Melt-spun precipitation hardened Sm(Co, Fe, Cu, Zr) magnets

A. Yan, A. Bollero, O. Gutfleisch, K.-H. Müller, L. Schultz

Publisher page

Abstract

Abstract The effects of alloy composition and the temperature range of cooling regime on microstructure and magnetic properties of melt-spun Sm(Co 0.74 Fe 0.1 Cu 0.12 Zr 0.04 ) 7.5 (Cu/Zr-rich) and Sm(Co 0.75 Fe 0.15 Cu 0.08 Zr 0.02 ) 7.6 (Cu/Zr-poor) magnets were investigated. A very high coercivity of 2.8 T was obtained by applying a simple aging procedure to the as-spun Sm(Co 0.74 Fe 0.1 Cu 0.12 Zr 0.04 ) 7.5 ribbons, which is much higher than that of Sm(Co 0.75 Fe 0.15 Cu 0.08 Zr 0.02 ) 7.6 one. Transmission electron microscopy (TEM) shows that an uniform cellular and lamellar structure was observed in the annealed Sm(Co 0.74 Fe 0.1 Cu 0.12 Zr 0.04 ) 7.5 ribbons, which results from the single-phase TbCu 7 type matrix in the as-spun ribbons, in contrast to a mixture of 2:17 and 1:7-type Sm–Co phases in the as-spun Sm(Co 0.75 Fe 0.15 Cu 0.08 Zr 0.02 ) 7.6 ribbons. High temperature measurements revealed that the temperature stability of the coercivity of Sm(Co 0.74 Fe 0.1 Cu 0.12 Zr 0.04 ) 7.5 ribbons is very sensitive to the temperature range of the cooling regime and the lower the quenching temperature, the more negative the temperature coefficient. A coercivity of 0.53 T at 500 °C was obtained in the sample quenched at 600 °C. Ribbons prepared by this simple processing route based on melt-spinning, in contrast to the conventional time consuming and intricate aging program, have a strong potential for a more economic preparation of bonded magnets in the future.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnetic Properties of Alloys · Magnetic Properties and Applications · Magnetic properties of thin films

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Hadjipanayis · IEEE Trans. Magn. Mag · 2000 · 36 · 338210.1109/20.908808 ↗
2. Durst · Phys. Status Solidi A · 1988 · 108 · 40310.1002/pssa.2211080143 ↗
3. Fidler · J. Magn. Magn. Mater · 1982 · 30 · 5810.1016/0304-8853(82)90010-5 ↗
4. Ray · J. Appl. Phys · 1990 · 67 · 497210.1063/1.344720 ↗
5. Yan · Appl. Phys. Lett · 2002 · 80 · 124310.1063/1.1450253 ↗
6. Morita · IEEE Trans. Magn · 1987 · 23 · 270210.1109/TMAG.1987.1065423 ↗
7. Liu · Appl. Phys. Lett · 1998 · 73 · 300710.1063/1.122659 ↗
8. Goll · Appl. Phys. Lett · 2000 · 76 · 105410.1063/1.125936 ↗
9. Zhou · Appl. Phys. Lett · 2000 · 77 · 151410.1063/1.1290719 ↗
10. Liu · J. Appl. Phys · 2000 · 87 · 672810.1063/1.372822 ↗