Abstract
Abstract When the composition of some P-type Cd0.96Zn0.04Te (CZT) crystals grown by the vertical Bridgman method (VB) is analyzed by component mapping spectrometer. It is observed that the short-wave (800–1000 nm) infrared absorption edge is inclined, accompanied by a decreased long-wave (400-4000 cm−1) infrared transmittance, which leads to an apparent interference of Zn component mapping measurement. In our research, effects of roughness, surface composition, and internal defects on the absorption edge slope of CZT (hereinafter referred to as the edge slope) were investigated by AFM, EDX, XPS and PICTS, and the main cause of non-uniformity of the slope mapping was obtained from annealing treatment. The results indicated that compared with the surface roughness and surface composition due to our surface treatment process, the dominant defect (Cd vacancy) in CZT was the principal influence factor for the edge slope, whose value was negatively correlated with the defect concentration. Furthermore, the inclination of the edge slope and the simultaneous decrease of long-wave infrared transmittance could be respectively explained by the tail state effect and the free carrier absorption caused by high-concentration Cd vacancy absorption. The mapping distribution trend of the slope presented consistency with that of the long-wave transmittance. In addition, the non-uniformity distribution of the edge slope mapping, can be effectively improved by adequate annealing under Cd atmosphere. Steep slopes and a monotonous distribution of Zn content was observed after annealing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Semiconductor Detectors and Materials · Semiconductor Quantum Structures and Devices · Optical Systems and Laser Technology
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Investigation of structural defects in In-doped CdZnTe under different in-situ annealing cooling rates10.1016/j.jcrysgro.2015.06.020 ↗
2. Carrier transport performance of Cd0.9Zn0.1Te detector by direct current photoconductive technology10.1063/1.4974201 ↗
3. Influences of Te-rich and Cd-rich precipitates of CdZnTe substrates on the surface defects of HgCdTe liquid-phase epitaxy materials10.1007/s11664-014-3110-9 ↗
4. Molecular beam epitaxy growth of HgCdTe on large-area Si and CdZnTe substrates10.1007/s11664-011-1665-2 ↗
5. The qualities of cadmium zinc telluride single crystals grown from different materials crucibles
6. Material properties of large-volume CZT crystals and their relationship to nuclear detector performance10.1007/s11664-998-0055-x ↗
7. Extracti on of mobile impurities from CdZnTe10.1007/s11664-000-0224-z ↗
8. Infrared attenuation spectrum of bulk high-resistivity CdZnTe single crystal in transparent wavelength region between electronic and lattice absorptions
9. Infrared absorption behavior in CdZnTe substrates10.1007/BF02665843 ↗
10. Electrodeless measurement method of conduction type based on the free carrier absorption effect in CdZnTe10.1016/j.mssp.2017.09.010 ↗
11. Quality improvement of CdZnTe single crystal by ultrasound processing10.1016/j.jcrysgro.2017.03.019 ↗
12. Zn concentration determination in CdZnTe by NIR spectroscopy10.1016/S0022-0248(98)00741-6 ↗
13. Band gap energy determination by photoacoustic absorption and optical analysis of Cd1-xZnxTe for low zinc concentrations10.1016/j.jcrysgro.2005.09.022 ↗
14. Optical techniques for composition measurement of bulk and thin-film Cd1-yZnyTe
15. X phase equilibrium and vapor pressure scanning of non-stoichiometry in CdTe10.1016/0022-0248(95)00603-6 ↗
16. Terracing in HgCdTe LPE films grown from Te solution
17. Investigation on the contact interface of Au/Zn on CdZnTe (111) B surface10.1016/j.mssp.2017.03.017 ↗
18. Point defects: their influence on electron trapping, resistivity, and electron mobility-lifetime product in CdTexSe1−x detectors10.1063/1.4939647 ↗
19. Chu · Appl. Phys. Lett. · 2001 · 79 · 2729
20. Characterization of p-type CdTe bridgman crystals by infrared extinction spectra10.1002/pssa.2211200240 ↗
21. Investigation about elliptical region observed on CdZnTe wafers after etching treatment10.1016/j.jcrysgro.2019.05.001 ↗