journal article·2001-06

Fracture characteristics and microstructural factors in single and duplex annealed Ti–4.5Al–3V–2Mo–2Fe

A. Gunawarman, Mitsuo Niinomi, Kei-ichi Fukunaga, Daniel Eylon, Shiro Fujishiro, Chiaki Ouchi

Materials Science and Engineering: A· Volume 308· Issue 1-2
Publisher page

Abstract

Abstract The influence of microstructure on fracture toughness of single and duplex annealed Ti–4.5Al–3V–2Mo–2Fe alloys was investigated. For the single-annealing treatment between 1103 and 1173 K for 3.6 ks, fracture toughness, J IC , decreases first with the increase of annealing temperature from 1103 to 1123 K and then increases with increasing annealing temperature upto 1173 K. As a result, there is a minimum of fracture toughness at 1123 K. This anomalous relation between fracture toughness and annealing temperature also exists in the duplex-annealed specimens at 993 K for 3.6 ks followed by the above single-annealing treatment. Examining the change of J IC and microstructure with annealing temperature, it can be found that J IC is related to volume fraction, aspect ratio and grain size of primary α phase, width of acicular α phase and prior β grain size. The decrease of fracture toughness in the temperature range from 1103 to 1123 K is mainly due to the decrease of volume fraction of primary α phase, while the increase of fracture toughness above 1123 K is mainly caused by the increase of prior β grain size.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. 1994 · 685
2. Brewer · Mat. Sci. Eng. A · 1998 · A243 · 29910.1016/S0921-5093(97)00818-6 ↗
3. A. Ogawa, M. Niikura, C. Oichi, K. Minakawa, M. Yamada, J. Testing Eval., (1996) 100–109.10.1520/JTE12683J ↗
4. Ouchi · 1994 · 37
5. Ishikawa · 1993 · 2 · 141
6. Fujita · 1993 · 61
7. Ogawa · 1996 · 2 · 1251
8. Boyer · 1996 · 2 · 933
9. Nakajima · Mat. Sci. Eng. A · 1998 · A243 · 17610.1016/S0921-5093(97)00797-1 ↗
10. Fan · J. Mat. Sci. Lett. · 1993 · 12 · 166510.1007/BF00418824 ↗
11. Helbert · Metall. Mat. Trans. A · 1999 · 30A · 285310.1007/s11661-999-0123-8 ↗
12. Margolin · Metall. Trans. A · 1982 · 13A · 219110.1007/BF02648389 ↗
13. Terlinde · Metall. Mat. Trans. A · 1988 · 19A · 103710.1007/BF02628388 ↗
14. Niinomi · Mat. Sci. Tech. · 1988 · 4 · 80310.1179/mst.1988.4.9.803 ↗
15. Niinorni · Mat. Sci. Eng. A · 1996 · M13 · 16
16. Hunter · 1996 · 2 · 925
17. ASTM Designation E813-89, Standard test method for JIC, ASTM, Philadelphia, PA, 1996.
18. Niinoml · Mat. Sci. Eng. A · 1988 · A100 · 4510.1016/0025-5416(88)90238-8 ↗
19. Hirano · J. Mat. Testing Eval. · 1985 · 13 · 35610.1520/JTE10962J ↗