journal article·2021-06

Effects of different cusp magnetic ratios and crucible rotation conditions on oxygen transport and point defect formation during Cz silicon crystal growth

Thi-Hoai-Thu Nguyen, Jyh-Chen Chen

Publisher page

Abstract

Abstract The effects of different crucible counter- and iso-rotation rates and cusp magnetic ratios (MRs) on the melt flow, temperature, oxygen content, and point defect formation during the growth of a 5-inch diameter silicon crystal are discussed numerically. In cases without a cusp magnetic field (CMF), the oxygen content gets smaller at a low crucible rotation speed than at a high one, for both counter- and iso-rotation conditions. This trend is reversed under a CMF. The flow field is controlled by the crucible rotation rate, the rotation direction between the crucible and the crystal, and the MR. Since the melt flow motion is retarded by the Lorentz force at a high MR, diffusion has a greater effect on oxygen transport in the bulk melt. It promotes the transport of oxygen atoms from the crucible wall towards the melt surface and the growth interface. The point defect density is quite dependent on the thermal field arising from changes in the growth interface shape. Microdefects in the silicon crystal can be reduced in density and enhanced in the radial uniformity using a high crucible iso-rotation rate and high unbalanced MR. A flatter shape of growth interface can be obtained under these growth conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Solidification and crystal growth phenomena · Metallurgical Processes and Thermodynamics · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Effect of asymmetric magnetic field on crystal-melt interface in silicon Cz process10.1016/j.jcrysgro.2012.11.050 ↗
2. Thermally induced microdefects in Czochralski-grown silicon crystal10.1016/0022-0248(82)90474-2 ↗
3. Effects of dislocation and bulk micro defects on device leakage
4. Numerical investigation of the effect of heat shield shape on the oxygen impurity distribution at the crystal–melt interface during the process of Czochralski silicon crystal growth10.1016/j.jcrysgro.2011.12.070 ↗
5. Numerical simulation of the effect of heater position on the oxygen concentration in the CZ silicon crystal growth process10.1155/2012/395235 ↗
6. Numerical simulation of oxygen transport during the CZ silicon crystal growth process10.1016/j.jcrysgro.2010.11.145 ↗
7. Application of dynamic and combined magnetic fields in the 300mm silicon single-crystal growth10.1016/S1369-8001(02)00134-8 ↗
8. Active control of melt convection of silicon by electromagnetic force under cusp-shaped magnetic fields10.1016/S1369-8001(02)00135-X ↗
9. Transient global modeling for the pulling process for the Czochralski silicon crystal growth. I. Principles, formulation, and implementation of the model
10. Numerical simulation of oxygen transport during the Czochralski silicon crystal growth with a cusp magnetic field10.1016/j.jcrysgro.2013.10.040 ↗
11. Effects of cusp-shaped magnetic field on melt convection and oxygen transport in an industrial CZ-Si crystal growth10.1016/j.jcrysgro.2012.06.004 ↗
12. Global analysis of effects of magnetic field configuration on melt–crystal interface shape and melt flow in Cz-Si crystal growth10.1016/j.jcrysgro.2004.11.292 ↗
13. Analysis of the effect of symmetric/asymmetric cusp magnetic fields on melt/crystal interface during Czochralski silicon growth
14. Effects of crystal-crucible iso-rotation and a balanced/unbalanced cusp magnetic field on the heat, flow, and oxygen transport in a Czochralski silicon melt10.1016/j.jcrysgro.2019.125373 ↗
15. Effect of zero-Gauss plane and magnetic intensity on oxygen concentration in cusp-magnetic Cz crystals10.1016/j.jcrysgro.2006.06.044 ↗
16. The effects of several growth parameters on the formation behavior of point defects in Czochralski-grown silicon crystals10.1016/j.jcrysgro.2006.04.023 ↗
17. Flow and temperature field in molten silicon during Czochralski crystal growth in a cusp magnetic field10.1016/S0022-0248(98)00529-6 ↗
18. Use of an inhomogeneous magnetic field for silicon crystal growth10.1016/S0022-0248(97)00239-X ↗
19. Numerical simulation of heat and mass transfer during Czochralski silicon crystal growth under the application of crystal-crucible counter- and iso-rotations10.1016/j.jcrysgro.2018.10.049 ↗
20. Numerical study on the effect of operating parameters on point defects in a silicon crystal during Czochralski growth, I. Rotation effect10.1016/S0022-0248(00)00637-0 ↗
21. Effect of location of zero gauss plane on oxygen concentration at crystal melt interface during growth of magnetic silicon single crystal using Czochralski technique10.1016/j.protcy.2016.03.053 ↗
22. Three-dimensional numerical simulation of flow, thermal and oxygen distributions for a Czochralski silicon growth within a transverse magnetic field10.1016/j.jcrysgro.2014.01.028 ↗
23. Numerical simulation of the oxygen concentration distribution in silicon melt for different crystal lengths during Czochralski growth with a transverse magnetic field10.1016/j.jcrysgro.2016.03.024 ↗
24. 2011
25. Evaluating k–ε with one–equation turbulence model10.1016/j.proeng.2013.03.109 ↗
26. Three dimensional simulation of melt flow un Cz crystal growth with steady magnetic field10.1016/j.jcrysgro.2011.11.029 ↗
27. Oxygen concentration in the Czochralski grown crystals with cusp-magnetic field10.1016/j.jcrysgro.2004.12.037 ↗
28. Oxygen concentration inhomogeneity in the silicon melt of the Czochralski single crystal growth system10.1007/BF03026070 ↗
29. The mechanism of swirl defects formation10.1016/0022-0248(82)90386-4 ↗
30. Vacancy and self-interstitial concentration incorporated into growing silicon crystals10.1063/1.371642 ↗
31. Prediction of bulk defects in CZSi crystals using 3D unsteady calculations of melt convection10.1016/S1369-8001(02)00132-4 ↗
32. Systematic study of the influence of the Czochralski hot zone design on the point defect distribution with respect to a ‘‘perfect’’ crystal10.1016/S1369-8001(02)00120-8 ↗