journal article·2025-01

Investigation of the elastic-plastic evolution mechanism of 4H-SiC substrates with external thermal-assisted abrasion

Piao Zhou, Chi Fai Cheung

Publisher page

Abstract

Plastic removal is easier to achieve nanometric surfaces of monocrystalline SiC with brittleness in nano-polishing. This paper mainly focuses on the nano-scale elastic-plastic evolution mechanism of 4H-SiC substrates in thermal-assisted polishing using molecular dynamics simulation. The results show that 4H-SiC substrates undergo elastic deformation, elastic-plastic deformation, and plastic deformation in ramp nano-abrasion. The critical depth from elastic to elastic-plastic deformation rises with higher external temperature, and elastic-plastic deformation stage is compressed. Amorphization dominates the elastic recovery in elastic-plastic deformation stage. Furthermore, the step-terrace structure appears in elastic deformation stage, and is observed at a greater depth rising from 0.679 nm to 1.226 nm with increasing external temperature from 298 K to 700 K. High surface quality and subsurface damage-free of SiC substrates are performed with forming the atomic step-terrace structure.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Aluminum Alloys Composites Properties · Silicon Carbide Semiconductor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. High-temperature electronics - a role for wide bandgap semiconductors?10.1109/JPROC.2002.1021571 ↗
2. Modeling and prediction of surface topography and surface roughness in magnetic-field-enhanced shear-thickening polishing of SiC mold10.1016/j.triboint.2023.108761 ↗
3. Fundamental investigation on damage evolution and material removal mechanism in scratching anisotropic brittle material10.1016/j.triboint.2024.109764 ↗
4. Temperature effect on the material removal mechanism of soft-brittle crystals at nano/micron scale10.1016/j.ijmachtools.2020.103620 ↗
5. Investigation of the material removal process in in-situ laser-assisted diamond cutting of reaction-bonded silicon carbide10.1016/j.jeurceramsoc.2023.01.011 ↗
6. Advances in laser assisted machining of hard and brittle materials10.1016/j.jmapro.2020.08.034 ↗
7. Removal mechanism on 4H–SiC single crystal by picosecond laser ablation-assisted chemical mechanical polishing (CMP)10.1016/j.ceramint.2024.01.239 ↗
8. The study of plasma-assisted machining to Inconel-71810.1177/1687814017735789 ↗
9. A study on optimal machining conditions and energy efficiency in plasma assisted machining of Ti-6Al-4V10.3390/ma12162590 ↗
10. Plasma hot machining for new engineering materials10.1016/0043-1648(90)90049-G ↗
11. Atomic scale investigation of notch evolution on 4H-SiC under different cutting surfaces and environments10.1016/j.jmapro.2023.09.014 ↗
12. Effect of relative tool sharpness on subsurface damage and material recovery in nanometric cutting of mono-crystalline silicon: a molecular dynamics approach10.1016/j.mssp.2019.104868 ↗
13. Study on subsurface damage mechanism of gallium nitride in nano-grinding10.1016/j.mssp.2021.105760 ↗
14. Nanometric cutting: mechanisms, practices and future perspectives10.1016/j.ijmachtools.2022.103905 ↗
15. Molecular dynamics simulation of SiC removal mechanism in a fixed abrasive polishing process10.1016/j.ceramint.2019.04.180 ↗
16. Deep insights into interaction behaviour and material removal of β-SiC wafer in nanoscale polishing10.1016/j.triboint.2023.108639 ↗
17. Towards a deeper understanding of temperature-dependent material removal of single-crystal AlN: an atomistic study10.1016/j.triboint.2023.108575 ↗
18. Effects of initial temperature on the damage of GaN during nanogrinding10.1016/j.apsusc.2021.149771 ↗
19. Study on nanometer cutting mechanism of single crystal silicon at different temperatures10.1016/j.jmapro.2023.03.026 ↗
20. Atomic-scale characterization of occurring phenomena during hot nanometric cutting of single crystal 3C–SiC10.1039/C6RA05830B ↗
21. Molecular simulation of the plastic deformation and crack formation in single grit grinding of 4H-SiC single crystal10.1016/j.ijmecsci.2023.108147 ↗
22. Atomistic origin of brittle-to-ductile transition behavior of polycrystalline 3C–SiC in diamond cutting10.1016/j.ceramint.2021.05.098 ↗
23. Atomic understanding of elastic-plastic deformation and crack evolution for single crystal AlN during nanoscratch10.1016/j.ceramint.2023.08.209 ↗
24. Molecular dynamics modelling of brittle–ductile cutting mode transition: case study on silicon carbide10.1016/j.ijmachtools.2014.10.007 ↗
25. Towards understanding the crack suppression mechanism in brittle materials with high grinding speed at different temperatures10.1016/j.ijmachtools.2023.104088 ↗
26. Origin and evolution of a crack in silicon induced by a single grain grinding10.1016/j.jmapro.2022.01.037 ↗
27. Fast parallel algorithms for short-range molecular dynamics10.1006/jcph.1995.1039 ↗
28. Visualization and analysis of atomistic simulation data with OVITO–the Open Visualization Tool10.1088/0965-0393/18/1/015012 ↗
29. Effect of water film on the nano-scratching process of 4H-SiC under the constant load10.1016/j.triboint.2022.107802 ↗
30. Analytical potential for atomistic simulations of silicon, carbon, and silicon carbide
31. PNADIS: an automated Peierls–Nabarro analyzer for dislocation core structure and slip resistance10.1016/j.cpc.2019.03.005 ↗
32. Constitutive description of dynamic deformation: physically-based mechanisms10.1016/S0921-5093(01)01131-5 ↗
33. Atomic-scale study of vacancy defects in SiC affecting on removal mechanisms during nano-abrasion process10.1016/j.triboint.2019.106136 ↗
34. Molecular dynamics study on friction due to ploughing and adhesion in nanometric scratching process10.1007/s11249-010-9681-6 ↗
35. Atomic-scale smoothing of semiconducting oxides via plasma-enabled atomic-scale reconstruction10.1016/j.ijmachtools.2024.104119 ↗
36. Extended study of the atomic step-terrace structure on hexagonal SiC (0001) by chemical-mechanical planarization10.1016/j.apsusc.2013.07.080 ↗
37. A study of chemical products formed on sapphire (0001) during chemical–mechanical polishing10.1016/j.surfcoat.2015.02.053 ↗