journal article·2017-11

Ni and Ti silicide oxidation for CMOS applications investigated by XRD, XPS and FPP

M.K. Rahman, F. Nemouchi, T. Chevolleau, P. Gergaud, K. Yckache

Publisher page

Abstract

Abstract Although silicide oxidation was studied 20 years ago, the interest of obtaining a robust process for new application appears significant today. Indeed, for the new architectural development process are required dense and narrow spaces. This paper focuses to bury a silicide layer under a protective layer such as silica in order to keep constant the physical and electrical properties of silicide after oxidation. Earlier works show the possibility to oxidize preferably the silicon (Si) in metal contained silicide rather than a pure crystalline Si at high temperatures. Thus, we first tried to reproduce and study these conditions and once acquired, targeted to decrease the oxidation temperature in order to fit with industrial requirements. Titanium (Ti) and Nickel (Ni) are chosen for their metallurgical interest and their integration capability in devices. Thus, four different group/phases (TiSi, TiSi2, Ni2Si, NiSi) of silicide were targeted by adjusting the temperature. In situ X-ray diffraction (XRD), photoelectron spectroscopy and sheet resistance (four point probe) measurements were carried out simultaneously before and after oxidation of silicide to characterize the phase and chemical composition. After silicide formation last three phases (TiSi2, Ni2Si, NiSi) were confirmed by XRD and G1(Ti/Si) was unknown, where only for NiSi was observed the low sheet resistance (≈7.3 Ω/□) and resistivity (18 μΩ·cm). After (dry, wet and plasma) oxidation, the phases of TiSi2 and Ni2Si changed and only NiSi was observed the constant phase, even pure SiO2 was noted on NiSi after wet oxidation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and interfaces · Silicon and Solar Cell Technologies · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Kinetics study of NiPt(10at%)/Si0.7Ge0.3 solid state reactions10.1016/j.mee.2013.12.009 ↗
2. Advanced model and analysis of series resistance for CMOS scaling into nanometer regime. II. Quantative analysis10.1109/16.987118 ↗
3. Salicidation process using NiSi and its device application10.1063/1.365410 ↗
4. NiSi salicide technology for scaled CMOS10.1016/S0167-9317(01)00684-0 ↗
5. Self-aligned nickel-mono-silicide technology for high-speed deep submicrometer logic CMOS ULSI10.1109/16.381988 ↗
6. Improvement of thermal stability of nickel silicide using co-sputtering of Ni and Ti for nano-scale CMOS technology10.5573/JSTS.2013.13.3.252 ↗
7. Reduction of sheet resistance and low-thermal-budget relaxation of stress gradients in polysilicon microcantilever beams using nickel-silicides10.1109/JMEMS.2007.892898 ↗
8. Self-aligned nickel–platinum silicide oxidation10.1016/j.mseb.2008.08.010 ↗
9. Spectroscopic ellipsometry model for optical constant of NiSi formed on silicon-on-insulator substrates10.1063/1.4706561 ↗
10. H. Lee, N. Sekwon, J. Kang, Method for preparing silicide of a semiconductor Device and a Source/Drain for use in the semiconductor device, U.S Patent USPTO 20150279737, 2015.
11. Reactive vapor deposition and electrochemical performance of nano-structured magnesium silicide on silicon and silicon carbide substrates10.1016/j.mssp.2014.09.003 ↗
12. Thermal oxidation of silicides10.1063/1.334212 ↗
13. J. Electrochem. Soc. · 1984 · 131 · 37110.1149/1.2115587 ↗
14. Room-temperature oxidation of Ni, Pd, and Pt silicides10.1063/1.334371 ↗
15. A study of the oxidation of selected metal silicides10.1063/1.339383 ↗
16. Rate of formation of silicon dioxide; semiconducting ruthenium silicide10.1063/1.96315 ↗
17. Interface effects in the formation of silicon oxide on metal silicide layers over silicon substrates10.1063/1.332821 ↗
18. Oxidation of silicide thin films: TiSi210.1063/1.93940 ↗
19. XPS calibration study of thin-film nickel silicides10.1002/sia.3050 ↗
20. Microstructural investigation of nickel silicide thin films and the silicide–silicon interface using transmission electron microscopy10.1016/j.micron.2008.01.012 ↗
21. Effects of additive elements on the phase formation and morphological stability of nickel monosilicide films10.1016/j.mee.2006.09.006 ↗