗
14. Effects of Al content on structure and mechanical properties of hot-rolled ZrTiAlV alloys10.1016/j.matdes.2013.05.065 ↗
15. Microstructure and mechanical properties of hot-rolled ZrTiAlV alloys10.1016/j.msea.2011.10.053 ↗
16. Structure and mechanical properties of Ti–6Al–4 V alloy after zirconium addition10.1016/j.msea.2012.05.043 ↗
17. Structure and mechanical properties of TiZr binary alloy after Al addition10.1016/j.msea.2013.08.029 ↗
18. Aging effects on the microstructures and mechanical properties of the Ti–20Zr–6.5Al–4V alloy10.1016/j.msea.2012.08.128 ↗
19. Preparation of the ZrTiAlV alloy with ultra-high strength and good ductility10.1016/j.msea.2012.01.022 ↗
20. Microstructure and shape memory effect of Ti–20Zr–10Nb alloy10.1016/j.msea.2009.08.063 ↗
21. Research of tizrv pumping coatings on the inner walls of vacuum chamber10.1016/j.phpro.2012.03.648 ↗
22. Factsage, Fe–Ti Phase Diagram, SGTE2007 Alloy Database. 〈http://www.crct.polymtl.ca/FACT/phase_diagram.php?file=Fe-Ti.jpg&dir=SGTE2007〉.
23. Factsage, Fe–Zr Phase Diagram, SGTE2007 Alloy Database. 〈http://www.crct.polymtl.ca/FACT/phase_diagram.php?file=Fe-Zr.jpg&dir=SGTE2007〉.
24. Effect of Fe content on mechanical properties of Ti–6Al–4V alloy
25. Effect of Fe and Mo additions on microstructure and mechanical properties of TiAl intermetallics10.1016/S1003-6326(11)61208-9 ↗
26. Stability of the beta phase in Ti–Mo–Cr alloy fabricated by powder metallurgy10.2298/JMMB121024030S ↗
27. Super elastic behavior and microstructure of Ti19Nb9Zr1Mo (at%) alloy10.1016/j.matlet.2013.07.083 ↗
28. Wikipedia, Titanium. 〈http://en.wikipedia.org/wiki/Titanium〉, (accessed 06.04.15).
29. Wikipedia, Zirconium. 〈http://en.wikipedia.org/wiki/Zirconium〉 (accessed 10.04.15).
30. Wikipedia, Iron. 〈http://en.wikipedia.org/wiki/Iron〉 (accessed 07.04.15).
31. Deformation and dynamic recrystallization behavior of a high Nb containing TiAl alloy10.1016/j.jallcom.2012.11.076 ↗
32. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
33. Hot deformation behavior of ZrTiAlV alloy with a coarse grain structure in the β phase field10.1016/j.msea.2013.04.056 ↗
34. Hot deformation behavior of Ti–20Zr–6.5Al–4V alloy in the α+β and single β phase field10.1016/j.msea.2014.05.014 ↗
35. A mean field model of dynamic and post-dynamic recrystallization predicting kinetics, grain size and flow stress10.1016/j.commatsci.2015.02.043 ↗
36. Effects of boron on the fracture behavior and ductility of cast Ti–6Al–4V alloys10.1016/j.scriptamat.2014.12.022 ↗
37. The orthorhombic αʺ martensite transformation during water quenching and its influence on mechanical properties of Ti–41Zr–7.3Al alloy10.1016/j.intermet.2014.03.010 ↗
38. Microstructure evolution and mechanical properties response of a TZAV alloy during combined thermomechanical treatments10.1016/j.msea.2014.09.071 ↗
39. Deformation behavior of an ordered B2 phase in Ti–25Al–25Zr alloy10.1016/j.intermet.2009.07.015 ↗
40. Strengthening mechanism of two-phase titanium alloys with basketweave microstructure10.1016/j.jallcom.2014.03.057 ↗
41. Development of α-phase morphologies during low temperature isothermal heat treatment of a Ti–5Al–5Mo–5V–3Cr alloy10.1016/j.msea.2010.09.061 ↗
42. Effect of cold rolling on structure and tensile properties of cast Ti–7.5Mo alloy10.1016/j.msea.2015.02.045 ↗
43. Plastic deformation mode of retained β phase in β-eutectoid Ti–Fe alloys10.1007/BF01117366 ↗