Cracking mechanism of CdZnTe polycrystalline film deposited on TFT circuit board at high temperature by close-spaced sublimation method
Source abstract
Abstract
Abstract In this paper, CdZnTe polycrystalline films are grown on TFT circuit boards and ITO/TFT substrates by using close-spaced sublimation (CSS) technique. The phase, morphology and structure of CZT polycrystalline film were characterized by XRD, SEM and EDS, and the cracking mechanism of CZT film deposited on TFT circuit board at high temperature was studied. The results show that the substrate temperature was too high during experiment, which released the stress between Al film and ITO film, produced small hills, and made the binding force of ITO and CZT film greater than that of ITO film and Mo/Al/Mo, resulting in CZT film falling off. The presence of SiNx on TFT circuit board can promote the rupture of CZT film.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Semiconductor Detectors and Materials · ZnO doping and properties · Chalcogenide Semiconductor Thin Films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. CdTe and CdZnTe materials for room-temperature X-ray and gamma ray detectors10.1016/S0022-0248(97)00808-7 ↗
2. Investigation on the contact interface of Au/Zn on CdZnTe (111) B surface10.1016/j.mssp.2017.03.017 ↗
3. Sigmoid-growth curve of lattice-constant against annealing-temperature of Cd1−xZnxTe thin films and its structural, optical and morphological characteristics10.1016/j.mssp.2016.06.003 ↗
4. Electrical, structural and optical properties of Cd1-xZnxTe thick polycrystalline films10.1016/j.vacuum.2018.01.010 ↗
5. The surface morphology, structural properties and chemical composition of Cd1−xZnxTe polycrystalline thick films deposited by close spaced vacuum sublimation10.1016/j.mssp.2017.02.004 ↗
6. Photoluminescence of CdZnTe thick films obtained by close-spaced vacuum sublimation10.1016/j.jlumin.2015.11.027 ↗
7. Thick film compound semiconductors for X-ray imaging applications10.1016/j.nima.2006.01.110 ↗
8. Control of Zn composition (0<x<1) in Cd1−xZnxTe epitaxial layers on GaAs substrates grown by MOVPE10.1016/j.apsusc.2004.09.144 ↗
9. Study on factors influencing the edge slope of infrared absorption of CdZnTe crystal10.1016/j.mssp.2019.104871 ↗
10. Improvement of crystalline quality of CdZnTe epilayers on GaAs(001) substrates with a two-step growth by Close Spaced Sublimation10.1016/j.vacuum.2019.03.036 ↗
11. Spectroscopic and electrical analysis of vacuum co-evaporated CdxZn1-xTe thin films10.1016/j.spmi.2020.106521 ↗
12. Influence of device deposition techniques on the process optimization of CdZnTe thin-film matrix using charge-based analysis10.1016/j.mssp.2020.105074 ↗
13. Understanding individual defects in CdTe thin-film solar cells via STEM: from atomic structure to electrical activity10.1016/j.mssp.2016.06.017 ↗
14. Improvement of temporal response and output uniformity of polycrystalline CdZnTe films for high-sensitivity x-ray imaging
15. Gao · 2020 · 109855
16. Novel CdZnTe micro pillar films deposited by CSS method10.1016/j.matlet.2019.127277 ↗
17. Surface passivation of CdZnTe wafers10.1016/j.mssp.2005.11.001 ↗
18. Study on radiation damage effects on CdZnTe detectors under 3 MeV and 2.08 GeV Kr ion irradiation10.1016/j.mssp.2020.105369 ↗
19. Growth and properties of CdZnTe films on different substrates10.1016/j.surfcoat.2018.10.083 ↗
20. The influence of surface processing on properties of CdZnTe films prepared by close-spaced sublimation10.1016/j.surfcoat.2018.10.043 ↗
21. Impact of polishing on crystallinity and static performance of Cd1−xZnxTe10.1016/j.nima.2020.164568 ↗
22. The effect of Ar plasma etching time on the microstructure, optical and photoelectric properties of CdZnTe films10.1016/j.surfcoat.2016.04.036 ↗
23. Enhanced structural, electrical and optical properties of evaporated CdZnTe thin films deposited on different substrates10.1016/j.matlet.2016.09.093 ↗