journal article·2025-09Open access

Influence of the microstructure on the high temperature ductility of the Al-4Mn-3Ni-2Cu-1Zr aluminium alloy designed for laser powder bed fusion

Tristan Lenoir, Maxence Buttard, Béchir Chehab, Stéphane Coindeau, Arthur Després, Jean-Jacques Blandin, Guilhem Martin

Abstract

The elevated-temperature mechanical properties of a new Al-4Mn-3Ni-2Cu-1Zr (wt%) aluminium alloy designed for LB-PBF in its stress-relieved condition (4h/300°C), were evaluated using tensile tests conducted from 100°C up to 350°C at different strain rates ranging from 10 -2 s -1 to 10 -5 s -1 . The ductility decreases when decreasing strain rates for temperatures >150°C. The microstructure is highly heterogeneous across multiple scales. At the grain scale, regions near the melt pool boundaries consist of submicron fine equiaxed grains (FZ) while coarser columnar grains (CZ) are found in the melt pool interiors. The microstructure is also decorated by a large fraction of intermetallic particles (about 20%). Their morphology, size, and spatial distribution depend on the region of interest (FZ or CZ). Based on a multi-scale microstructural analysis of the deformed and fractured specimens using scanning and transmission electron microscopy, we investigate the damage mechanisms and identify the main deformation mechanisms operating in the FZ and CZ regions. Regardless of the temperature between 100 and 350°C, both regions FZ and CZ deform by dislocation creep at high strain rates. From 150°C up to 350°C, the FZ is subjected to a change in deformation mechanism from dislocation creep at high strain rate (insensitive to grain size) to grain boundary sliding (sensitive to grain size) at low strain rate. This change in deformation mechanism of the FZ at low strain rates leads to early strain localization and damage development. At the same time, the CZ remains in a regime governed by dislocation creep. Thus, the contrast between the mechanical response in the FZ and CZ increases for temperatures >150°C at low strain rates.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing10.1080/09506608.2021.1951580 ↗
2. A novel laser powder bed fusion al-fe-zr alloy for superior strength-conductivity trade-off10.1016/j.scriptamat.2022.114878 ↗
3. Multi-scale microstuctural investigation of a new al-mn-ni-cu-zr aluminium alloy processed by laser powder bed fusion10.1016/j.mtla.2021.101160 ↗
4. A creep-resistant additively manufactured al-ce-ni-mn alloy10.1016/j.actamat.2022.117699 ↗
5. An additively manufactured near-eutectic al-ce-ni-mn-zr alloy with high creep resistance10.1016/j.actamat.2024.119787 ↗
6. Al-Cu-Ce(-Zr) alloys with an exceptional combination of additive processability and mechanical properties
7. Design of al–fe–mn alloy for both high-temperature strength and sufficient processability of laser powder bed fusion
8. Microstructural evolution and strengthening mechanisms in a heat-treated additively manufactured al–cu–mn–zr alloy10.1016/j.msea.2022.142928 ↗
9. Change in microstructural characteristics of laser powder bed fused Al–Fe binary alloy at elevated temperature10.1016/j.jmst.2021.04.038 ↗
10. An Al-5Fe-6Cr alloy with outstanding high temperature mechanical behavior by laser powder bed fusion
11. Elevated temperature ductility dip in an additively manufactured al-cu-ce alloy10.1016/j.actamat.2021.117285 ↗
12. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
13. Additive manufacturing of novel aluminium matrix composites with enhanced strength and processability via boron nitride functionalization
14. Revealing the precipitation behavior of crack-free TiB2/Al-Zn-Mg-Cu composites manufactured by laser powder bed fusion
15. An additively manufactured AlCuMnZr alloy microstructure and tensile mechanical properties10.1016/j.mtla.2020.100758 ↗
16. Coarsening- and creep resistance of precipitation-strengthened al–mg–zr alloys processed by selective laser melting10.1016/j.actamat.2020.02.008 ↗
17. Microstructures and high temperature tensile behaviours of laser powder bed fusion fabricated al-mn-sc alloy10.3390/met13040788 ↗
18. Creep property and microstructural evolution of laser powder bed fused binary Al–10Ce alloy10.1016/j.msea.2023.145631 ↗
19. Ageing response and strengthening mechanisms in a new al-mn-ni-cu-zr alloy designed for laser powder bed fusion10.1016/j.actamat.2023.119271 ↗
20. An understanding of duplex microstructures encountered during high strength aluminium alloy laser beam melting processing10.1016/j.actamat.2021.117024 ↗
21. Effect of laser rescanning on the grain microstructure of a selective laser melted al-mg-zr alloy10.1016/j.matchar.2018.03.033 ↗
22. Microstructure and mechanical properties of al-mg-zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
23. Cracking mechanism and its sensitivity to processing conditions during laser powder bed fusion of a structural aluminum alloy10.1016/j.mtla.2020.100976 ↗
24. Optimization of the strength vs. conductivity trade-off in an aluminium alloy designed for laser powder bed fusion10.1016/j.msea.2022.144139 ↗
25. Additive manufacturing and mechanical properties of the dense and crack free Zr-modified aluminum alloy 6061 fabricated by the laser-powder bed fusion
26. Precipitation kinetics, microstructure evolution and mechanical behavior of a developed al–mn–sc alloy fabricated by selective laser melting10.1016/j.actamat.2020.04.015 ↗
27. Synthesis of precipitation-strengthened al-sc, Al-Zr and al-sc-zr alloys via selective laser melting of elemental powder blends
28. Microstructure and mechanical properties of a precipitation-strengthened al-zr-sc-er-si alloy with a very small Sc content10.1016/j.actamat.2017.10.040 ↗
29. Durcissement par précipitation des alliages d’aluminium
30. Tailored Mg and Cu contents affecting the microstructures and mechanical properties of high-strength al–zn–mg–cu alloys10.1016/j.msea.2016.01.039 ↗
31. Influence of microstructure heterogeneity on the tensile response of an aluminium alloy designed for laser powder bed fusion10.1016/j.actamat.2024.119786 ↗
32. Microstructural development and aging behavior of al–cr–zr heat-resistant alloy fabricated using laser powder bed fusion10.1016/j.jmrt.2021.10.027 ↗
33. Automated crystal orientation and phase mapping in TEM10.1016/j.matchar.2014.08.010 ↗
34. Bauschinger effect in an aluminium alloy designed for laser powder bed fusion10.1016/j.mtla.2024.102093 ↗
35. Evidence that the liquid structure affects the nucleation of the primary metastable L12-Al3Zr in additive manufacturing10.1016/j.scriptamat.2022.115212 ↗
36. Towards an alloy design strategy by tuning liquid local ordering: what solidification of an Al-alloy designed for laser powder bed fusion teaches Us
37. High-temperature mechanical properties of AlSi10Mg specimens fabricated by additive manufacturing using selective laser melting technologies (AM-SLM)
38. Microstructure, tensile properties and thermal stability of AlMgSiScZr alloy printed by laser powder bed fusion10.1016/j.jmst.2020.08.033 ↗
39. Additively manufactured scalmalloy via laser powder bed fusion (L‐PBF): temperature-dependent tensile and fatigue behaviors10.1111/ffe.14549 ↗
40. Buttard · 2023
41. « creep of metal matrix composites
42. « solute-induced strengthening during creep of an aged-hardened al-mn-zr alloy10.1016/j.actamat.2021.117268 ↗
43. Creep rupture of a silicon carbide reinforced aluminum composite10.1007/BF02644396 ↗
44. The effect of processing route and reinforcement geometry on isothermal creep behaviour of particulate and short fibre MMCs10.1016/S0921-5093(97)00524-8 ↗
45. Contribution of grain boundary sliding in low-temperature superplasticity of ultrafine-grained aluminum alloys10.1016/j.scriptamat.2009.10.010 ↗
46. Superplastic deformation mechanism of an ultrafine-grained aluminum alloy produced by friction stir processing10.1016/j.actamat.2010.05.003 ↗
47. Development of ultrafine-grained microstructure and low temperature (0.48 tm) superplasticity in friction stir processed al–mg–zr10.1016/j.scriptamat.2005.03.018 ↗
48. Deformation mechanisms during low-and high-temperature superplasticity in 5083 Al-Mg alloy10.1007/s11661-002-0062-0 ↗
49. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting10.1016/j.actamat.2020.07.015 ↗
50. Direct ageing of LPBF Al-1Fe-1Zr for high conductivity and mechanical performance10.1016/j.actamat.2023.119199 ↗
51. Microstructure, tensile properties and heat-resistant properties of selective laser melted AlMgScZr alloy under long-term aging treatment10.1016/j.msea.2021.142527 ↗