Microstructure and electrical properties of Sm2O3 doped Bi2O3-based ZnO varistor ceramics
Source abstract
Abstract
Abstract The dependence of the bulk density, microstructure and dc electrical properties of bismuth oxide (Bi 2 O 3 )-based zinc oxide (ZnO) varistor ceramics for various samarium oxide (Sm 2 O 3 ) contents was investigated. The value of bulk density was found to 5.43–5.50 g cm −3 with Sm 2 O 3 (mol%) content. The maximum value of bulk density is observed to be 5.50 for 0.30 mol% Sm 2 O 3 containing varistor ceramics. The grain sizes for all the samples calculated from the scanning electron micrographs were found to decrease as Sm 2 O 3 increases. The presence of ZnO phases, Bi-rich phases, spinel phases and Sm 2 O 3 phases were observed in the samples by the energy dispersive X-ray analysis and X-ray diffraction analysis. As the Sm 2 O 3 amount increased in the Bi 2 O 3 -based ZnO varistor ceramics, the nonlinear coefficient, α increased up to 0.10 mol%, reaching a maximum value of 58 and then decreased. The breakdown electric field, E b , increased with the increase of Sm 2 O 3 content with a maximum value of 3220 V cm −1 for the 0.75 mol% Sm 2 O 3 doped ZnO varistor ceramics. The leakage current, I L , showed a minimum value of 1.10 μA for the composition of 0.30 mol% Sm 2 O 3 doped Bi 2 O 3 -based ZnO varistor ceramics. The 0.30 mol% Sm 2 O 3 -doped Bi 2 O 3 -based ZnO varistor ceramics sintered at 1200 °C exhibited a good stability for dc accelerated aging stress of 0.90 V 1 mA /90 °C/12 h.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Ga2O3 and related materials · Advancements in Solid Oxide Fuel Cells
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Matsuka · Jpn. J. Appl. Phys. · 1971 · 10 · 73610.1143/JJAP.10.736 ↗
2. Levinson · J. Am. Ceram. Soc. Bull. · 1986 · 65 · 639
3. Gupta · J. Am. Ceram. Soc. · 1990 · 73 · 181710.1111/j.1151-2916.1990.tb05232.x ↗
4. Clarke · J. Am. Ceram. Soc. · 1999 · 82 · 48510.1111/j.1151-2916.1999.tb01793.x ↗
5. Cordaro · J. Appl. Phys. · 1986 · 60 · 418610.1063/1.337504 ↗
6. William · J. Appl. Phys. · 1980 · 51 · 393010.1063/1.328168 ↗
7. Lei · J. Phys. D: Appl. Phys. · 2004 · 37 · 80410.1088/0022-3727/37/5/024 ↗
8. Houabes · Ceram. Int. · 2007 · 33 · 119110.1016/j.ceramint.2006.04.004 ↗
9. Nahm · Mater. Lett. · 2007 · 61 · 495010.1016/j.matlet.2007.03.078 ↗
10. Nahm · J. Mater. Sci. · 2008 · 43 · 285710.1007/s10853-007-2263-9 ↗
11. Nahm · Solid State Commun. · 2009 · 149 · 79510.1016/j.ssc.2009.02.029 ↗
12. Peiteado · J. Eur. Ceram. Soc. · 2007 · 27 · 386710.1016/j.jeurceramsoc.2007.02.046 ↗
13. Bernik · J. Eur. Ceram. Soc. · 2004 · 24 · 119510.1016/S0955-2219(03)00412-6 ↗
14. Bernik · J. Eur. Ceram. Soc. · 2007 · 27 · 316110.1016/j.jeurceramsoc.2007.02.176 ↗
15. Ashraf · J. Phys. B · 2010 · 405 · 377010.1016/j.physb.2010.05.084 ↗
16. Wurst · J. Am. Ceram. Soc. · 1972 · 55 · 10910.1111/j.1151-2916.1972.tb11224.x ↗