Effects of deposition temperature on the structure and thermal stability of a-C:F films with low dielectric constant
Source abstract
Abstract
Abstract Fluorinated amorphous carbon films (a-C:F) with low dielectric constant were prepared at different temperatures by electron cyclotron resonance chemical vapor deposition (ECR-CVD) using CHF 3 and C 2 H 2 as precursors. The changes of structures, chemical compositions, and dielectric properties with deposition temperature were investigated by Fourier transform infrared spectroscopy, X-ray photoelectron spectroscopy, Raman spectroscopy and capacitance–voltage characteristics. We found that a-C:F films prepared at high deposition temperature of 300 °C remained amorphous, but the dielectric constant increased from 2.2 for the films deposited at room temperature to 2.75 while F/C composition ratio in the films decreased from 2.3 to 1.5. In order to study the thermal stability the samples were annealed up to 500 °C in vacuum ambience. The films deposited at high substrate temperature have lower F/C, less CF 3 , CF 2 bonding and more cross-linking structures, and thereby lead to better thermal stability.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Copper Interconnects and Reliability · Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Yi · Thin Solid Films · 2000 · 374 · 10310.1016/S0040-6090(00)01021-X ↗
2. Murarka · Solid State Technol · 1996 · 3 · 83
3. Laxman · Semicond Intern · 1995 · 5 · 71
4. Endo · J Appl Phys · 1995 · 78 · 137010.1063/1.360313 ↗
5. Endo · Jpn J Appl Phys · 1998 · 37 · 180910.1143/JJAP.37.1809 ↗
6. Yokomichi · Appl Phys Lett · 1998 · 72 · 270410.1063/1.121105 ↗
7. Yang · Appl Phys Lett · 1998 · 73 · 151410.1063/1.122190 ↗
8. Shirafuji · Thin Solid Films · 2000 · 374 · 25610.1016/S0040-6090(00)01159-7 ↗
9. Ariel · Mater Sci Semicond Process · 2001 · 4 · 38310.1016/S1369-8001(00)00096-2 ↗
10. Yang · Acta Phys Sinica · 2002 · 51 · 132110.7498/aps.51.1321 ↗
11. Zhaoyuan · Current Appl Phys · 2002 · 2 · 43910.1016/S1567-1739(02)00153-0 ↗
12. Yang · Microchem J · 1999 · 63 · 16110.1006/mchj.1999.1778 ↗
13. Theil · Mater Res Soc Symp Proc · 1997 · 476 · 3110.1557/PROC-476-31 ↗
14. Muller · Surf Coat Technol · 1995 · 76–77 · 36710.1016/0257-8972(95)02560-X ↗