Investigation of “fur-like” residues post dry etching of polyimide using aluminum hard etch mask
Source abstract
Abstract
The authors found that oxygen plasma etching of polyimide (PI) with aluminum (Al) as a hard-etch mask results in lightly textured arbitrary shaped “fur-like” residues. Upon investigation, the presence of Al was detected in these residues. Ruling out several causes of metal contamination that were already reported in literature, a new theory for the presence of the metal containing residues is described. Furthermore, different methods for the residue free etching of PI using an Al hard-etch by using different metal deposition and patterning methods are explored. A fur-free procedure for the etching of PI using a one step-reactive ion etch of the metal hard-etch mask is presented.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Sensor and Energy Harvesting Materials · Synthesis and properties of polymers · Surface Modification and Superhydrophobicity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. W. Li, J.-L. Zhang, H.-M. Li, T. Ding, L. Wang, Preparation of ultrafiltration membranes with aromatic polyimide, in: Proceedings of the Fifth International Membrane Science & Technology Conference, Sydney, Australia, 2003, pp. 1–6.
2. Bessonov · 1987
3. Ghosh, Malay K., and Polyimides, K.L., Mittal K.L., Fundamentals and applications, 1996, Marcel Dekker, New York.
4. Properties of thin polyimide films10.1149/1.2129377 ↗
5. Recent applications of polyimide to micromachining technology10.1109/41.464605 ↗
6. Dielectric properties of polyimide film. ii. dc properties10.1109/TEI.1979.298160 ↗
7. Emerging flexible and wearable physical sensing platforms for healthcare and biomedical applications10.1038/micronano.2016.43 ↗
8. Flex-to-rigid (f2r): A generic platform for the fabrication and assembly of flexible sensors for minimally invasive instruments10.1109/JSEN.2013.2252613 ↗
9. Ultra-stretchable interconnects for high-density stretchable electronics10.3390/mi8090277 ↗
10. Studies of adhesion of metal films to polyimide10.1116/1.577228 ↗
11. Residue-free plasma etching of polyimide coatings for small pitch vias with improved step coverage10.1116/1.4788795 ↗
12. Investigation of polyimide residue due to reactive ion etching in o 210.1149/1.1836660 ↗
13. Adhesion improvement of polyimide/pdms interface by polyimide surface modification10.1557/adv.2016.56 ↗
14. Aeromems wall hot-wire anemometer on polyimide substrate featuring top side or bottom side bondpads10.1109/JSEN.2007.897933 ↗
15. Plasma surface modification of polymers for improved adhesion: a critical review10.1163/156856193X00600 ↗
16. S.J.B. Reed, S.J.B. Reed, Electron microprobe analysis, Vol. 2, Cambridge University Press Cambridge, 1975.
17. Competitive mechanisms in reactive ion etching in a cf 4 plasma10.1149/1.2129063 ↗
18. The effect of aluminum vs. photoresist masking on the etching rates of silicon and silicon dioxide in cf 4/o 2 plasmas10.1149/1.2100408 ↗
19. Xps and water contact angle measurements on aged and corona-treated pp10.1002/(SICI)1097-4628(19991114)74:7<1846::AID-APP29>3.0.CO;2-B ↗
20. Improvement of the polyimide surface wettability using siox films deposited in a decr reactor from hmdso/o2 mixtures10.1002/ppap.200500016 ↗
21. Surface modifications of kapton and cured polyimide films by arf excimer laser: applications to imagewise wetting and metallization10.1016/0169-4332(90)90154-R ↗
22. In situ synthesized al4c3 nanorods with excellent strengthening effect in aluminum matrix composites10.1002/adem.201400232 ↗
23. Rapid, energy-efficient synthesis of the layered carbide, al 4c 310.1039/C4GC01277A ↗