Etch-stop process for precisely controlling the vertical cavity length of GaN-based devices
Source abstract
Abstract
Abstract In this study, an etch-stop process was developed using inductively coupled plasma reactive-ion etching for precisely controlling the vertical cavity length of GaN-based devices, such as vertical-cavity surface-emitting lasers (VCSELs) and VCSEL 2D arrays. An AlN layer, which was the etch-stop layer, was added to the epitaxial structure for defining the bottom of a vertical cavity. A uniform vertical cavity length was thus obtained across the entire wafer. Consequently, the flatness of the bottom-end facet was determined from the quality of epitaxial growth rather than the quality of chemical mechanical polishing. The surface morphologies of the wafer in various processing stages were also inspected and compared.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: GaN-based semiconductor devices and materials · Semiconductor materials and devices · Semiconductor Lasers and Optical Devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Characteristics of current-injected GaN-based vertical-cavity surface-emitting lasers10.1109/JSTQE.2011.2116771 ↗
2. GaN-based vertical-cavity surface emitting lasers with sub-milliamp threshold and small divergence angle10.1063/1.4972182 ↗
3. GaInN VCSELs with AlInN/GaN DBRs
4. Improvement in lasing characteristics of GaN-based vertical-cavity surface-emitting lasers fabricated using a GaN substrate10.1143/APEX.2.052101 ↗
5. Demonstration of blue and green GaN-based vertical-cavity surface-emitting lasers by current injection at room temperature10.1143/APEX.4.072103 ↗
6. Room-temperature continuous-wave operation of GaN-based vertical-cavity surface-emitting lasers fabricated using epitaxial lateral overgrowth10.7567/APEX.8.062702 ↗
7. Demonstration of nonpolar GaN-based vertical-cavity surface-emitting lasers10.1143/APEX.5.092104 ↗
8. Smooth top-down photoelectrochemical etching of m-plane GaN10.1149/1.3005978 ↗
9. An etch-stop barrier structure for GaN high-electron-mobility transistors10.1109/LED.2012.2237374 ↗
10. Common emitter current gain >1 in III-N hot electron transistors with 7-nm GaN/InGaN base10.1109/LED.2015.2416345 ↗
11. A GaN HEMT structure allowing self-terminated, plasma-free etching for high-uniformity, high-mobility enhancement-mode devices10.1109/LED.2016.2533422 ↗
12. “Ultra-low rate dry etching conditions for fabricating normally-off field effect transistors on AlGaN/GaN heterostructures10.1016/j.sse.2017.10.010 ↗
13. High-performance normally off p-GaN gate HEMT with composite AlN/Al0.17Ga0.83N/Al0.3Ga0.7N barrier layers design10.1109/JEDS.2018.2789908 ↗
14. Oxygen-based digital etching of AlGaN/GaN structures with AlN as etch-stop layers
15. Origin of etch delay time in Cl2 dry etching of AlGaN/GaN structures10.1063/1.1632035 ↗
16. Surface properties of AlxGa1-xN/GaN heterostructures treated by fluorine plasma: an XPS study10.1002/pssc.201000927 ↗
17. Comparison between AlGaN surfaces etched by carbon tetrafluoride and argon plasmas: effect of the fluorine impurities incorporated in the surface10.1016/j.vacuum.2015.06.002 ↗
18. Normally-off AlGaN/GaN-based MOS-HEMT with self-terminating TMAH wet recess etching10.1016/j.sse.2017.11.002 ↗
19. “C 1s and Au 4f7/2 referenced XPS binding energy data obtained with different aluminum oxides, -hydroxides and –fluorides10.1007/s002160050376 ↗