Length effect on the plastic deformation of SiO2 microcantilevers
Source abstract
Abstract
SiO 2 films are of much interest for the realization of suspended micromechanical structures such as microcantilevers and micro-bridges owing to their superior characteristics when compared to conventional c-Si. However, presence of residual stress induced bending and structural plastic deformation in these devices especially at elevated temperatures hinder their potential for real-time field applications. Moreover, the impact of micro-scale dimensional effects on the magnitude of deformation in these devices is not well understood. In this work, we have investigated the effect of post-release high temperature annealing on the bending and resonance frequency characteristics of SiO 2 microcantilevers (MCs) with a specific focus on the length effect. For this purpose, SiO 2 MCs of various lengths (Length: 50–190 μm, Width: 37 μm and thickness: 0.98 μm) were fabricated using direct laser writer and wet chemical etching methods and were subjected to high temperature annealing under N 2 and O 2 environments. We demonstrate through our experiments that the curvature of SiO 2 MCs increases with both annealing temperature and length square of MCs. Our experiments revealed that, apart from onset of plastic deformation, stress accumulation at the fixed end of SiO 2 MCs is also responsible for the observed curvature increase. From the measured curvature, mean ( σ 0) and gradient ( σ 1) residual stress values were estimated and found to increase with annealing temperature. Interestingly, there exists a critical length of MCs (90 μm) below which both σ 0 and σ 1 were found to increase further with reducing MC length and is shown to be due to the existence of large transverse curvature at these dimensions. High temperature annealing was also found to increase the resonance frequency of MCs and the increase was maximum ∼ 8% for 130 μm long MC. Various possible reasons for the frequency shift is discussed in detail.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced MEMS and NEMS Technologies · Mechanical and Optical Resonators · Force Microscopy Techniques and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Nam · 2006
2. Silicon dioxide films by RF sputtering for microelectronic and MEMS applications10.1088/0960-1317/17/5/029 ↗
3. A single-sided micromachined piezoresistive SiO2 cantilever sensor for ultra-sensitive detection of gaseous chemicals10.1088/0960-1317/16/12/004 ↗
4. Silicon dioxide microcantilever with piezoresistive element integrated for portable ultraresoluble gaseous detection
5. Bio/chemical detection in liquid with self-sensing Pr-Oxi-Lever (piezo-resistive SiO2 cantilever) sensors10.1016/j.mee.2010.05.001 ↗
6. Chen · 2007 · 1436
7. Simple fabrication of an uncooled Al/SiO2 microcantilever IR detector based on bulk micromachining10.1007/s00542-013-1854-4 ↗
8. Fabrication and characterization of suspended beam structures for SiO2 photonic MEMS10.1088/0960-1317/25/10/105003 ↗
9. Determining mean and gradient residual stresses in thin films using micromachined cantilevers10.1088/0960-1317/6/3/002 ↗
10. Effect of biaxial curvature on the resonance frequency of uncoated microcantilevers10.1016/j.sna.2020.111857 ↗
11. High resolution determination of local residual stress gradients in single- and multilayer thin film systems10.1016/j.actamat.2015.10.044 ↗
12. An effective method of determining the residual stress gradients in a micro-cantilever10.1007/s00542-005-0065-z ↗
13. Optimizing amorphous indium zinc oxide film growth for low residual stress and high electrical conductivity10.1016/j.apsusc.2013.06.019 ↗
14. Residual-stress relaxation in polysilicon thin films by high-temperature rapid thermal annealing10.1016/S0924-4247(97)01661-0 ↗
15. Laser bending for high-precision curvature adjustment of microcantilevers
16. Effect of post-deposition annealing on atomic layer deposited SiO2 film for silicon surface passivation10.1016/j.mssp.2019.104777 ↗
17. Overview of residual stress in MEMS structures: its origin, measurement, and control10.1007/s10854-021-05405-8 ↗
18. Size effect on brittle-ductile transition temperature of silicon by means of tensile testing
19. The plastic deformation of silicon between 300°C and 600°C10.1080/01418618108235821 ↗
20. Plastic deformation of micromachined silicon diaphragms with a sealed cavity at high temperatures
21. Plastic deformation of membrane with mesa silicon microstructure10.1007/s00542-016-3059-0 ↗
22. A micro plasticity model for pure bending analysis of curved beam-like MEMS devices
23. Creep of thin film Au on bimaterial Au/Si microcantilevers10.1016/j.actamat.2004.01.005 ↗
24. Kuo · 2005 · 290
25. Inelastic deformation of bilayer microcantilevers with nanoscale coating10.1016/j.sna.2011.03.016 ↗
26. Post-release deformation and curvature correction of an electrothermally actuated MEMS bilayer platform10.1016/j.mee.2019.111192 ↗
27. Fabrication and characterization of SiO2 microcantilevers by direct laser writing and wet chemical etching methods for relative humidity sensing10.1016/j.mee.2019.04.005 ↗
28. EVOLUTION OF Si/SiO//2 INTERFACE ROUGHNESS
29. In-plane stress development in sol–gel-derived titania and silica thin films on Si(100) substrates10.1007/s10971-019-05212-y ↗
30. Madou · 2011
31. Determination of compressive residual stress in a doubly-clamped microbeam according to its buckled shape10.1016/j.mee.2007.07.008 ↗
32. Effect of width on the stress-induced bending of micromachined bilayer cantilevers10.1088/0960-1317/13/1/320 ↗
33. On the determination of thermal expansion coefficient of thermal oxide
34. Thin films stress extraction using micromachined structures and wafer curvature measurements10.1016/j.mee.2004.07.003 ↗
35. Intrinsic stress and stress gradients at the SiO2/Si interface in structures prepared by thermal oxidation of Si and subjected to rapid thermal annealing10.1116/1.584599 ↗
36. Frequency response of curved bilayer microcantilevers with applications to surface stress measurement
37. Effect of surface stress on the stiffness of thin elastic plates and beams10.1103/PhysRevB.85.085440 ↗
38. Stress-induced variations in the stiffness of micro- and nanocantilever beams10.1103/PhysRevLett.108.236101 ↗
39. Temperature and pressure dependence of resonance in multi-layer microcantilevers10.1088/0960-1317/15/8/011 ↗
40. Microbridge testing of plasma-enhanced chemical-vapor deposited silicon oxide films on silicon wafers10.1063/1.1898449 ↗
41. Density relaxation of silicon dioxide on (100) silicon during thermal annealing10.1063/1.345563 ↗
42. Dimension effect on mechanical behavior of silicon micro-cantilever beams, Measurement10.1016/j.measurement.2007.12.007 ↗
43. How two-dimensional bending can extraordinarily stiffen thin sheets10.1038/srep29627 ↗
44. Effect of surface stress induced curvature on the eigenfrequencies of microcantilever plates10.1063/1.5053561 ↗
45. The plastic and creep characteristics of silicon microstructure at elevated temperature10.1007/s00542-014-2184-x ↗