journal article·2017-03

Normally-off AlGaN/AlN/GaN/Si oxide-passivated HEMTs and MOS-HEMTs by using CF4 plasma and ozone water oxidization treatment

Ching-Sung Lee, Han-Yi Liu, Wei-Chou Hsu, Si-Fu Chen

Publisher page

Abstract

Abstract The letter reports normally-off device characteristics of Al0.26Ga0.74N/AlN/GaN oxide-passivated high electron mobility transistors (HEMTs) and metal-oxide-semiconductor HEMTs (MOS-HEMTs) grown on a Si substrate. Al2O3 was formed as the surface passivation oxide or gate dielectric on a thin AlGaN barrier layer by using a cost-effective ozone water oxidization technique. CF4 plasma was used to enable normally-off operation. For the gate dimensions of 1×100 µm2, the present oxide-passivated HEMT and MOS-HEMT (a control Schottky-gate HEMT) have demonstrated superior on/off-current ratio (Ion/Ioff) of 2.5×106 and 1×107 (3.9×103), maximum extrinsic transconductance (gm, max) of 154 and 175 (120) mS/mm, maximum drain-source current density (IDS, max) of 312 and 349 (300) mA/mm, two-terminal gate-drain breakdown voltage (BVGD) of −80 and −140 (−36) V, turn-on voltage (Von) of 1.2 and 1.3 (1) V, and three-terminal on-state breakdown voltage (BVDS) of 93 and 109 (48) V. Excellent BVGD and BVDS enhancements of 122% (288%) and 94% (127%) are achieved in the present oxide-passivated HEMT (MOS-HEMT) design.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: GaN-based semiconductor devices and materials · Ga2O3 and related materials · Semiconductor Quantum Structures and Devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Lv · Nanoscale Res. Lett. · 2016 · 11 · 37310.1186/s11671-016-1591-6 ↗
2. Huang · Appl. Phys. Lett. · 2015 · 106 · 03350710.1063/1.4906601 ↗
3. Hansen · J. Vac. Sci. Technol. B · 2005 · 23 · 49910.1116/1.1868672 ↗
4. Gregušova · Semicond. Sci. Technol. · 2007 · 22 · 94710.1088/0268-1242/22/8/021 ↗
5. Chou · IEEE Electron Device Lett. · 2014 · 35 · 109110.1109/LED.2014.2354643 ↗
6. Brown · IEEE Electron Device Lett. · 2014 · 35 · 90610.1109/LED.2014.2334394 ↗
7. Wang · IEEE Electron Device Lett. · 2013 · 34 · 137010.1109/LED.2013.2279844 ↗
8. H.Y. Liu, C.W. Lin, W.C. Hsu, C.S. Lee, M.H. Chiang, W.C. Sun, S.W. Wei, and S.M. Yu, Accepted and to be published in IEEE Electron Device Lett 2017.
9. K.Ota, K.Endo, Y.Okamoto, Y.Ando, H.Miyamoto, H.Shimawaki in: Proceedings of the IEEE International Electron Devices Meeting (IEDM), vol. 9, 2009, pp. 153–156.
10. Zhang · IEEE Electron Device Lett. · 2015 · 36 · 112810.1109/LED.2015.2483760 ↗
11. Liu · IEEE Trans. Electron. Devices · 2013 · 60 · 223110.1109/TED.2013.2260753 ↗
12. S.F. Chen, M.S. thesis, Dept. Electron. Eng., Feng Chia Univ., Taichung City, Taiwan, Jun, 2016.
13. Vetury · IEEE Trans. Electron Devices · 2001 · 48 · 56010.1109/16.906451 ↗
14. Im · IEEE Electron Device Lett. · 2010 · 31 · 19210.1109/LED.2009.2039024 ↗
15. Kambayashi · IEEE Electron Device Lett. · 2007 · 28 · 107710.1109/LED.2007.909978 ↗