journal article·2016-10

SiC sedimentation and carbon migration in mc-Si by election beam melting with slow cooling pattern

Shiqiang Qin, Dachuan Jiang, Pengting Li, Shuang Shi, Xiaoliang Guo, Guangye An, Yi Tan

Publisher page

Abstract

Abstract The development of photovoltaic industry demands great amount of multicrystalline silicon. Carbon and SiC in silicon need to be contained in a limited amount since they can cause great adverse affect to solar cells. The behavior of carbon and its precipitation SiC in silicon by electron beam melting (EBM) with a slow cooling pattern was investigated in this study. SiC is found to sedimentate to ingot bottom after EBM. The presence of Si 3 N 4 can be heterogeneous nucleation agent for SiC to nucleate continually and both of them precipitate to the ingot bottom. The comprehensive effect of slow solidification condition, temperature gradient and melt convection causes the sedimentation of SiC. It is also found that oxygen plays an important role on the migration of the dissolved carbon. The formation of carbon-oxygen complexes tend to migrate to ingot top since oxygen can transfer from silicon melt to vacuum environment during EBM.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Removal of aluminum from silicon by electron beam melting with exponential decreasing power10.1016/j.seppur.2015.08.002 ↗
2. Impurity segregation behavior in polycrystalline silicon ingot grown with variation of electron- beam power
3. Removal of aluminum and calcium in multicrystalline silicon by vacuum induction melting and directional solidification10.1016/j.vacuum.2013.06.015 ↗
4. Boron removal from silicon melts by H2O/H2 gas blowing: mass transfer in gas and melt
5. Application of electron beam melting to the removal of phosphorus from silicon: toward production of solar-grade silicon by metallurgical processes10.1155/2013/857196 ↗
6. Characterization of a 75kg multicrystalline Si ingot grown in a KRISTMAG®-type G2-sized directional solidification furnace10.1016/j.solmat.2014.04.028 ↗
7. Impurity segregation in directional solidified multi-crystalline silicon10.1016/j.jcrysgro.2010.07.052 ↗
8. Oxygen and carbon precipitation in multicrystalline solar silicon10.1002/(SICI)1521-396X(199901)171:1<175::AID-PSSA175>3.0.CO;2-Q ↗
9. A TEM study of SiC particles and filaments precipitated in multicrystalline Si for solar cells10.1016/j.solmat.2008.04.016 ↗
10. A rapid thermal process for silicon recycle and refining from cutting kerfloss slurry waste10.1016/j.seppur.2015.05.030 ↗
11. Modified sedimentation system for improving separation of silicon and silicon carbide in recycling of sawing waste10.1016/j.seppur.2011.01.011 ↗
12. Separation of silicon and silicon carbide using an electrical field10.1016/j.seppur.2009.04.009 ↗
13. Silicon and silicon carbide powders recycling technology from wire-saw cutting waste in slicing process of silicon ingots10.1016/j.seppur.2014.06.036 ↗
14. Silicon recovery from cutting slurry by phase transfer separation10.1016/j.seppur.2014.06.037 ↗
15. Crystallization of 640kg mc-silicon ingots under traveling magnetic field by using a heater-magnet module10.1016/j.jcrysgro.2012.11.049 ↗
16. Removal of silicon carbide from kerf loss slurry by Al-Si alloying process10.1016/j.seppur.2012.01.021 ↗
17. Characterization of mc-Si directionally solidified in travelling magnetic fields10.1016/j.jcrysgro.2012.03.017 ↗
18. Behavior of carbon in electron beam melted mc-silicon10.1016/j.vacuum.2015.08.022 ↗
19. Carbon concentration and particle precipitation during directional solidification of multicrystalline silicon for solar cells10.1016/j.jcrysgro.2007.11.165 ↗
20. Defects in nitrogen-doped multicrystalline silicon10.1016/j.physb.2003.10.027 ↗
21. Removal of oxygen from silicon by electron beam melting10.1007/s00339-014-8367-6 ↗