Understanding the microstructure evolution mechanism and the microstructure-strength correlations of Ti3SiC2/Ti2AlNb joint brazed with AgCu interlayer
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Structure and synthesis of MAX phase materials: a brief review
2. MAX phase Zr2SeC and its thermal conduction behavior10.1016/j.jeurceramsoc.2021.03.013 ↗
3. Processing of MAX phases: from synthesis to applications10.1111/jace.17544 ↗
4. Oxidation behaviors of compositionally complex MAX phases in air10.1016/j.ceramint.2021.07.198 ↗
5. Synthesis and enhanced mechanical properties of compositionally complex MAX phases10.1016/j.jeurceramsoc.2021.03.027 ↗
6. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
7. Density functional theory study of Mn+1AXn phases: a review10.1080/10408436.2017.1370577 ↗
8. High temperature oxidation behavior of Ti3SiC2-based material in air10.1016/S1359-6454(01)00247-6 ↗
9. Oxidation behavior of C/SiC-Ti3SiC2 at 800–1300 °C in air10.1016/j.jeurceramsoc.2016.03.029 ↗
10. Oxidation behavior of Al-doped Ti3SiC2-20 wt.%Ti5Si3 composite10.1016/j.ceramint.2021.08.272 ↗
11. Effect of grain size on friction and wear behavior of Ti SiC210.1016/S0043-1648(99)00348-8 ↗
12. Ti SiC —a layered ceramic exhibiting ultra-low friction10.1016/S0167-577X(98)00206-7 ↗
13. Synthesis and characterization of a remarkable ceramic: Ti3SiC210.1111/j.1151-2916.1996.tb08018.x ↗
14. Effect of composition on the mechanical properties of newly developed Ti2AlNb-based titanium aluminide10.1016/j.intermet.2004.12.003 ↗
15. Short- and long-term oxidation behaviour of an advanced Ti2AlNb alloy10.1016/j.corsci.2018.11.036 ↗
16. Part III. The tensile behavior of Ti-Al-Nb O ≦ bcc orthorhombic alloys10.1007/s11661-001-0010-4 ↗
17. Microstructure and mechanical properties of Ti3SiC2/Ti3SiC2 diffusion bonded joints using Ti foil as an interlayer10.1016/j.ceramint.2019.07.079 ↗
18. Direct diffusion bonding of Ti3SiC2 and Ti3AlC210.1016/j.materresbull.2008.12.002 ↗
19. Microstructural evolution and growth kinetics of interfacial compounds in TiAl/Ti3SiC2 diffusion bonding joints10.1016/j.msea.2019.04.034 ↗
20. Evaluation on diffusion bonded joints of TiAl alloy to Ti3SiC2 ceramic with and without Ni interlayer: interfacial microstructure and mechanical properties10.1016/j.matdes.2014.01.029 ↗
21. Enhanced TiAl/Ti3SiC2 diffusion bonding by introducing amorphous intergranular films in Ti3SiC2 through Al doping10.1016/j.scriptamat.2019.12.031 ↗
22. Effect of electric current on diffusion of aluminum in Ti3AlC2 into zirconium alloy10.1007/s11595-017-1647-1 ↗
23. Reactivity of Zircaloy-4 with Ti3SiC2 and Ti2AlC in the 1100–1300 °C temperature range10.1016/j.jnucmat.2015.02.006 ↗
24. Interfacial study of NiTi–Ti3SiC2 solid state diffusion bonded joints10.1016/j.msea.2014.10.033 ↗
25. Phase and morphology evolution in high-temperature Ti3SiC2–NiTi diffusion-bonded joints10.1016/j.scriptamat.2011.04.015 ↗
26. Interfacial microstructure and mechanical properties of Ti3SiC2 ceramic and TC11 alloy joint diffusion bonded with a Cu interlayer10.1016/j.ceramint.2020.08.115 ↗
27. Joining of Ti3SiC2 by magnetron sputtering a layer of Cu or Zr followed by heat treating at relatively low temperatures10.1111/j.1551-2916.2011.04566.x ↗
28. Microstructural evolution and growth kinetics of interfacial reaction layers in SUS430/Ti3SiC2 diffusion bonded joints using a Ni interlayer10.1016/j.ceramint.2021.10.234 ↗
29. Microstructure and mechanical strength of transient liquid phase bonded Ti3SiC2 joints using Al interlayer10.1016/j.jeurceramsoc.2007.01.012 ↗
30. Wetting kinetics and spreading phenomena of the precursor film and bulk liquid in the AgCuTi/TC4 system10.1016/j.jallcom.2019.06.168 ↗
31. Contact-reactive brazing of Ti3SiC2 ceramic to TC4 alloy using a Ni interlayer: interfacial microstructure and joining properties10.1016/j.ceramint.2018.04.006 ↗
32. Interfacial microstructure and mechanical properties of TC4/Ti3SiC2 contact-reactive brazed joints using a Cu interlayer10.1016/j.ceramint.2018.08.328 ↗
33. Effects of interfacial reaction and atomic diffusion on the mechanical property of Ti3SiC2 ceramic to Cu brazing joints10.1016/j.vacuum.2016.05.002 ↗
34. Effects of surface microstructure on the active element content and wetting behavior of brazing filler metal during brazing Ti3SiC2 ceramic and Cu10.1016/j.vacuum.2018.07.043 ↗
35. Controlling interfacial reactions of Ti3SiC2/Ti2AlNb brazed joints by transferring graphene layers10.1016/j.msea.2019.138624 ↗
36. Improvement for interfacial microstructure and mechanical properties of Ti3SiC2/Cu joint brazed by Ag-Cu-Ti filler with copper mesh10.3390/cryst11040401 ↗
37. Synthesis of single-phase Ti3SiC2 from coarse elemental powders and the effects of excess Al10.1016/j.ceramint.2018.09.270 ↗
38. Effect of Al addition on low-temperature synthesis of Ti3SiC2 powder10.1016/j.jallcom.2007.07.090 ↗
39. Effect of Al addition on the synthesis of Ti3SiC2 bulk material by pulse discharge sintering process10.1016/j.jeurceramsoc.2007.03.038 ↗
40. Low-temperature fabrication of high purity Ti3SiC210.1016/j.jallcom.2007.05.074 ↗
41. Microstructure and mechanical properties of Ti2AlNb alloy and C/C composite joints brazed with Ag–Cu–Zn and Ag–Cu–Zn/Cu/Ag–Cu–Ti filler metals10.1016/j.acme.2019.04.008 ↗
42. Laik · 2022
43. A detailed study of phase evolution in Cu–16at. %Al and Cu–30at. %Al alloys under different types of mechanical alloying processes10.1016/j.apt.2014.12.005 ↗
44. Selective etching of silicon from Ti3 SiC2 (MAX) to obtain 2D titanium carbide (MXene)10.1002/anie.201802232 ↗
45. Chemical bonding and electronic-structure in MAX phases as viewed by X-ray spectroscopy and density functional theory10.1016/j.tsf.2016.11.005 ↗
46. Microstructure evolution and brazing mechanisms of the Ti2AlC/Ni joints using nickel based filler alloy10.1016/j.jeurceramsoc.2016.05.024 ↗
47. Wettability of Ti3SiC2 by Ag–Cu and Ag–Cu–Ti melts10.1007/s10853-009-3941-6 ↗
48. Experimental evidence of copper insertion in a crystallographic structure of Ti3SiC2 MAX phase10.1016/j.scriptamat.2015.03.015 ↗
49. Chemical reaction and stability of Ti3SiC2 in Cu during high-temperature processing of Cu/Ti3SiC2 composites
50. Interface structure and wetting behaviour of Cu/Ti3SiC2system10.1179/1743676114Y.0000000185 ↗
51. Thermodynamic and kinetic study of solid state reactions in the Cu–Si system10.1063/1.371357 ↗
52. Calorimetric measurements and assessment of the binary Cu–Si and ternary Al–Cu–Si phase diagrams10.1016/j.calphad.2016.03.002 ↗
53. Intermetallic alloys based on orthorhombic titanium aluminide10.1002/1527-2648(200111)3:11<851::AID-ADEM851>3.0.CO;2-G ↗
54. In-Situ synthesized TiC nano-flakes reinforced C/C composite-Nb brazed joint10.1016/j.jeurceramsoc.2017.11.059 ↗
55. Correlation of yield strength and tensile strength with hardness for steels10.1007/s11665-008-9225-5 ↗
56. Thermal expansion coefficients of Ag, Cu and diamond nanoparticles: in situ TEM diffraction and EELS measurements10.1016/j.matchar.2021.111296 ↗