Abstract Self-aligned electroplating is applied to form the Cu pillar/Sn-Ag bump for semiconductor device packaging, while passivation SiN cracks are usually observed at the bump edge on the bump of the array (BOA). In this paper, the simulation method was used to investigate the mechanism of SiN cracks and then, the bump process was optimized to improve the mechanical properties of the Cu pillar/Sn-Ag bump. It was found that higher reflow rounds could improve the shear strength due to the large degree of contact between the rugged scallop-like shape of the Cu6Sn5 and the Sn-Ag solder. The fracture plane cleaved between the Sn-Ag and Cu6Sn5 interface is consistent with the simulation results. The hardness of the Sn‒Ag solder is proportional to the reflow rounds, and the amount of Ag3Sn phase precipitation within the Sn-Ag solder contributes to the hardness value. In contrast, the disadvantage is that thermal residual stress could deteriorate the SiN crack, especially for a BOA structure The study concludes that an optimal bump process, including Sn-2%Ag solders at 260 °C for 30 s, could obtain a high shear strength and appropriate solder hardness without passivated SiN cracking.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Tunnel field-effect transistors as energy-efficient electronic switches10.1038/nature10679 ↗
2. L. Meinshausen, K. Weide-Zaage, M. Petzold, Electro- and thermomigration in micro bump interconnects for 3D integration, in: Proceedings of the 61st Electronic Components and Technology Conference (ECTC), 2011 IEEE, 2011, pp. 1444–1451.10.1109/ECTC.2011.5898701 ↗
3. Effect of Al-trace dimension on joule heating and current crowding in flip-chip solder joints under accelerated electromigration10.1063/1.2198809 ↗
4. Thermomigration in flip-chip SnPb solder joints under alternating current stressing10.1063/1.2721136 ↗
5. Mean-time-to-failure study of flip chip solder joints on Cu/Ni(V)/Al thin-film under-bump-metallization10.1063/1.1616993 ↗
6. Interfacial morphology and shear deformation of flip chip solder joints10.1557/JMR.2000.0242 ↗
7. Electromigration in flip chip solder joints having a thick Cu column bump and a shallow solder interconnect10.1063/1.2402475 ↗
8. Influence of Cu column under-bump-metallizations on current crowding and joule heating effects of electromigration in flip-chip solder joints10.1063/1.3682484 ↗
9. Effects of sulfide-forming element additions on the Kirkendall void formation and drop impact reliability of Cu/Sn-3.5Ag solder joints10.1016/j.actamat.2009.06.060 ↗
10. Fe addition to Sn-3.5Ag solder for the suppression of Kirkendall void formation10.1016/j.scriptamat.2013.04.010 ↗
11. Effects of Ag on the Kirkendall void formation of Sn-xAg/Cu solder joints10.1063/1.3488629 ↗
12. Effects of residual S on Kirkendall void formation at Cu/Sn-3.5Ag solder joints10.1016/j.actamat.2008.07.022 ↗
13. Reinhardt · 2008 · 202
14. Silicon nitride foams from emulsions10.1016/j.matlet.2014.04.102 ↗