journal article·2017-06

On the metallic bonding of GaN-based vertical light-emitting diode

M.A. Khan, P.W. Trimby, H.W. Liu, R.K. Zheng

Publisher page

Abstract

Abstract In this work, metallic bonding in GaN-based vertical light-emitting diode (VLED) is systematically characterized by using combined methodology of transmission Kikuchi diffraction (TKD) and energy dispersive X-ray spectroscopy (EDS) in a scanning electron microscope (SEM). SEM-based TKD with EDS identifies chemical composition, grain morphology, orientation, and phases at metallic bonding, while transmission electron microscopy (TEM) provides nanoscale characteristics of metallic diffusion bonding, and its interface-related defects and nano-twinned boundaries. Our results from SEM-TKD and TEM techniques provide unparalleled insight into the metallic bonding, and its future optimization.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: GaN-based semiconductor devices and materials · Semiconductor materials and devices · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (80)

Show source-provided references
1. Materials integration of gallium arsenide and silicon by wafer bonding10.1063/1.121586 ↗
2. Integration of optical interconnects and optoelectronic elements on wafer-scale10.1016/S1369-8001(00)00070-6 ↗
3. 2004
4. Dragoi · 2009 · 215
5. Colinge · 2010
6. High-brightness GaN-based light-emitting diodes on Si using wafer bonding technology10.1143/APEX.4.066501 ↗
7. New challenges for 300mm Si technology: 3d interconnects at wafer scale by aligned wafer bonding10.1016/S1369-8001(02)00133-6 ↗
8. Introduction to 3D Integration
9. Wafer-level bonding/stacking technology for 3D integration10.1016/j.microrel.2009.09.015 ↗
10. Au–Sn flip-chip solder bump for microelectronic and optoelectronic applications10.1007/s00542-006-0330-9 ↗
11. N. Belov, T.K. Chou, J. Heck, K. Kornelsen, D. Spicer, S. Akhlaghi, M. Wang, T. Zhu, Thin-layer Au-Sn solder bonding process for wafer-level packaging, electrical interconnections and MEMS applications, in: Proceedings of 2009 IEEE International Interconnect Technol. Conference, 2009, pp. 128–130. 〈doi:10.1109/IITC.2009.5090361〉.10.1109/IITC.2009.5090361 ↗
12. V. Dragoi, G. Mittendorfer, J. Burggraf, M. Wimplinger, Metal Thermocompression Wafer Bonding for 3D Integration and MEMS Applications, 2010, pp. 27–35. doi:10.1149/1.3483491.10.1149/1.3483491 ↗
13. R.-H. Horng, C.-H. Chen, W.-C. Kao, D.-S. Wuu, High-yield thin GaN LED using metal bonding and laser lift-off technology, in: M.H. Kane, C. Wetzel, J.-J. Huang, I.T. Ferguson (Eds.), 2012, p. 84841H. http://dx.doi.org/10.1117/12.930287.10.1117/12.930287 ↗
14. The Au-Sn phase diagram10.1016/0925-8388(93)90273-P ↗
15. W. Kim, Q. Wang, K. Jung, J. Hwang, C. Moon, Application of Au-Sn eutectic bonding in hermetic RF MEMS wafer level packaging, in: Proceedings of the 9th International Symp. Adv. Packag. Mater. Process. Prop. Interfaces, 2004, pp. 215–219. 〈doi:10.1109/ISAPM.2004.1288016〉.10.1109/ISAPM.2004.1288016 ↗
16. Z. Ling, N.S. Ching, L. Zheng, F.S. Nong, T. Nguty, E. de Bruin, A. Xiao, H. Thoonen, Development of advanced AuSn alloy plating technology for semiconductor application, in: Proceedings of the 15th International Conference Electron. Packag. Technol. ICEPT, 2014, pp. 113–116. 〈doi:10.1109/ICEPT.2014.6922616〉.10.1109/ICEPT.2014.6922616 ↗
17. Au-Sn (gold-tin)
18. Au-Sn SLID bonding: a reliable HT interconnect and die attach technology10.1007/s11663-012-9789-1 ↗
19. Study on the gold-gold thermocompression bonding for wafer-level packaging10.4028/www.scientific.net/AMR.60-61.325 ↗
20. N. Malik, K. Schjolberg-Henriksen, E. Poppe, T.G. Finstad, Al-Al thermocompression bonding for wafer-level MEMS packaging, in: IEEE, 2013, pp. 1067–1070. 〈doi:10.1109/Transducers.2013.6626955〉.10.1109/Transducers.2013.6626955 ↗
21. Strong, high-yield and low-temperature thermocompression silicon wafer-level bonding with gold10.1088/0960-1317/14/7/007 ↗
22. Interfacial characterization of Al-Al thermocompression bonds10.1063/1.4952709 ↗
23. Copper wafer bonding10.1149/1.1390894 ↗
24. C.H. Tsau, M.A. Schmidt, S.M. Spearing, Characterization of Low Temperature, Wafer-Level Gold-Gold Thermocompression Bonds, MRS Online Proceedings Libr. Arch. /core/journals/mrs-online-proceedings-library-archive/article/characterization-of-low-temperature-wafer-level-gold-gold-thermocompression-bonds/554794A9323DD1E36FAC8FE5EB7C6B5E [Accessed 13 November 2016], 1999.
25. V. Dragoi, E. Pabo, Wafer bonding process selection, 2010, pp. 509–517. http://dx.doi.org/10.1149/1.3483542.10.1149/1.3483542 ↗
26. Z. Chen, Buffer layer for GaN-on-Si LED, US8686430 B2. 〈http://www.google.com/patents/US8686430〉 [accessed 11 April 2016), 2014.
27. Fabrication of wafer-level thermocompression bonds10.1109/JMEMS.2002.805214 ↗
28. Characterization of wafer-level thermocompression bonds10.1109/JMEMS.2004.838393 ↗
29. Development of high-efficiency and high-power vertical light emitting diodes10.7567/JJAP.53.100208 ↗
30. GaN/mirror/Si light-emitting diodes for vertical current injection by laser lift-off and wafer bonding techniques10.1143/JJAP.43.5239 ↗
31. Enhanced light extraction of GaN-based vertical LEDs with patterned trenches and nanostructures10.1016/j.mssp.2016.09.036 ↗
32. Characterization of large-area AlGaInP/mirror/Si light-emitting diodes fabricated by wafer bonding10.1143/JJAP.43.2510 ↗
33. Enhanced external quantum efficiency in GaN-based vertical-type light-emitting diodes by localized surface plasmons10.1038/srep22659 ↗
34. D. Lauvernier, D. Van Thourhout, C. Detavernier, R. Baets, Metal bonding with ultra-thin layer for optical applications, in: Proceedings 12th Annu. Symp. IEEELEOS Benelux Chapter, 2007, pp. 79–82. 〈https://biblio.ugent.be/publication/393238/file/587055.PDF〉 [accessed 31 May 2016].
35. Assembly and packaging technologies for high-temperature and high-power GaN devices10.1109/TCPMT.2015.2468595 ↗
36. Wafer-to-wafer bonding for microstructure formation10.1109/5.704262 ↗
37. Enhanced semi-empirical potentials in molecular dynamics simulations of wafer bonding10.1016/S1369-8001(00)00020-2 ↗
38. Controlling the microstructure from the gold-tin reaction10.1007/s11664-005-0231-1 ↗
39. Effect of the silver content of SnAgCu solder on the interfacial reaction and on the reliability of angle joints fabricated by laser-jet soldering10.1007/s11664-014-3516-4 ↗
40. Characterizing deformed ultrafine-grained and nanocrystalline materials using transmission Kikuchi diffraction in a scanning electron microscope10.1016/j.actamat.2013.09.026 ↗
41. A. Chitnis, Permanent wafer bonding using metal alloy preform discs, US20080096365 A1. 〈http://www.google.com/patents/US20080096365〉 [Accessed 17 February 2017], 2008.
42. The lattice spacing relationships in close-packed α and ζ phases based on gold10.1016/0001-6160(60)90198-X ↗
43. Thermal expansion and elastic properties of high gold-Tin alloys10.1007/BF02647236 ↗
44. Au-Sn SLID bonding—properties and possibilities10.1007/s11663-011-9609-z ↗
45. Au-Sn bonding metallurgy of TAB contacts and its influence on the Kirkendall effect in the ternary Cu-Au-Sn10.1109/33.232060 ↗
46. Gusev · 2010
47. EBSD Oxford Instruments - Home, (n.d.). 〈http://www.ebsd.com/〉 [Accessed 17 November 2016].
48. Mechanical properties of intermetallic compounds in the Au–Sn system10.1557/JMR.2005.0269 ↗
49. Solidification and interfacial interactions in gold–tin system during eutectic or thermo-compression bonding for 200 mm MEMS wafer level hermetic packaging10.1007/s10854-013-1515-5 ↗
50. W.D. Callister, D.G. Rethwisch, Materials Science and Engineering: An Introduction, 9th Edition 〈https://books.google.com.au/books?Id=TmxbAgAAQBAJ〉, 2013.
51. Mechanical properties of bulk ultrafine grained aluminum fabricated by torsion deformation at various temperatures and strain rates10.2320/matertrans.MA201321 ↗
52. Tougher ultrafine grain Cu via high-angle grain boundaries and low dislocation density10.1063/1.2870014 ↗
53. Influence of grain size on electrical and optical properties of InP films10.1088/0256-307X/25/11/069 ↗
54. Electronic properties of twin boundaries and twinning superlattices in diamond-type and zinc-blende-type semiconductors10.1103/PhysRevB.48.17181 ↗
55. The influence of ∑3 twin boundaries on the formation of radiation-induced defect clusters in nanotwinned Cu10.1557/jmr.2011.56 ↗
56. Role of twin boundaries in semiconductor to metal transition characteristics of VO2 films10.1063/1.3481075 ↗
57. Electromigration in thin silver, copper, gold, indium, tin, lead and magnesium films10.1016/S0022-3697(72)80101-X ↗
58. Kim · 2011
59. Li · 2015 · 1
60. High strength, epitaxial nanotwinned Ag films10.1016/j.actamat.2010.09.011 ↗
61. Thermal stability of twins and strengthening mechanisms in differently oriented epitaxial nanotwinned Ag films10.1557/jmr.2013.50 ↗
62. Wafer-level SLID bonding for MEMS encapsulation10.1007/s40436-013-0035-0 ↗
63. Aging effects in gold thermocompression bonds to complex metallizations10.1109/TR.1970.5216376 ↗
64. Grain size and interface dependence of bias stress stability of n-type organic field effect transistors10.1021/acsami.5b06210 ↗
65. M. Krause, M. Muller, M. Petzold, S. Wiese, K.-J. Wolter, Scaling effects on grain size and texture of lead free interconnects #x2014; investigations by electron backscatter diffraction and nanoindentation, in: Electron. Compon. Technol. Conference 2008 ECTC 2008 58th, 2008, pp. 75–81. 〈doi:10.1109/ECTC.2008.4549953〉.10.1109/ECTC.2008.4549953 ↗
66. M.A. Khan, R.K. Zheng, Nanostructural Analysis of CMOS-MEMS-based Digital Microphone for Performance Optimization, (n.d.). 〈doi:10.1109/TNANO.2016.2554602〉.10.1109/TNANO.2016.2554602 ↗
67. Nanostructural analysis of CMOS-MEMS-based digital microphone for performance optimization10.1109/TNANO.2016.2554602 ↗
68. Effect of copper–copper direct bonding on voiding in metal thin films10.1007/s11664-015-3992-1 ↗
69. Voiding Phenomena in copper-copper bonded structures: role of creep10.1149/06405.0357ecst ↗
70. K.E. Aasmundtveit, T.A. Tollefsen, T.T. Luu, A. Duan, K. Wang, N. Hoivik, Solid-Liquid Interdiffusion (SLID) bonding #x2014; Intermetallic bonding for high temperature applications, in: 2013 Eurpoean Microelectron. Packag. Conference EMPC, 2013, pp. 1–6.
71. Reliability study of Au-in solid-liquid interdiffusion bonding for GaN-based vertical LED packaging10.1088/0960-1317/25/12/127002 ↗
72. Doan · 2006
73. High brightness GaN vertical light-emitting diodes on metal alloy for general lighting application10.1109/JPROC.2009.2037026 ↗
74. Critical temperatures in thermocompression gold stud bonding10.1063/1.2783974 ↗
75. Natural substrate lift-off technique for vertical light-emitting diodes10.7567/APEX.7.042103 ↗
76. Platinum diffusion barrier breakdown in a-Si/Au eutectic wafer bonding10.1109/TCPMT.2013.2239363 ↗
77. Aging effects in gold thermocompression bonds to complex metallizations10.1109/TR.1970.5216376 ↗
78. A novel bonding approach and its electrical performance for flexible substrate integration10.1109/JEDS.2016.2537359 ↗
79. A.Q.A. Qureshi, S. Colpo, D.A. Vasilache, S. Girardi, P. Conci, B. Margesin, Thermocompression bonding for 3D RF MEMS devices using gold and silver as intermediate layer, in: CAS 2012 International Semicond. Conference, 2012, pp. 183–186. doi:10.1109/SMICND.2012.6400660.10.1109/SMICND.2012.6400660 ↗
80. Atom probe tomography on semiconductor devices10.1002/admi.201500713 ↗