Creep of MARBN-type 9Cr martensitic steel in gaseous CO2 environment

K.A. Rozman, R.P. Oleksak, Ö.N. Doğan, M. Detrois, P.D. Jablonski, J.A. Hawk

Abstract

Abstract With an interest in moving from steam to supercritical CO2 as the working fluid in advanced energy systems, it is important to study the mechanical response of structural alloys to CO2-containing environments. MARBN-type 9Cr martensitic steel was originally developed for application in boilers for supercritical and ultra-supercritical power plants where the steam temperature reaches 650 °C. In this research, a MARBN-type 9Cr martensitic steel designed and manufactured at NETL was creep tested in a gaseous CO2 environment (i.e., 0.1 MPa at 650 °C), and the results are directly compared to creep tests conducted in air. It was found that environmentally-assisted cracking facilitated by carbide formation beneath the growing oxide accelerated failure in gaseous CO2. This work indicates that creep-oxidation interactions in advanced martensitic steels represent an important consideration for materials selection in supercritical CO2 power cycles. Furthermore, this work confirms that more oxidation-resistant alloys will be required for the highest temperature portions of these systems.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Effect of pressure on supercritical CO2compatibility of structural alloys at 750 °C10.1002/maco.201508783 ↗
2. THE EFFECT OF TEMPERATURE ON THE sCO2 COMPATIBILITY OF CONVENTIONAL STRUCTURAL ALLOYS
3. Effect of surface finish on high-temperature oxidation of steels in CO2, supercritical CO2, and air10.1007/s11085-019-09938-6 ↗
4. Holcomb · 2016
5. 4.14 - materials performance in CO2 and supercritical CO2
6. High-temperature oxidation of commercial alloys in supercritical CO2 and related power cycle environments
7. Effect of pressure and thermal cycling on long-term oxidation in CO2 and supercritical CO210.1007/s11085-020-10004-9 ↗
8. Corrosion and carburization behavior of chromia-forming heat resistant alloys in a high-temperature supercritical-carbon dioxide environment10.1016/j.corsci.2015.07.007 ↗
9. Corrosion of a stainless steel and nickel-based alloys in high temperature supercritical carbon dioxide environment10.1016/j.corsci.2012.11.041 ↗
10. Effects of corrosion in supercritical CO2 on the microstructural evolution in 800H alloy10.1007/s11085-018-9852-7 ↗
11. Effect of CO2 gas pressure on composition, growth rate, and structure of duplex oxide formed on 9Cr steel at 550 °C10.1016/j.corsci.2019.108252 ↗
12. Effect of sample thickness on the oxidation and carburization kinetics of 9Cr-1Mo steel in high and atmospheric pressure CO2 at 550 °C10.1016/j.corsci.2019.108292 ↗
13. Effect of pressure on the corrosion and carburization behavior of chromia-forming heat-resistant alloys in high-temperature carbon dioxide environments10.1016/j.corsci.2016.06.004 ↗
14. Fatigue crack growth mechanisms for nickel-based superalloy Haynes 282 at 550-750 °C10.1007/s11665-015-1678-8 ↗
15. Corrosion and mechanical performance of grade 92 ferritic-martensitic steel after exposure to supercritical carbon dioxide10.1007/s11661-020-05691-7 ↗
16. Effect of specimen thickness on the degradation of mechanical properties of ferritic-martensitic P91 steel by direct-fired supercritical CO2 power cycle environment10.1007/s11661-020-06065-9 ↗
17. Martin · 1962
18. McPherson · 1961
19. Effect of carburization (pyrolysis furnace tube main failure factor) on the microstructure and properties of HPNb alloy tube10.1016/j.engfailanal.2020.104610 ↗
20. Corrosion and creep behavior of a Ni-base alloy in supercritical-carbon dioxide environment at 650 °C10.1016/j.corsci.2020.108843 ↗
21. Feasibility of MARBN steel for application to thick section boiler components in USC power plant at 650°C
22. Homogenizing advanced alloys: thermodynamic and kinetic simulations followed by experimental results10.1007/s11665-016-2451-3 ↗
23. Correlation of creep fracture lifetime with microstructure evolution and cavity behaviors in G115 martensitic heat-resistant steel10.1016/j.msea.2020.139468 ↗
24. Corrosion of 9-12Cr ferritic–martensitic steels in high-temperature CO210.1016/j.corsci.2016.01.009 ↗
25. Effect of boron on carbide coarsening at 873 K (600 °C) in 9 to 12 pct chromium steels10.1007/s11661-012-1205-6 ↗
26. Effect of boron in the coarsening rate of chromium-rich carbides in 9%–12% chromium martensitic creep-resistant steel: experiment and modeling at 650 °C