Electrical properties of Al/Al 4 C 3 /4H-SiC diodes
Source abstract
Abstract
Abstract The impact of aluminum carbide (Al 4 C 3 ) at the metal/silicon-carbide (SiC) interface is presented here with respect to 4H-SiC Schottky barrier diodes (SBDs). A post-annealing process at a high temperature (1000 °C) has been employed for the reaction between the aluminum and the carbon. The current density of the fabricated device was measured as ~ 13.4 A/cm 2 at 5 V with a leakage current density of less than ~ 6.84 × 10 −9 A/cm 2 at − 5 V. The thermal-activation energy ( E A = 0.35 eV) extracted from the Arrhenius plot decreased by ~ 37% via the formation of the Al 4 C 3 . According to the experiment results, the sample with the Al 4 C 3 layer yields a rectification ratio of 1.95 × 10 9 that is 33 times higher than that of the reference SBDs. The structural defects of the SiC interface may be available for the formation of the Al 4 C 3 layer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon Carbide Semiconductor Technologies · Semiconductor materials and interfaces · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Cooper · Mater. Sci. Forum · 1998 · 264–268 · 89510.4028/www.scientific.net/MSF.264-268.895 ↗
2. Ewing · J. Appl. Phys. · 2007 · 101 · 11451410.1063/1.2745436 ↗
3. Defives · IEEE Trans. Electron Devices · 1999 · 46 · 44910.1109/16.748861 ↗
4. Schoen · IEEE Trans. Electron Devices · 1998 · 45 · 159510.1109/16.701494 ↗
5. F.D. Meyer, Ph.D. Thesis, Universita¨t Freiburg, 1998, p.199.
6. Blucher · Mater. Sci. Eng. A · 2004 · 387 · 86710.1016/j.msea.2003.11.083 ↗
7. Petrusha · Sci. Direct · 2004 · 13 · 666
8. Khalid · Sci. Direct · 2004 · 13 · 393
9. Vladimir · Sci. Direct · 2005 · 135 · 87
10. Yao · RSC Adv. · 2016 · 6 · 8121110.1039/C6RA15164G ↗
11. Moulder · 1992
12. Farhan · Springe. Link · 2015 · 22 · 897
13. Bermudez · Appl. Phys. Lett. · 1983 · 42 · 7010.1063/1.93730 ↗
14. Biedermann · Phys. Rev. B · 2009 · 79 · 12541110.1103/PhysRevB.79.125411 ↗
15. Zhang · Solid-State Electron · 2001 · 45 · 184710.1016/S0038-1101(01)00191-5 ↗
16. Ayalew · Microelectron. Reliab. · 2004 · 44 · 147310.1016/j.microrel.2004.07.042 ↗
17. Sochacki · Diam. Relat. Mater. · 2005 · 14 · 113810.1016/j.diamond.2004.12.020 ↗
18. Park · Appl. Phys. Lett. · 2016 · 109 · 03160310.1063/1.4958841 ↗
19. Rhoderick · 1988 · 19
20. Neamen · 2003
21. Lundberg · Solid-State Electron. · 1996 · 39 · 155910.1016/0038-1101(96)00071-8 ↗
22. J. P. Doyle, M. O. Aboelfotoh, M. K. Linnarsson, B. G. Svensson, A. Schoner, N. Nordell, C. Harris, J. L. Lindström, E. Janzen, and C. Hemmingsson, MRS Symp. in: Proceedings of the Ser. 423, 1996, p. 519.10.1557/PROC-423-519 ↗
23. Ci · Acta Mater. · 2006 · 54 · 536710.1016/j.actamat.2006.06.031 ↗