Metallic impurity gettering to defects remaining in the RP/2 region of MeV-ion implanted and annealed silicon
Source abstract
Abstract
Abstract Damage has been observed in MeV-ion-implanted Si away from the projected ion range, RP, mainly around RP/2, after annealing at temperatures between 700 and 1000°C. The most suitable way to detect this damage is to decorate it with metals and to measure the metal distribution. The formation and disappearance of the RP/2 damage has been investigated by Cu gettering in Si+-ion implanted Si versus temperature and time of the annealing cycle. It is believed that an excess of vacancies around RP/2 getter metal impurities. By means of positron annihilation spectroscopy no vacancy defects have been detected. In contrast, XTEM investigation reveals small (20–30 nm) interstitial loops in the RP/2 region. The creation of these loops is triggered by interstitials injected during the ion milling procedure used for TEM specimen preparation. The ion bombardment of Si gives rise to self-interstitials that may modify the existing interstitial clusters to bigger agglomerates observable by XTEM.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Ion-surface interactions and analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Proximity gettering with mega-electron-volt carbon and oxygen implantations10.1063/1.99233 ↗
2. Koegler R, Panknin D, Skorupa W, Werner P, Danilin A. Impurity gettering in damaged regions of Si produced by high energy ion implantation. Proceedings of the 11th International Conference on Ion Implantation and Technology, 1996. p. 679–81.10.1109/IIT.1996.586502 ↗
3. Koegler R, Posselt M, Yankov RA, Kaschny JR, Skorupa W, Danilin AB. Detection of metastable defective regions in ion-implanted silicon by means of metal gettering. Material Research Society Symposium Proceedings, 1997, vol. 469, p. 463–8.10.1557/PROC-469-463 ↗
4. MeV-ion-indused damage in Si and its annealing10.1016/0168-583X(91)95282-I ↗
5. Metallic impurity gettering in MeV implanted Si10.4028/www.scientific.net/SSP.57-58.69 ↗
6. Impurity gettering to secondary defects created by MeV ion implantation in silicon10.1063/1.368438 ↗
7. Heinig KH, Jaeger HU. Simulations for impurity gettering in silicon by ion implantation induced defects. Mater Sci Semicond Processing.
8. Spatial distribution of defects in ion-implanted and annealed Si10.1016/S0168-583X(98)00341-3 ↗
9. Mechanism of iron gettering in MeV Si ion implanted epitaxial silicon10.1063/1.368462 ↗
10. A magnetically guided slow positron beam system for defect studies10.12693/APhysPolA.88.7 ↗
11. Proximity gettering of heavy metals by high-energy ion implantation10.1143/JJAP.32.303 ↗
12. Defects remaining in MeV-ion-implanted and annealed Si away from the peak of the nuclear energy deposition profile10.1016/S0168-583X(98)00534-5 ↗
13. Injection of self-interstitials during sputter depth profiling of Si at room temperature10.1063/1.122681 ↗
14. Proximity gettering of transition metals in separation by implanted oxygen structures10.1063/1.114929 ↗
15. Distribution of gettering centres at a buried amorphous layer in silicon10.1016/S0168-583X(98)00762-9 ↗