journal article·2016-10

Sigmoid-growth curve of lattice-constant against annealing-temperature of Cd1−xZnxTe thin films and its structural, optical and morphological characteristics

Monisha Chakraborty, Sugata Bhattacharyya

Publisher page

Abstract

Abstract Stacked CdTe/Zn/CdTe layers were deposited on glass substrates. The vacuum-evaporated thin films were subsequently annealed in vacuum ambience at various temperatures. Change in lattice-constant of major Cd1−xZnxTe planes against temperature was plotted from the XRD results. The graphs followed sigmoid-growth model and were regressed well by standard Boltzmann and Logistic functions. Lattice-constant varied maximum in between 375–400 °C and 425–450 °C, giving two separate growth trends. Optical studies suggested that presence of charge impurities and defects reduced the transmittance and band-gap values of the samples. Such reduction occurred, despite of greater formation of Cd1−xZnxTe. Decreasing granularity was however associated with increasing band-gap for samples annealed at 425 and 450 °C. SEM micrographs showed that granularity decreased significantly for samples annealed at higher temperatures. EDX results were further used to co-relate the compositional characteristics with structural and optical features.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Semiconductor Detectors and Materials · Chalcogenide Semiconductor Thin Films · Quantum Dots Synthesis And Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Martín-Martín · Radiat. Prot. Dosim. · 2009 · 133 · 19310.1093/rpd/ncp038 ↗
2. Prokesch · IEEE Trans. Nucl. Sci. · 2010 · 57 · 239710.1109/TNS.2010.2049120 ↗
3. Sordo · Sensors · 2009 · 9 · 349110.3390/s90503491 ↗
4. Carvalho · Phys. Rev. B · 2010 · 81 · 07521510.1103/PhysRevB.81.075215 ↗
5. Szczerbakow · Cryst. Res. Technol. · 2010 · 45 · 89510.1002/crat.201000237 ↗
6. Ganguly · Appl. Surf. Sci. · 2010 · 256 · 487910.1016/j.apsusc.2010.02.076 ↗
7. Gamal · J. Alloy. Compd. · 2007 · 431 · 3210.1016/j.jallcom.2006.05.042 ↗
8. Scheiber · Nucl. Instrum. Methods Phys. Res. A · 2001 · 458 · 1210.1016/S0168-9002(00)01032-9 ↗
9. D. Shvydka, X. Jin, E.I. Parsa, IJMPCERO, http://dx.doi.org/10.4236/ijmpcero.2013.23014.10.4236/ijmpcero.2013.23014 ↗
10. S. Kang, B. Jung, S. Noh, C. Cho, I. Yoon, J. Park, J. Instrum., http://dx.doi.org/10.1088/1748-0221/7/01/C0101010.1088/1748-0221/7/01/C01010 ↗
11. Kim · TRANSEEM · 2003 · 4 · 15
12. Nasieka · Nucl. Instrum. Methods Phys. Res. A · 2011 · 64810.1016/j.nima.2011.06.040 ↗
13. 〈www.dtic.mil/cgi-bin/GetTRDoc?AD=ADA366608〉.
14. Prabakar · Sol. Energy Mater. Sol. Cells · 2004 · 81 · 110.1016/j.solmat.2003.08.008 ↗
15. Prabakar · Matter Chem. Phys. · 2003 · 78 · 80910.1016/S0254-0584(02)00388-7 ↗
16. Prasada-Rao · Opt. Mater. · 1996 · 5 · 6310.1016/0925-3467(95)00041-0 ↗
17. Chack · J. Cryst. Growth · 1999 · 198–199 · 117910.1016/S0022-0248(98)01202-0 ↗
18. Sridharan · Cryst. Res. Technol. · 2004 · 39 · 32810.1002/crat.200310190 ↗
19. Kim · IEEE Trans. Nucl. Sci. · 2004 · 51 · 309410.1109/TNS.2004.839084 ↗
20. Zha · Vacuum · 2011 · 86 · 24210.1016/j.vacuum.2011.06.013 ↗
21. Tariq · Mater. Sci. Semicond. Process. · 2015 · 30 · 66510.1016/j.mssp.2014.09.012 ↗
22. Shanmugan · J. Alloy. Compd. · 2011 · 509 · 214310.1016/j.jallcom.2010.10.169 ↗
23. Chakraborty · Superlattices Microstruct. · 2015 · 86 · 32010.1016/j.spmi.2015.07.060 ↗
24. Optical properties of semiconductor
25. El-Nahass · J. Alloy. Compd. · 2014 · 604 · 25310.1016/j.jallcom.2014.03.104 ↗
26. Banerjee · Thin Solid Films · 2013 · 531 · 20310.1016/j.tsf.2013.01.071 ↗