journal article·2024-10Open access

Effect of grain size on tungsten material removal rate during chemical mechanical planarization process

Haoqi Liu, Tao Yang, Yue Zhang, Yihong Lu, Jianfeng Gao, Junfeng Li, Jun Luo

Abstract

The effect of grain size on the tungsten (W) material removal rate (MRR) was studied during chemical mechanical planarization (CMP) process in this paper. It was found that the average grain size of atomic layer deposition (ALD) W was significantly smaller than that of chemical vapor deposition (CVD) W by TEM and SEM analysis . The MRR of ALD W with small grain size was higher than that of CVD W with large grain size. The static etch rate and XPS results indicated that the W film with smaller grain size had a higher oxidation rate , which were further demonstrated by the analysis of potentiodynamic polarization and the electrochemical impedance spectroscopy (EIS). This can be explained that W film with smaller grain size has a higher grain boundary density, leading to easier oxidizers diffusion along the grain boundaries and faster oxidation in the W film surface consequently. According to the oxidation-removal model, it is concluded that smaller grain size facilitates faster oxidation on the W film surface, leading to higher material removal rates during W CMP process.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Application of atomic layer deposition tungsten (ALD W) as gate filling metal for 22 nm and beyond nodes CMOS technology10.1149/2.015404jss ↗
2. Studies on passivation behavior of tungsten in application to chemical mechanical polishing10.1116/1.581790 ↗
3. Atomic layer deposition (ALD) of metal gates for CMOS10.3390/app9112388 ↗
4. Comparison of NBTI kinetics in RMG Si p-FinFETs featuring atomic layer deposition tungsten (ALD W) filling metal using B2H6 and SiH 4 precursors
5. pMOSFETs featuring ALD W filling metal using SiH4 and B2H6 precursors in 22 nm node CMOS technology10.1186/s11671-017-2080-2 ↗
6. Steigerwald · 1997
7. Effect of iron(III) nitrate concentration on tungsten chemical-mechanical-planarization performance10.1016/j.apsusc.2013.06.003 ↗
8. Chemical‐mechanical polishing for Fabricating Patterned W metal features as Chip Interconnects10.1149/1.2085434 ↗
9. Tungsten passivation layer (WO3) formation mechanisms during chemical mechanical planarization in the presence of oxidizers10.1016/j.apsusc.2020.147862 ↗
10. Effects of oxidants on the removal of tungsten in CMP process10.1016/j.wear.2004.02.007 ↗
11. Effect of particle size during tungsten chemical mechanical polishing10.1149/1.1390851 ↗
12. In Situ electrochemical investigation of tungsten electrochemical behavior during chemical mechanical polishing10.1149/1.1838785 ↗
13. Atomic force microscopy, lateral force microscopy, and transmission electron microscopy investigations and adhesion force measurements for elucidation of tungsten removal mechanisms10.1557/JMR.1999.0499 ↗
14. Investigation of the kinetics of tungsten chemical mechanical polishing in potassium iodate‐based slurries: II. Roles of colloid species and slurry chemistry10.1149/1.1391869 ↗
15. Impact of film morphology on chemical mechanical polishing of tungsten10.1149/2.0371606jss ↗
16. Effect of CVD temperature on orientation, roughness, and chemical mechanical polish removal rate of W thin films10.1149/1.1518991 ↗
17. Homogeneous tungsten chemical vapor deposition on silane pretreated titanium nitride10.1149/1.1390850 ↗
18. Interface formation between Be and W layers depending on its thickness and ordering10.1016/j.apsusc.2020.147636 ↗
19. Lassner · Tungsten · 199910.1007/978-1-4615-4907-9 ↗
20. Electrochemistry of chemical vapor deposited tungsten films with relevance to chemical mechanical polishing10.1149/1.1837342 ↗
21. The influence of pH and H2O2 on surface quality and material removal rate during W-CMP10.1007/s00170-023-11805-3 ↗
22. Effect of pH on the anodic behavior of tungsten10.1149/1.1471544 ↗
23. The kinetics of oxide film formation on metals and alloys10.1149/1.3071793 ↗
24. Grain boundaries in nanocrystalline catalytic materials as a source of surface chemical functionality10.1515/revce-2014-0011 ↗
25. Enhanced chemical reactions of oxygen at grain boundaries in polycrystalline graphene10.1016/j.poly.2013.03.032 ↗
26. Application of ALD W films as gate filling metal in 22nm HKMG-last integration: evaluation and improvement of the adhesion in CMP process10.1016/j.mee.2015.01.007 ↗
27. Investigation of cu-BTA complex formation during Cu chemical mechanical planarization process10.1016/j.apsusc.2016.05.106 ↗
28. R. Huggins, Simple Method to Determine Electronic Conductivity in Mixed A Review.
29. Enhanced ionic conductivity in LAGP/LATP composite electrolyte10.1088/1674-1056/27/3/038201 ↗
30. Effect of pH value and Glycine in alkaline CMP slurry on the corrosion of aluminum by electrochemical analysis10.1149/2.0221906jss ↗
31. Characterization of different cobalt surfaces and interactions with benzotriazole for CMP application10.1149/2162-8777/aba331 ↗
32. A method to separate process contributions in impedance spectra by variation of test conditions10.1149/1.2790791 ↗