Defects annealing in 4H–SiC epitaxial layer probed by low temperature photoluminescence
Source abstract
Abstract
Abstract The thermal evolution of defects induced in 4H–SiC by multiple implantation of C ions was investigated by Low Temperature Photoluminescence in the temperature range 450–1000 K. The photoluminescence spectra show sharp luminescent lines (alphabet lines) in the wavelength range 426–440 nm upon irradiation and thermal treatment at 450 K induces the appearance of a new line at 427 nm ( D I centre). The trend shown by the luminescence lines as a function of the temperature is quite complex. The alphabet lines intensity increases up to 850 K, whereas at higher temperature decreases with an activation energy of 2.0 eV, suggesting that the defect, responsible for these lines, is the Si-vacancy. The luminescence yield of D I centre is always increasing as a function of the temperature, with a higher slope from 750 K, suggesting a correlation to the reconfiguration and to the annealing of point defects.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon Carbide Semiconductor Technologies · Semiconductor materials and devices · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. SiC materials and devices
2. Matsunami · Japanese Journal of Applied Physics · 2004 · 43 · 683510.1143/JJAP.43.6835 ↗
3. Hallen · Nuclear Instruments and Methods B · 2002 · 186 · 18610.1016/S0168-583X(01)00880-1 ↗
4. Saks · Applied Physics Letters · 2002 · 81 · 495810.1063/1.1531838 ↗
5. Litrico · Radiation Effects and Defects in Solids · 2011 · 166 · 48010.1080/10420150.2011.569718 ↗
6. Yan · Applied Physics Letters · 2012 · 100 · 13210710.1063/1.3699269 ↗
7. Alfieri · Material Science Forum · 2011 · 679 · 25310.4028/www.scientific.net/MSF.679-680.253 ↗
8. Beyer · Material Science Forum · 2011 · 679 · 24910.4028/www.scientific.net/MSF.679-680.249 ↗
9. Von Bardeleben · Physical Review B · 2003 · 62 · 1084110.1103/PhysRevB.62.10841 ↗
10. Henry · Physica Scripta · 2005 · 72 · 25410.1238/Physica.Regular.072a00254 ↗
11. Negoro · Applied Physics Letters · 2004 · 8 · 171610.1063/1.1790032 ↗
12. Rüschenschmidt · Journal of Applied Physics · 2004 · 96 · 145810.1063/1.1766101 ↗
13. Bedoya-Martínez · Physical Review B · 2010 · 82 · 13411510.1103/PhysRevB.82.134115 ↗
14. Lefèvre · Journal of Applied Physics · 2009 · 106 · 08350910.1063/1.3245397 ↗
15. Itoh · Journal Applied Physics · 1989 · 66 · 452910.1063/1.343920 ↗
16. David · Journal Applied Physics · 2004 · 95 · 472810.1063/1.1689731 ↗
17. Storasta · Journal Applied Physics · 2004 · 96 · 490910.1063/1.1778819 ↗
18. Egilsson · Physical Review B · 1999 · 59 · 800810.1103/PhysRevB.59.8008 ↗
19. Litrico · Diamond and Related Materials · 2009 · 18 · 3910.1016/j.diamond.2008.08.011 ↗
20. Choyke · Physical Review B · 1971 · 4 · 184310.1103/PhysRevB.4.1843 ↗
21. Egilsson · Physical Review B · 1999 · 59 · 195610.1103/PhysRevB.59.1956 ↗
22. Sridhara · Journal of Applied Physics · 1998 · 84 · 296310.1063/1.368403 ↗
23. Eberlein · Physical Review B · 2002 · 65 · 18410810.1103/PhysRevB.65.184108 ↗
24. Eberlein · Physical Review B · 2006 · 74 · 14410610.1103/PhysRevB.74.144106 ↗
25. Storasta · Applied Physics Letters · 2005 · 86 · 09190310.1063/1.1811381 ↗
26. Zolnai · Materials Science Forum · 2004 · 457 · 47310.4028/www.scientific.net/MSF.457-460.473 ↗