Evaluation of Schottky barrier source/drain contact on gate-all-around polycrystalline silicon nanowire MOSFET
Source abstract
Abstract
Abstract Self-aligned nickel salicide of gate-all-around silicon nanowires (GAA Si NWs) MOSFET has been investigated using very-large-scale integration (VLSI) process. The nickel salicide (NiSi x ) characteristics including sheet resistance (R s ), phase transformation and Schottky barrier height (SBH) are discussed via line structures and Schottky diode, respectively. RTA temperature strongly affects R s of NiSi x and related with surface morphology. Below 700 °C, near 4.5 Ω/□ of smooth surface of NiSi R s is obtained in comparison with 12.6 Ω/□ of NiSi 2 at 700 °C. Both forward bias of current-voltage (I-V) and temperature-dependency of activation-energy methods have been used to characterize Schottky barrier height (SBH). For 400 °C RTA sample, the SBH and ideality factor extracted from the forward bias of current-voltage (I-V) method are 0.38 eV and 1.53, respectively. Besides, the SBH extracted from temperature-dependency of activation-energy methods is 2.9 eV. The variation of SBH values are attributed to the thermionic-field emission (TFE) which the interface states and inhomogeneity induce slightly tunneling current. Moreover, various channel lengths of Schottky source/drain contacts of GAA Si NWs MOSFET devices were measured and results demonstrate that enough electrical performances combined with ambipolar behavior are available for future application in logical circuit and non-volatile memory.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and interfaces · Nanowire Synthesis and Applications · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Improvement of the poly-SiGe electrode contact technology for MEMS10.1088/0960-1317/20/9/095029 ↗
2. Nanotorsional resonator torque magnetometry10.1063/1.3319502 ↗
3. VLSI-NEMS chip for parallel AFM data storage10.1016/S0924-4247(99)00254-X ↗
4. RF MEMS from a device perspective10.1088/0960-1317/10/4/201 ↗
5. Zavracky · J. Micromech. Switch. Microelectromech. Syst. · 1997 · 6 · 310.1109/84.557524 ↗
6. Nickel silicide thin films as masking and structural layers for silicon bulk micro-machining by potassium hydroxide wet etching10.1088/0960-1317/18/9/095002 ↗
7. Copper-encapsulated silicon micromachined structures10.1109/84.870052 ↗
8. Study on the application of silicide in surface micromachining10.1088/0960-1317/12/2/310 ↗
9. Wolf · 1990 · 2
10. Effects of N-induced heterogeneous nucleation and growth of cavities at the CoSi2/polycrystalline–silicon10.1063/1.1488697 ↗
11. Characterization of a self‐aligned cobalt silicide process10.1149/1.2100597 ↗
12. Thermal stability of thin submicrometer lines of CoSi210.1149/1.2056087 ↗
13. Thermal stability of cobalt suicide stripes on Si (001)10.1063/1.371172 ↗
14. In situ transmission electron microscopy study of Ni silicide phases formed on (001) Si active lines10.1063/1.1378812 ↗
15. Formation of Ni germano-silicide on single crystalline Si/sub 0.3/Ge/sub 0.7//Si10.1109/LED.2002.801288 ↗
16. Tuning of nickel silicide Schottky barrier height on p-type silicon by indium implantation10.1109/LED.2009.2033451 ↗
17. Field and thermionic-field emission in Schottky barriers10.1016/0038-1101(66)90097-9 ↗
18. Characterisation of advanced LOCOS isolation
19. High-temperature degradation of NiSi films: agglomeration versus NiSi2 nucleation10.1063/1.2005380 ↗
20. Phase formation and thermal stability of ultrathin nickel-silicides on Si(100)10.1063/1.3384997 ↗
21. Low Schottky barrier height for silicides on η-type Si (100) by interfacial selenium segregation during silicidation10.1063/1.2970958 ↗
22. Tuning of the nickel silicide Schottky barrier height on p-type silicon by indium implantation10.1109/LED.2009.2033451 ↗
23. Current transport in metal-semiconductor barriers10.1016/0038-1101(66)90127-4 ↗
24. Tuning the Schottky barrier height of nickel silicide on p-silicon by aluminum segregation10.1063/1.2940596 ↗
25. Modulation of Ni Ge/Ge Schottky barrier height by sulfur segregation during Ni germanidation10.1063/1.2191829 ↗
26. Low Schottky barrier height for silicides on nn-type Si (100) by interfacial selenium segregation during silicidation10.1063/1.2970958 ↗
27. On the existence of a distribution of barrier heights in Pd2Si/Si Schottky diodes10.1063/1.362818 ↗
28. Barrier inhomogeneities at Schottky contacts10.1063/1.347243 ↗
29. Ambipolar conduction behavior on high performance Schottky barrier source/drain gate-all-around Si nanowire nonvolatile SONOS memory10.1149/2.019205jss ↗