Elimination of splash damage for smaller scribe widths in next-gen memory devices via stealth dicing

Dao Kun Lim, Venkata Rama Satya Pradeep Vempaty, Aibin Yu, Wen How Sim, Harjashan Veer Singh

Publisher page

Abstract

Scattered light damage (splash) is one of the common defects that can be observed from the stealth dicing process, and it is mainly due to the interaction of the pulsed laser beam with the micro-crack and modified layer formed. This might cause thermal damage on the active layer of the die and degrade the reliability and yield of the device. The development of new technology node for memory devices aims to reduce scribe width, thereby increasing the number of dies per wafer. The ongoing trend towards scribe width reduction from 120 μm to current sub-60 μm, results in increased throughput and decreased cost per die. Furthermore, this reduction allows for greater functionality integration within a confined space, thereby enhancing overall device performance. Hence, the elimination of splash during the SD process is imperative to enable further shrinking of scribe width. This paper focuses on the impact of pulse pitch and distance from 1st focal depth to silicon (Si) frontside on the maximum splash distance. Lower pulse pitch and lower distance from 1st focal depth to Si frontside will introduce higher splash distance. An empirical model for splash elimination was established to determine the critical distance from 1st focal depth to Si frontside as a function of pulse pitch.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Integrated Circuits and Semiconductor Failure Analysis · Ferroelectric and Negative Capacitance Devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Mechanical dicing challenges and development on 50um saw street with wafer backside coating (WBC)
2. Through-focus spot shaping with asymmetric pupil optimization for laser stealth dicing
3. Damage-less singulation of ultra-thin wafers using stealth dicing
4. Multistrata subsurface laser-modified microstructure with backgrind-assisted controlled fracture for defect-free ultrathin die fabrication10.1109/TCPMT.2015.2435369 ↗
5. High throughput and improved edge straightness for memory applications using stealth dicing
6. Improving throughput of zero-kerf singulation for ultra-thin wafers using stealth dicing
7. Effects of stealth dicing parameters on singulation defects and die strength
8. Fine optimization of aberration compensation for stealth dicing10.1016/j.optlastec.2024.110668 ↗
9. Comparative analysis of laser parameters effect on laser splash performance during wafer stealth dicing
10. Suppression of backside damage in stealth dicing
11. Modelling of laser absorption and modification layer formation within silicon due to stealth dicing10.1109/TCPMT.2023.3308923 ↗
12. Impact of wafer pre-thin thickness on stealth dicing performance
13. Temperature rise of silicon due to absorption of permeable pulse laser