Impact of the temperature process on the morphology of 3D temporary bonded wafers: Quantification and reducing of the effect
Source abstract
Abstract
Abstract 300 mm diameter thinned-down wafers are manufactured using temporary adhesive bonding. A thermoplastic adhesive and a silicon carrier are used to fabricate 100 μm thick silicon wafers. The impact of temperature on the thickness homogeneity of temporary bonded stacks is studied. From 150 °C up to 300 °C, the total thickness of the structure increases with the temperature. Moreover, its amplitude strongly increases with the thinned wafer stress and the adhesive thickness. On the contrary, it does not depend on the different interface adherence. The thinned wafer stress results in a significant peeling force which drives the deformation of the structure. This deformation is possible because of the high elasticity of the polymer at high temperature. To reduce this deformation, an alternative carrier is proposed yielding reduction of the adhesive thickness at the bonded edge only.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: 3D IC and TSV technologies · Nanofabrication and Lithography Techniques · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Adhesive wafer bonding10.1063/1.2168512 ↗
2. Fine keyed alignment and bonding for wafer-level 3D ICs
3. Die-on-wafer and wafer-level three-dimensional (3D) integration of heterogeneous IC technologies for RF-microwave-millimeter applications10.1557/PROC-833-G6.8 ↗
4. Fabrication of a microfluidic chip by UV bonding at room temperature for integration of temperature-sensitive layers10.1088/0960-1317/13/4/313 ↗
5. Wafer-scale microdevice transfer/interconnect: its application in an AFM-based data-storage system10.1109/JMEMS.2004.835769 ↗
6. A method for UV-bonding in the fabrication of glass electrophoretic microchips10.1002/1522-2683(200110)22:18<3924::AID-ELPS3924>3.0.CO;2-4 ↗
7. PMMA to SU-8 bonding for polymer based lab-on-a-chip systems with integrated optics10.1088/0960-1317/14/6/008 ↗
8. BCB contact printing for patterned adhesive full-wafer bonded 0-level packages10.1109/JMEMS.2004.839030 ↗
9. A low-temperature wafer bonding technique using patternable materials10.1088/0960-1317/12/5/315 ↗
10. Hybrid integration of III-V optoelectronic devices on Si platform using BCB10.1117/12.479453 ↗
11. Application of temporary adherence to improve the manufacturing of 3D thin silicon wafers10.1016/j.ijadhadh.2019.03.009 ↗
12. Micromachines packaging for chemical microsensors10.1109/16.2532 ↗
13. Vertically coupled microring resonators using polymer wafer bonding10.1109/68.903217 ↗
14. Bonding characterization of oxidized PDMS thin films
15. Wafer-scale microdevice transfer/interconnect: its application in an AFM-based data-storage system10.1109/JMEMS.2004.835769 ↗
16. Silicon wafer-to-wafer bonding at T-less-than-200-degrees-C with polymethylmethacrylate10.1063/1.112326 ↗
17. Flain · 2009
18. Temporary bonding of wafer to carrier for 3D-wafer level packaging
19. Wafer backside thinning process integrated with post-thinning clean and TSV exposure recess etch10.1149/1.3694407 ↗
20. Fine-pitch backside via-last TSV process with optimization on temporary glue and bonding conditions
21. Z. Wang, 3-D integration and through-silicon vias in MEMS and microsensors, J. Microelectromech. Syst., Vol 24–5, pp 1211-1244.10.1109/JMEMS.2015.2448681 ↗
22. P. Montméat, L. Bally, J. Dechamp, T. Enot and F. Fournel, Temporary polymer bonding for the manufacturing of thin wafers: an innovative low temperature process, Mater. Sci. Semicond. Process., 123(2021), 105550.10.1016/j.mssp.2020.105550 ↗
23. Origin of the TTV of thin films obtained by temporary bonding ZoneBond® technology10.1007/s00542-015-2431-9 ↗
24. K. Abadie P; Montméat, F. Fournel and M. Wimplinger, Test vehicle development and comparison of thermoplastic adhesives in temporary bonding, 2016 6th Electronic System-Integration Technology Conference, ESTC 20167764688.
25. https://www.brewerscience.com/wp-content/uploads/2016/05/BrewerBOND-305-Data-Sheet.pdf.
26. Warping of silicon wafers subjected to back-grinding process10.1016/j.precisioneng.2014.10.009 ↗
27. Schroder · 2016 · 450
28. Klug · 2009 · S 1 AND 2 · 814
29. Fine grinding of silicon wafers: machine configurations for spindleangle adjustments10.1016/j.ijmachtools.2004.06.013 ↗
30. Process study on large-size silicon wafer grinding by using a small-diameter wheel
31. Peeling from a biomimetically patterned thin elastic film10.1098/rspa.2004.1313 ↗
32. Peel mechanics for an elastic-plastic adherend10.1002/app.1977.070211018 ↗